摘要:
The invention relates to a previously known method for producing synthetic silica glass, comprising the following steps: a gas stream containing a vaporizable initial substance, which can be converted into SiO2 by means of oxidation or flame hydrolysis, is formed; the gas stream is delivered to a reaction zone in which the initial substance is converted so as to form amorphous SiO2 particles; the amorphous SiO2 particles are deposited on a support so as to form an SiO2 layer; and the SiO2 is vitrified during or following deposition of the SiO2 particles in order to obtain the silica glass. The aim of the invention is to create an economical method for producing synthetic silica glass, which is characterized by a favorable damaging behavior towards short-wave UV radiation while being particularly suitable for producing an optical component used for transmitting high-energy ultraviolet radiation having a wavelength of 250 nm or less. Said aim is achieved by using a mixture of a monomeric silicon compound containing a singular Si atom and an oligomeric silicon compound containing several Si atoms as an initial substance, provided that the oligomeric silicon compound in the mixture contributes less than 70 percent to the total silicon content.
摘要:
The present invention relates to a quartz glass blank for an optical component for transmission of ultraviolet radiation of a wavelength of 250 nm or shorter, and to a use of the quartz glass blank in microlithography in combination with ultraviolet radiation of a wavelength of 250 nm or shorter. Moreover, the invention relates to a procedure for manufacture of the quartz glass blank. A quartz glass blank of the described type should show little induced absorption and be optimized with respect to compaction and decompaction. The quartz glass blank according to the invention is characterized by the following properties: a glass structure essentially free of oxygen defect sites, an H2-content in the range of 0.1×1016 molecules/cm3 to 4.0×1016 molecules/cm3, an OH-content in the range of 125 wt-ppm to 450 wt-ppm, an SiH group-content of less than 5×1016 molecules/cm3, a refractive index inhomogeneity, Δn, of less than 2 ppm, and a stress birefringence of less than 2 nm/cm. In the use according to the invention, the quartz glass blank complies with dimensioning rules (2), (3), and (4) in terms of its OH-content, minimal and maximal hydrogen contents, COH, CH2min, and CH2max, respectively, with P being the pulse number and ε being the energy density: COH [wt-ppm]=1,700×ε[mJ/cm2]0.4±50, (2) CH2min [molecules/cm3]=1×106ε2 P, (3) CH2max [molecules/cm3]=2×1018ε. (4) The procedure according to the invention is characterized in that a mixed quartz glass is generated from a first and a second quartz glass by mixing the two quartz glasses.
摘要:
The present invention relates to a quartz glass blank for an optical component for transmission of ultraviolet radiation of a wavelength of 250 nm or shorter, and to a use of the quartz glass blank in microlithography in combination with ultraviolet radiation of a wavelength of 250 nm or shorter. Moreover, the invention relates to a procedure for manufacture of the quartz glass blank. A quartz glass blank of the described type should show little induced absorption and be optimized with respect to compaction and decompaction. The quartz glass blank according to the invention is characterized by the following properties: a glass structure essentially free of oxygen defect sites, an H2-content in the range of 0.1×1016 molecules/cm3 to 4.0×1016 molecules/cm3, an OH-content in the range of 125 wt-ppm to 450 wt-ppm, an SiH group-content of less than 5×1016 molecules/cm3, a refractive index inhomogeneity, Δn, of less than 2 ppm, and a stress birefringence of less than 2 nm/cm. In the use according to the invention, the quartz glass blank complies with dimensioning rules (2), (3), and (4) in terms of its minimal and maximal hydrogen contents and OH-content, CH2min, CH2max, and COH, respectively, with P being the pulse number and ε being the energy density (in mJ/cm2): CH2min [molecules/cm3]=1×106ε2P, (2) CH2max [molecules/cm3]=2×1018ε, (3) COH [wt-ppm]=1,700×ε[mJ/cm2]0.4±50. (4) The procedure according to the invention is characterized in that a mixed quartz glass is generated from a first and a second quartz glass by mixing the two quartz glasses in the course of a homogenization treatment.
摘要:
A known method for producing synthetic quartz glass comprises the method steps: (a) forming a cylindrical SiO2 soot body having an inner portion and at least one free cylinder jacket surface surrounding the inner portion; (b) thermally drying the porous soot body; and (c) vitrifying the dried soot body with formation of the cylinder from synthetic quartz glass. Starting therefrom, to indicate a method which permits a particularly flat radial distribution in the inner portion of the cylinder, it is suggested according to the invention that the dried SiO2 soot body that is present after method step b) should be subjected to a homogenizing method prior to vitrification, the homogenizing method comprising the following steps: (I) heating the soot body to a consolidation temperature to form a sealing layer in the area of the at least one cylinder jacket, the sealing layer sealing the inner portion to the outside; (II) cooling the soot body from the consolidation temperature; and (III) annealing the soot body in the range of a homogenization temperature during a period of at least 5 hours so that the radial profile of the hydroxyl group concentration flattens in the inner portion.
摘要:
An object of the present invention is to provide an improved blank such that an optical member of a high homogeneity can be obtained therefrom, and to provide a vessel and a heat treatment method for heat-treating a highly uniform synthetic quartz blank. In a first aspect of the invention a special designed blank is provided showing a concave shaped outer surface. In a second aspect of the invention a special designed vessel for heat-treating blanks is provided, whereby the degree of heat emission at the center is set higher than that of the surroundings.
摘要:
In a known method for producing quartz glass that is doped with nitrogen, an SiO2 base product is prepared in the form of SiO2 grains or in the form of a porous semi-finished product produced from the SiO2 grains and the SiO2 base product is processed into the quartz glass with the nitrogen chemically bound therein in a hot process in an atmosphere containing a reaction gas containing nitrogen. From this starting point, a method is provided for achieving nitrogen doping in quartz glass with as high a fraction of chemically bound nitrogen as possible. This object is achieved according to the invention in that a nitrogen oxide is used as the nitrogen-containing reaction gas, and that a SiO2 base product is used that in the hot process has a concentration of oxygen deficient defects of at least 2×1015 cm−3, wherein the SiO2 base product comprises SiO2 particles having an average particle size in the range of 200 nm to 300 μm (D50 value).
摘要:
A known method for producing synthetic quartz glass comprises the method steps: (a) forming a cylindrical SiO2 soot body having an inner portion and at least one free cylinder jacket surface surrounding the inner portion; (b) thermally drying the porous soot body; and (c) vitrifying the dried soot body with formation of the cylinder from synthetic quartz glass. Starting therefrom, to indicate a method which permits a particularly flat radial distribution in the inner portion of the cylinder, it is suggested according to the invention that the dried SiO2 soot body that is present after method step b) should be subjected to a homogenizing method prior to vitrification, the homogenizing method comprising the following steps: (I) heating the soot body to a consolidation temperature to form a sealing layer in the area of the at least one cylinder jacket, the sealing layer sealing the inner portion to the outside; (II) cooling the soot body from the consolidation temperature; and (III) annealing the soot body in the range of a homogenization temperature during a period of at least 5 hours so that the radial profile of the hydroxyl group concentration flattens in the inner portion.
摘要:
To provide an optical component of quartz glass for use in a projection objective for immersion lithography at an operating wavelength below 250 nm, which component is optimized for use with linearly polarized UV laser radiation and particularly with respect to compaction and birefringence induced by anisotropic density change, it is suggested according to the invention that the quartz glass should contain hydroxyl groups in the range of from 1 wtppm to 60 wtppm and chemically bound nitrogen, and that the mean hydrogen content of the quartz glass should be in the range of 5×1015 molecules/cm to 1×1017 molecules/cm3.
摘要翻译:为了提供石英玻璃的光学部件,用于在250nm以下的工作波长下用于浸没式光刻的投影物镜,该成分被优化用于线偏振UV激光辐射,特别是关于由各向异性密度变化引起的压实和双折射 根据本发明,建议石英玻璃应含有1〜60重量ppm的羟基和化学键合的氮,石英玻璃的平均氢含量应在5×1015的范围内 分子/ cm至1×1017分子/ cm 3。
摘要:
The invention is concerned with a material which shows low absorption for UV radiation having a wavelength below 250 nm, low birefringence, high chemical resistance and high radiation resistance and which is therefore particularly usable for Making optical components for microlithography. According to the invention the material consists of synthetically produced quartz crystallites which form a polycrystalline structure and have a mean grain size in the range between 500 nm and 30 μm. The method according to the invention for making a blank from the material comprises providing granules consisting of synthetically produced quartz crystals having a mean grain size in the range between 500 nm and 30 μm, and sintering the granules to obtain a blank of polycrystalline quartz.
摘要:
The invention is concerned with a material which shows low absorption for UV radiation having a wavelength below 250 nm, low birefringence, high chemical resistance and high radiation resistance and which is therefore particularly usable for making optical components for microlithography. According to the invention the material consists of synthetically produced quartz crystallites which form a polycrystalline structure and have a mean grain size in the range between 500 nm and 30 μm. The method according to the invention for making a blank from the material comprises providing granules consisting of synthetically produced quartz crystals having a mean grain size in the range between 500 nm and 30 μm, and sintering the granules to obtain a blank of polycrystalline quartz.