Abstract:
A composite body of the present invention includes a base and an oxide layer arranged on the base, the oxide layer containing more than 45% by volume of a perovskite-type oxide phase. The composite body may include a first member, a second member, and a joining portion that joins the first member and the second member, at least one of the first member and the second member serving as the base, and the joining portion serving as the oxide layer. The composite body may include the base and a covering portion that covers the whole or part of a surface of the base, the covering portion being formed of the oxide layer.
Abstract:
A joined body 20 according to the present invention includes a first member 22 made of a porous ceramic, a second member 24 made of a metal, and a joint 30 formed of an oxide ceramic of a transition metal, the joint 30 joining the first member 22 to the second member 24. Alternatively, a joined body may include a first member made of a dense material, a second member made of a dense material, and a joint formed of an oxide ceramic of a transition metal, the joint joining the first member to the second member.
Abstract:
A silicon carbide porous body according to the present invention contains silicon carbide particles, metallic silicon, and an oxide phase, in which the silicon carbide particles are bonded together via at least one of the metallic silicon and the oxide phase. The primary component of the oxide phase is cordierite, and the open porosity is 10% to 40%. Preferably, the silicon carbide porous body contains 50% to 80% by weight of silicon carbide, 15% to 40% by weight of metallic silicon, and 1% to 25% by weight of cordierite. Preferably, the volume resistivity is 1 to 80 Ωcm, and the thermal conductivity is 30 to 70 W/m·K.
Abstract:
There is provided a positive electrode active material containing a lithium composite oxide having a layered rock salt structure containing Li, Ni, Co and Mn, and further containing at least one additive selected from Li3BO3, Li3PO4 and Li2SO4.
Abstract:
A joined body 20 includes a first member 21 which is a ceramic containing Si, a second member 22, and a joining portion 30 which is formed of an electrically conductive oxide containing a Fe3O4 phase and which joins the first member 21 and the second member 22. In the joined body 20, no reaction layer is preferably formed at a joining interface between the electrically conductive oxide and the first member 21. The joining portion 30 is preferably formed to have a multilayer structure in which from the first matter 21 to the second member 22, a first layer containing a first oxide of a transition metal, a second layer containing an electrically conductive oxide of a transition metal having a low valence as compared to that of the first oxide, and a mixed layer containing a transition metal and an oxide thereof are formed.
Abstract translation:接合体20包括:第一构件21,其是含有Si的陶瓷,第二构件22和由包含Fe 3 O 4相的导电氧化物形成并且与第一构件21和第二构件22接合的接合部30 在接合体20中,优选在导电性氧化物和第一构件21的接合界面处形成反应层。接合部30优选形成为具有从第一物质21到第二物质21的多层结构 元件22,含有过渡金属的第一氧化物的第一层,含有与第一氧化物相比具有低价态的过渡金属的导电氧化物的第二层,以及含有过渡金属和 形成氧化物。
Abstract:
A joined body 20 includes a porous ceramic 22 made of porous ceramic, a metal member 24 made of a metal, and a joint 30 formed of an oxide ceramic that penetrates into pores 23 of the porous ceramic 22 and joins the porous ceramic 22 to the metal member 24. The penetration depth of the oxide ceramic into the pores of the porous ceramic is preferably 10 μm or more, and more preferably 15 to 50 μm. The joined body 20 may be produced through a joining step of forming a joint by placing a metal raw material between a porous ceramic and a metal member and firing the metal raw material in the air at a temperature in the range of 400° C. to 900° C., where an oxide ceramic produced by oxidation of the metal raw material penetrates into the pores of the porous ceramic in the joint.
Abstract:
A composite body of the present invention includes a substrate and a forming portion which is composed of a composite phase containing a perovskite oxide and a metal oxide different from the perovskite oxide and which is formed on the substrate. This composite body may be a composite body manufactured by a manufacturing method including a forming step of firing in an oxidizing atmosphere, a laminated body in which an inorganic raw material powder containing a compound powder and a metal powder is disposed on a substrate so as to form a forming portion composed of a composite phase containing a perovskite oxide and a metal oxide different from the perovskite oxide on the substrate.
Abstract:
To provide a honeycomb structure capable of using as a catalyst carrier, which functions as a heater, and where a bonding layer is hard to break and an electrical resistance value is hard to rise; including a honeycomb segment bonded body where honeycomb segments are bonded by bonding layer, and a pair of electrode members disposed on a side surface of the bonded body, the electrode members is formed into a band shape, and in a cross section perpendicular to the cell extending direction, one electrode member is disposed on an opposite side across the center of the bonded body to another electrode member, and in at least a part of the bonding layer, inorganic fibers made of β-SiC and a metal silicide are included in a porous body where silicon carbide are bound with silicon in a state where pores are held among the particles.
Abstract:
A manufacturing method of a sintered ceramic body mixes barium silicate with aluminum oxide, a glass material, and an additive oxide to prepare a material mixture, molds the material mixture and fires the molded object. The barium silicate is monoclinic and has an average particle diameter in a range of 0.3 μm to 1 μm and a specific surface area in a range of 5 m2/g to 20 m2/g. The aluminum oxide has an average particle diameter in a range of 0.4 μm to 10 μm, a specific surface area in a range of 0.8 m2/g to 8 m2/g. A volume ratio of the aluminum oxide to the barium silicate is in a range of 10% by volume to 25% by volume.
Abstract:
A joined body 20 includes a first member 22 having a thermal expansion coefficient of 8 ppm/K or less, a second member 24 having a thermal expansion coefficient of 12 ppm/K or more, and a joining portion 30 composed of an electrically conductive oxide containing 50% by mass or more of a spinel-type ferrite phase, the joining portion 30 joining the first member and the second member. The electrically conductive oxide preferably contains Fe and element A (where element A represents one or more selected from the group consisting of Mg, Mn, Co, Ni, Cu, and Zn). The molar ratio of element A to Fe, i.e., A/Fe, is 0.5 or less.