摘要:
Biodegradable polyetheresteramides P1 which are obtained by reacting(a1) a mixture containing20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof and5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and(a2) a mixture of dihydroxy compounds(a21) from 15 to 99.3 mol % of a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,(a22) from 0.2 to 85 mol % of a dihydroxy compound containing ether functionalities of the formula IHO--((CH.sub.2).sub.n --O).sub.m --H I where n is 2, 3 or 4 and m is an integer from 2 to 250, or mixtures thereof and(a23) from 0.5 to 80 mol % of an amino-C.sub.2 -C.sub.12 -alkanol or amino-C.sub.5 -C.sub.10 -cycloalkanol,where the molar ratio of (a1) to (a2) is from 0.4:1 to 1.5:1, with the proviso, inter alia, that the polyetheresteramides P1 have a molecular weight (M.sub.n) in the range from 5000 to 80,000 g/mol, and biodegradable polymers, biodegradable moldings, and adhesives obtained from the disclosed polymers.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of(a1) a mixture consisting essentially offrom 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, andfrom 0 to 5 mol % of a sulfonate compound,the sum of the individual mole percentages being 100 mol %, and(a2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1,with the proviso that the polyesters P1 have a molecular weight (M.sub.n) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25.degree. C.) and a melting point within the range from 50 to 170.degree. C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to 5 mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation,and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of (a1) a mixture consisting essentially of from 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and (a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and CS-C10-cycloalkanediols, the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1, with the proviso that the polyesters P1 have a molecular weight (Mn) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25° C.) and a melting point within the range from 50 to 170° C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of(a1) a mixture consisting essentially offrom 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, andfrom 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and(a2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1,with the proviso that the polyesters P1 have a molecular weight (M.sub.n) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25.degree. C.) and a melting point within the range from 50 to 170.degree. C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to 5 mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation,and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of (a1) a mixture consisting essentially of from 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and (a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1, with the proviso that the polyesters P1 have a molecular weight (Mn) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25° C.) and a melting point within the range from 50 to 170° C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to 5 mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyetheresteramides Q1 with a molecular weight (M.sub.n) in the range from 6000 to 80,000 g/mol, a viscosity number in the range from 30 to 450 g/ml (measured in o-dichlorobenzene/phenol (50/50 ratio by weight) at a concentration of 0.5% by weight polyetheresteramide Q1 at 25.degree. C.), and a melting point in the range from 50.degree. to 200.degree. C., obtained by reacting a1) from 95 to 99.9% by weight polyetheresteramide P1, obtained by reacting a mixture ofb1) 20-95 mol % adipic acid or ester-forming derivatives thereof, and5-80 mol % terephthalic acid or ester-forming derivatives thereof, andb2) a mixture of a dihydroxy compound selected from C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,b22) a dihydroxy compound which contains ether functionalities and has the formula IHO--((CH.sub.2).sub.n --O)).sub.m --H Iwhere n is 2, 3 or 4 and m is an integer from 2 to 250, andb23) from 0.5 to 80 mol % of an amino-C.sub.2 -C.sub.12 -alkanol or an amino-C.sub.5 -C.sub.10 -cycloalkanol, with or withoutb24) a diamino-C.sub.1 -C.sub.8 -alkane, and/orb25) a 2,2'-bisoxazolinewhere the molar ratio of (b1) to (b2) is in the range from 0.4:1 to 1.5:1, anda2) from 0.1 to 5% by weight of a divinyl ether C1.
摘要:
Biodegradable polyesteramides as defined in the specification are obtained by reacting a mixture consisting essentially of a1) a mixture consisting essentially of 35 to 95 mol % of adipic acid or ester-forming derivatives thereof, 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof, and 0 to 5 mol % of a compound containing sulfonate groups, a2) a mixture consisting essentially of 95.5 to 0.5 mol % of a dihydroxy compound, 0.5 to 99.5 mol % of an amino-C2-C12-alkanol or an amino-C5-C10-cycloalkanol, 0 to 50 mol % of a diamino-C1-C8-alkane, and 0 to 50 mol % of a 2,2′-bisoxazoline of the formula I wherein R1 is as set forth in the specification, and a3) 0 to 5 mol %, based on a1), of a compound D as set forth in the specification; and other biodegradable polymers and thermoplastic molding compositions, their manufacture and their use for producing biodegradable moldings, adhesives, foams, and coatings.
摘要:
A biodegradable polyester obtainable by reacting a mixture comprising (a1) from 95 to 99.9% by weight of a polyester P1 obtainable by reacting a mixture essentially comprising (b1) a mixture comprising 35-95 mol % of adipic acid or ester-forming derivatives thereof, 5-65 mol % of terephthalic acid or ester-forming derivatives thereof, and 0-5 mol % of a compound containing sulfonate groups, and (b2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols, with the proviso that a compound D with at least three groups capable of ester formation is employed to prepare the polyester P1, (a2) from 0.1 to 5% by weight of a divinyl ether C1 and (a3) from 0 to 5 mol %, based on component (b1) from the preparation of P1, of compound D, and other biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings and adhesives.
摘要:
Mixtures comprising (a) pieces of open-cell aminoplastic foam with an average diameter in the range from 50 μm to 5 mm (weight-average), (b) water, (c) at least one surfactant and (d) if appropriate an oil or fat phase.
摘要:
Absorber elements are described of at least one composite material having absorbent elements on a support, in which a plurality of elements of a superabsorbent foam are arranged on at least one support in a grid pattern at distances such that the elements in the swollen state touch at their peripheries.