Abstract:
An ethylene/alpha-olefin copolymer composition having a density from 0.935 to 0.955 g/cc; a ratio of weight average molecular weight to number average molecular weight, Mw/Mn, of from 3 to 10; a z-average molecular weight, Mz, from 200 kg/mol to 500 kg/mol; and a PENT value of greater than 500 hours at 80° C. and 2.4 MPa; wherein when the composition is formed into a monolayer pipe the pipe has a pipe hydrostatic strength of greater than 100 hours at 20° C. and 12.0 MPa. Also provided is a pipe or pipe fitting comprising the ethylene/alpha-olefin copolymer composition.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (I2) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min.
Abstract:
The invention provides a composition comprising a first composition, comprising at least one ethylene-based polymer, and wherein the first composition comprises a MWCDI value greater than 0.9, and a melt index ratio I10/I2 that meets the following equation: I10/I2≥7.0−1.2×log (I2). The invention also provides a process to form a composition comprising at least two ethylene-based polymers, said process comprising the following: polymerizing ethylene, and optionally at least one comonomer, in solution, in the presence of a catalyst system comprising a metal-ligand complex of Structure I, as described herein, to form a first ethylene-based polymer; and polymerizing ethylene, and optionally at least one comonomer, in the presence of a catalyst system comprising a Ziegler/Natta catalyst, to form a second ethylene-based polymer.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (12) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min.
Abstract:
The invention provides a composition comprising a first composition, comprising at least one ethylene-based polymer, and wherein the first composition comprises a MWCDI value greater than 0.9, and a melt index ratio I10/I2 that meets the following equation: I10/I2≧7.0−1.2×log (I2). The invention also provides a process to form a composition comprising at least two ethylene-based polymers, said process comprising the following: polymerizing ethylene, and optionally at least one comonomer, in solution, in the presence of a catalyst system comprising a metal-ligand complex of Structure I, as described herein, to form a first ethylene-based polymer; and polymerizing ethylene, and optionally at least one comonomer, in the presence of a catalyst system comprising a Ziegler/Natta catalyst, to form a second ethylene-based polymer.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
The instant invention provides a polyethylene blend-composition suitable for blown films, and films made therefrom. The polyethylene blend-composition suitable for blown films according to the present invention comprises the melt blending product of: (a) from 0.5 to 4 percent by weight of a low density polyethylene having a density in the range of from 0.915 to 0.935 g/cm3, and a melt index (I2) in the range of from greater than 0.8 to less than or equal to 5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 6 to 10; (b) 90 percent or greater by weight of a linear low density polyethylene composition has a density in the range of 0.900 to 0.935 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.5 to 4.5, a melt index (I2) in the range of 0.1 to 5 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 3, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition, and a zero shear viscosity ratio (ZSVR) in the range from 1 to less than 2; (c) optionally a hydrotalcite based neutralizing agent; (d) optionally one or more nucleating agents; (e) and optionally one or more antioxidants.
Abstract:
The instant invention provides a polyethylene blend-composition suitable for blown films, and films made therefrom. The polyethylene blend-composition suitable for blown films comprises the melt blending product of: (a) from 0.5 to 5 percent by weight of a high density polyethylene having a density in the range of from 0.950 to 0.970 g/cm3, and a melt flow rate (I2) in the range of from less than 0.5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 10 to 40, and Mz in the range of from 800,000 to 5,000,000 g/mol; (b) 90 percent or greater by weight of a linear low density polyethylene having a density in the range of from 0.910 to 0.950 g/cm3, and a melt index (I2) in the range of from 0.1 to less than or equal to 5 g/10 minutes; (c) optionally a hydrotalcite based neutralizing agent; (d) optionally one or more nucleating agents; (e) and optionally one or more anti-oxidants.
Abstract:
A linear low density polyethylene composition suitable for injection molding applications comprising less than or equal to 100 percent by weight of the units derived from ethylene, less than 35 percent by weight of units derived from one or more α-olefin comonomers, and characterized by its density, molecular weight distribution (Mw/Mn), a melt index (I2), a molecular weight distribution (Mz/Mw), vinyl unsaturation, and zero shear viscosity ratio (ZSVR). The linear low density polyethylene composition exhibits low hexane extractable levels.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)