摘要:
Biodegradable polyesteramides as defined in the specification obtained by reacting a mixture consisting essentially of(a1) from 95 to 99.9% by weight of a polyesteramide,(a2) from 0.1 to 5% by weight of a divinyl ether, and(a3) from 0 to 5 mol % of compound D as defined in the specification, and other biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings obtained from the polymers and molding compositions according to the invention.
摘要:
A biodegradable polyester obtainable by reacting a mixture comprising (a1) from 95 to 99.9% by weight of a polyester P1 obtainable by reacting a mixture essentially comprising (b1) a mixture comprising 35-95 mol % of adipic acid or ester-forming derivatives thereof, 5-65 mol % of terephthalic acid or ester-forming derivatives thereof, and 0-5 mol % of a compound containing sulfonate groups, and (b2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols, with the proviso that a compound D with at least three groups capable of ester formation is employed to prepare the polyester P1, (a2) from 0.1 to 5% by weight of a divinyl ether C1 and (a3) from 0 to 5 mol %, based on component (b1) from the preparation of P1, of compound D, and other biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings and adhesives.
摘要:
Biodegradable polyether esters are obtained by reacting a mixture of(a1) from 95 to 99.9% by weight of polyether ester obtained by reacting(b1) a mixture comprising20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and0-5 mol % of a compound which contains sulfonate groups, and(b2) a mixture of dihydroxy compounds,(a2) from 0.1 to 5% by weight of a divinyl ether C1 and(a3) from 0 to 5 mol %, based on component (b1) from the preparation of P1, of compound D,and other biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers and molding compositions according to the invention.
摘要:
Biodegradable polyetheresteramides Q1 with a molecular weight (M.sub.n) in the range from 6000 to 80,000 g/mol, a viscosity number in the range from 30 to 450 g/ml (measured in o-dichlorobenzene/phenol (50/50 ratio by weight) at a concentration of 0.5% by weight polyetheresteramide Q1 at 25.degree. C.), and a melting point in the range from 50.degree. to 200.degree. C., obtained by reacting a1) from 95 to 99.9% by weight polyetheresteramide P1, obtained by reacting a mixture ofb1) 20-95 mol % adipic acid or ester-forming derivatives thereof, and5-80 mol % terephthalic acid or ester-forming derivatives thereof, andb2) a mixture of a dihydroxy compound selected from C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,b22) a dihydroxy compound which contains ether functionalities and has the formula IHO--((CH.sub.2).sub.n --O)).sub.m --H Iwhere n is 2, 3 or 4 and m is an integer from 2 to 250, andb23) from 0.5 to 80 mol % of an amino-C.sub.2 -C.sub.12 -alkanol or an amino-C.sub.5 -C.sub.10 -cycloalkanol, with or withoutb24) a diamino-C.sub.1 -C.sub.8 -alkane, and/orb25) a 2,2'-bisoxazolinewhere the molar ratio of (b1) to (b2) is in the range from 0.4:1 to 1.5:1, anda2) from 0.1 to 5% by weight of a divinyl ether C1.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of(a1) a mixture consisting essentially offrom 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, andfrom 0 to 5 mol % of a sulfonate compound,the sum of the individual mole percentages being 100 mol %, and(a2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1,with the proviso that the polyesters P1 have a molecular weight (M.sub.n) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25.degree. C.) and a melting point within the range from 50 to 170.degree. C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to 5 mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation,and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of (a1) a mixture consisting essentially of from 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and (a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and CS-C10-cycloalkanediols, the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1, with the proviso that the polyesters P1 have a molecular weight (Mn) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25° C.) and a melting point within the range from 50 to 170° C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
摘要:
Biodegradable polyesters having a molecular weight (M.sub.n) of from 5000 to 50,000 g/mol (measured by gel permeation chromatography), a viscosity number of from 30 to 350 g/ml (measured in 50:50 by weight of o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester at 25.degree. C.), and a melting point of from 50 to 170.degree. C., and having both hydroxyl and carboxyl end groups, the molar ratio of carboxyl end groups to hydroxyl end groups being greater than one, which is obtained by reacting a mixture consisting essentially ofa.sub.1) a mixture consisting essentially offrom 45 to 80 mol % of adipic acid or ester-forming derivatives thereof, or mixtures thereof,from 20 to 55 mol % of terephthalic acid or ester-forming derivatives thereof, or mixtures thereof, andfrom 0 to 5 mol % of a sulfonate compound,where the sum of the individual mole percentages is 100 mol %, anda.sub.2) a dihydroxy compound selected from the group consisting of C.sub.2 -C.sub.6 -alkanediols and C.sub.5 -C.sub.10 -cycloalkanediols,in the presence of from 0.01 to 5 mol %, per mol of component a.sub.1), of a compound D having at least three groups capable of ester formation, the molar ratio of a.sub.1) to a.sub.2) being from 0.4:1 to 1.5:1,polymers and biodegradable thermoplastic molding compositions, processes for their preparation and their use for producing biodegradable moldings, adhesives, foams and blends with starch obtained from the polymers or molding compositions.
摘要:
Biodegradable polyether esters P1 obtainable by the reaction of a mixture consisting essentially of: (a1) a mixture essentiall) of 20 to 95 mol % adipic acid or ester-forming derivatives thereof or mixtures thereof, 5 to 80 mol % terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0 to 5 mol % of a sulphonate group-containing compounds In which the sum of the individual mol percentages is 100; and (a2) a mixture of dihydroxy compounds consisting essentially of (a21) 15 to 99 mol % of a dihydroxy compound selected from the group consisting of C2-C6 alkane diols and C5-C10 cycloalkane diols; (a22) 85 to 0.2 mol % of an ether function-containing dihydroxy compound as in formula I HO—[(CH2)n—O]m—H in which n is 2, 3 or 4 and m is a whole number from 2 to 250, or mixtures thereof, in which the molar ratio of (a1) to (a2) is in the range from 0.4:1 to 1.5:1 with the proviso that the polyether esters P1 have molar weight (Mn) in the range from 5,000 to 80,000 g/mol, a viscosity index in the range from 30 to 450 g/ml (measured in o-dichlorobenzole/phenol (weight ratio 50/50) at a concentration of 0.5 wt. % polyether esters P1 at a temperature of 25° C.) and a melting point in the range from 50 to 200° C., and with the further proviso that from 0.01 to 5 mol %, in relation to the molar quantity of the components (a) used of a compound D with at least three groups capable of ester formation are used to produce the polyether esters P1, and other biodegradable polymers and thermoplastic moulding compounds, process for their production and biodegradable mouldings, adhesives, foams and blends with starch obtainable from the polymers or moulding compounds of the invention.
摘要:
Biodegradable polyether esters P1 obtainable by reacting a mixture essentially comprising: (a1) a mixture essentially comprising: 20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, 5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0-5 mol % of a compound containing sulfonate groups, where the total of the individual mole percentages is 100 mol %, and (a2) a mixture of dihydroxy compounds essentially comprising (a21) from 15 to 99.8 mol % of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, (a22) from 85 to 0.2 mol % of a dihydroxy compound containing ether functionalities of the formula I: HO—[(CH2)n—O]m—H I where n is 2, 3 or 4 and m is an integer from 2 to 250, or mixtures thereof, where the molar ratio of (a1) to (a2) is chosen in the range from 0.4:1 to 1.5:1, with the proviso that the polyether ester P1 has a molecular weight (Mn) in the range from 5000 to 80,000 g/mol, a viscosity number in the range from 30 to 450 g/ml (measured in o-dichlorobenzene/phenol (50/50 ratio by weight) at a concentration of 0.5% by weight of polyether ester P1 at 25° C.) and a melting point in the range from 50 to 200° C., and with the further proviso that from 0.01 to 5 mol %, based on the molar quantity of component (a1) employed, of a compound D with at least three groups capable of ester formation are employed to prepare the polyether ester P1, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings and adhesives, biodegradable moldings, films and blends with starch obtainable from the polymers and molding compositions according to the invention.
摘要:
Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of (a1) a mixture consisting essentially of from 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and (a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1, with the proviso that the polyesters P1 have a molecular weight (Mn) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25° C.) and a melting point within the range from 50 to 170° C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to 5 mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.