Abstract:
Pressure-sensitive adhesive comprising at least one synthetic rubber based on at least one vinylaromatic (A) and at least one diene (B); the proportion of synthetic rubber being at most 45% by weight; at least one bio-based adhesive resin based to an extent of at least 85% on renewable raw materials and making up a proportion of at least 1% by weight to at most 25% by weight of the entire composition of the pressure-sensitive adhesive.
Abstract:
A single- or double-sidedly bonding adhesive-sheet strip having a self-adhesive composition comprising a) at least one elastomer, at least one type of polybutadiene block copolymer being used as an elastomer, b) at least one partially hydrogenated hydrocarbon resin having a softening temperature of at least 90° C., c) at least one additional hydrocarbon resin, a terpene phenol resin and/or a colophonium resin having a softening temperature of at least 90° C., d) an optional soft resin, and e) additional additives as applicable.
Abstract:
The invention relates to a method for adhering two substrates, namely a first substrate A and a second substrate B, to each other using a latent-reactive adhesive film with at least one latent-reactive adhesive film layer which has a thermoplastic component with a melting temperature T(melt), where 35° C.≦T(melt)≦90° C., said thermoplastic component containing functional groups that can react to isocyanate, and an isocyanate-containing component that is dispersed into the thermoplastic component in a particulate form and is blocked, microencapsulated, or substantially deactivated in the region of the particle surface. The particles have a start temperature T(start) of 40° C.≦T(start)≦120° C., wherein T(start)≧T(melt). A surface of the first substrate A is brought into contact with a first surface of the latent-reactive adhesive film, and a surface of the second substrate B is brought into contact with the second surface of the latent-reactive adhesive film. The adhesion is caused by heating the latent-reactive adhesive film to a temperature which corresponds to or is higher than at least the start temperature T(start). The invention is characterized in that at least the surface of the first substrate A which is brought into contact with the latent-reactive adhesive film is treated with a primer before the first substrate A is brought into contact with the latent-reactive adhesive film, and/or at least the first surface of the latent-reactive adhesive film which is brought into contact with the first substrate A is treated with a primer before the first substrate A is brought into contact with the latent-reactive adhesive film.
Abstract:
An acrylic pressure-sensitive adhesive was to be provided that finds use especially in a reversible adhesive tape that is redetachable without leaving any residue, the adhesive tape having a particularly flat paper backing with high air permeability, and thus gives rise to particularly precise and flat paint edges when applied. This is achieved by an acrylic pressure-sensitive adhesive based on polymers having the following monomer composition:
(a) 97% to 99% by weight of monomers from the group comprising 2-ethylhexyl acrylate or 2-octyl acrylate or n-heptyl acrylate or mixtures of at least two of said monomers, (b) 1% to 3% by weight of (meth)acrylic acid
and further comprising a crosslinking system, wherein the ratio of the reactive crosslinking groups and the carboxy groups of (meth)acrylic acid (b) is less than or equal to 7% and wherein the polymers are produced by emulsion polymerization.
The invention also provides an adhesive tape comprising a backing and—applied to at least one side of the backing—an acrylic pressure-sensitive adhesive of the invention in the form of a dried polymer dispersion and also the use of such an adhesive tape.
Abstract:
Adhesive tapes comprise a textile carrier and a pressure-sensitive adhesive, applied on at least one side of the carrier, in the form of a thickened dried polymer dispersion, wherein the unthickened dried polymer dispersion comprises: (a) 30.0 to 98.0 wt % of monomeric acrylates; (b) 0 to 50.0 wt % of ethylenically unsaturated comonomers which are not acrylates; (c) 1.0 to 10.0 wt % of tackifier; and (d) 1.0 to 10.0 wt % of kaolin, wherein a rheological additive is added to the polymer dispersion so that the polymer dispersion has a viscosity before drying of 40 to 100 Pa*s at a shear rate of 10/s and a viscosity of 3000 to 8000 Pa*s at a shear rate of 0.01/s.
Abstract:
Adhesive tapes comprise a textile carrier and a pressure-sensitive adhesive, applied on at least one side of the carrier, in the form of a thickened dried polymer dispersion, wherein the unthickened dried polymer dispersion comprises: (a) 30.0 to 98.0 wt % of monomeric acrylates; (b) 0 to 50.0 wt % of ethylenically unsaturated comonomers which are not acrylates; (c) 1.0 to 10.0 wt % of tackifier; and (d) 1.0 to 10.0 wt % of kaolin, wherein a rheological additive is added to the polymer dispersion so that the polymer dispersion has a viscosity before drying of 40 to 100 Pa*s at a shear rate of 10/s and a viscosity of 3000 to 8000 Pa*s at a shear rate of 0.01/s.
Abstract:
Disclosed is an adhesive composition comprising: (a) at least one kind of a saturated vinylaromatic block copolymer, (b) at least one kind of a first tackifier resin, which is a hydrocarbon resin having a DACP≥+25° C. and an MMAP≥+60° C., and also either (c1) at least one kind of a second tackifier resin, having a DACP≤0° C. and an MMAP≤+30° C., and (d1) at least one kind of an aliphatic or cycloaliphatic alkyl ester as a plasticizer, or (c2) at least one kind of a second tackifier resin, having a DACP≤0° C. and an MMAP≤+30° C., and (d2) at least one kind of an aliphatic or cycloaliphatic alkyl ester as a plasticizer, and also (e) optionally further additives. The adhesive composition combines high ageing stability with exceptional aptitude for bonding on porous and also on fibrous materials.
Abstract:
The invention relates to an adhesive tape in particular for wrapping cables, consisting of a preferably textile carrier and of a pressure sensitive adhesive, applied on at least one side of the carrier, in the form of a dried polymer dispersion, the polymer having been synthesized from: (a) 70.0 to 90.0 wt % of n-butyl acrylate and/or 2-ethylhexyl acrylate (b) 10.0 to 20.0 wt % of one or more ethylenically unsaturated monomers, where at least 50.0 wt % of the ethylenically unsaturated monomers (monomer (b)) comprises methyl methacrylate (c) 0 to 10.0 wt % of a further ethylenically unsaturated monomer, different from monomer (b) (d) 0 to 5.0 wt % of an ethylenically unsaturated monomer having an acid or acid-anhydride function and the pressure sensitive adhesive comprises between 3 and 20 parts by weight of tackifiers (based on the mass of the dried polymer dispersion), the tackifiers having a softening point of more than 90° C. according to ASTM E29-99 (2009).
Abstract:
Reactive adhesive film, comprising (a) a polymeric film-forming matrix, (b) at least one reactive monomer or reactive resin, and (c) a reagent selected from the group consisting of a radical initiator and an activator, and a reactive 2-component adhesive film system for bonding various materials, such as metal, wood, glass and/or plastic.
Abstract:
Reactive adhesive film, comprising (a) a polymeric film-forming matrix, (b) at least one reactive monomer or reactive resin, and (c) a reagent selected from the group consisting of a radical initiator and an activator, and a reactive 2-component adhesive film system for bonding various materials, such as metal, wood, glass and/or plastic