Abstract:
Examples include a method of forming an electromagnetic shielding material, the method including: applying a magnetic field to a precursor material that includes first ferromagnetic particles embedded within a first portion of a matrix material and second ferromagnetic particles embedded within a second portion of the matrix material, thereby causing the first ferromagnetic particles and the second ferromagnetic particles to move such that longitudinal axes of the first ferromagnetic particles and the second ferromagnetic particles become more aligned with the magnetic field; thereafter forcing the first portion of the matrix material through a filter, thereby moving the first ferromagnetic particles from the first portion of the matrix material into the second portion of the matrix material; and curing the second portion of the matrix material to form the electromagnetic shielding material. Additional examples include an electromagnetic shielding material and an apparatus for forming an electromagnetic shielding material.
Abstract:
Disclosed are conductive composites comprising a polymer, a conductor selected from metals and metal alloys, a compatibilizing agent, and an optional thickening agent.
Abstract:
The present disclosure is directed to a method of making a composite part. The method comprises covering a mold tool for a composite part with a parting film. The method further comprises laying up at least one layer of pre-preg on the parting film covering the mold tool to form a laid-up composite part and removing the laid-up composite part from the parting film. The parting film comprises a polymer sheet having a first major surface and a second major surface; and a first adhesive disposed on the first major surface of the polymer sheet, the first adhesive adhering the polymer sheet to the mold tool.
Abstract:
A low viscosity polysulfide sealant composition. The composition comprises a curable polysulfide polymer; a crosslinking agent; and a plurality of core-shell particles. The core-shell particles comprise: a core comprising a ferromagnetic material; and a shell comprising silica treated with an organic sulfur containing compound. The shell is capable of bonding with the polysulfide polymer.
Abstract:
A coating includes at least one coating layer containing first particles, second particles, and third particles distributed throughout a cross-linked, continuous polymer matrix. An outer surface of the coating layer includes surfaces of at least first particles extending outward from a top periphery of the polymer matrix. The outer surface exhibits a property of delaying ice formation compared to the coating layer without the first particles. A method includes applying a coating composition in one application step. The one-step coating composition contains first particles, second particles, and third particles in a base containing a polymer. A coating composition includes first particles, second particles, and third particles distributed in a matrix precursor.
Abstract:
Methods and formulations for modified silicone resins of Formula (I) are presented: The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
Abstract:
A low viscosity polysulfide sealant composition. The composition comprises a curable polysulfide polymer; a crosslinking agent; and a plurality of core-shell particles. The core-shell particles comprise: a core comprising a ferromagnetic material; and a shell comprising silica treated with an organic sulfur containing compound. The shell is capable of bonding with the polysulfide polymer.
Abstract:
A coating includes at least one coating layer containing first particles, second particles, and third particles distributed throughout a cross-linked, continuous polymer matrix. An outer surface of the coating layer includes surfaces of at least first particles extending outward from a top periphery of the polymer matrix. The outer surface exhibits a property of delaying ice formation compared to the coating layer without the first particles. A method includes applying a coating composition in one application step. The one-step coating composition contains first particles, second particles, and third particles in a base containing a polymer. A coating composition includes first particles, second particles, and third particles distributed in a matrix precursor.
Abstract:
A composition comprising a cyclic olefin copolymer; a particulate filler dispersed in the cyclic olefin copolymer; and a solvent is disclosed. The composition can be used to make a transmissive composite. The transmissive composite and a method of making a transmissive composite panel are also disclosed.
Abstract:
There is provided a method of synthesizing and using a segmented copolymer that includes mixing one or more α,ω (alpha, omega) amine or α,ω (alpha, omega) hydroxyl terminated polysiloxane first soft segments having an average molecular weight of between about 2500 grams per mole to about 10,000 grams per mole, and one or more diisocyanate species, together to form a first reaction product; mixing the first reaction product and one or more low molecular weight diol or diamine chain extenders each having an average molecular weight of less than 400 grams per mole, together in a solvent to form a segmented copolymer in solution; and applying the segmented copolymer in solution to one or more surfaces via spray coating directly from the solution with the segmented copolymer, wherein the segmented copolymer formed has a high flexibility at an environmental temperature of down to about −100 degrees Celsius.