Method of fabricating pneumatic tire
    64.
    发明授权
    Method of fabricating pneumatic tire 有权
    充气轮胎的制造方法

    公开(公告)号:US08821664B2

    公开(公告)日:2014-09-02

    申请号:US12180622

    申请日:2008-07-28

    申请人: Norihiko Nakamura

    发明人: Norihiko Nakamura

    摘要: A pneumatic tire provided with a resin film at an outer surface of the tire side portion to be able to be exfoliated therefrom by pasting a smooth resin film having a melting point equal to or higher than 23° C., a Young's modulus equal to or larger than 2.5 GPa and a thickness of 10 through 150 μm to an outer surface of a side portion of an unvulcanized tire and vulcanizing and molding the unvulcanized tire in a state of pasting the resin film.

    摘要翻译: 一种充气轮胎,其在轮胎侧部的外表面设置有树脂膜,以能够通过粘贴熔点等于或高于23℃的光滑树脂膜,杨氏模量等于或等于或等于 大于2.5GPa,厚度为10至150μm的未硫化轮胎的侧部的外表面,并且在粘合树脂膜的状态下对未硫化轮胎进行硫化和模塑。

    Pneumatic tire
    66.
    发明授权
    Pneumatic tire 有权
    气动轮胎

    公开(公告)号:US08376005B2

    公开(公告)日:2013-02-19

    申请号:US12442969

    申请日:2007-08-07

    申请人: Norihiko Nakamura

    发明人: Norihiko Nakamura

    IPC分类号: B60C19/08 B60C1/00 B60C15/06

    摘要: A pneumatic tire that can be manufactured according to the conventional method without requiring special tire manufacturing steps and without needing addition of material members and production steps, has excellent rolling resistance and wet properties, and has conductivity. A pneumatic tire 10 has a side wall 16 contacted with a rim strip 19 of a bead part 11 and extended outward in a radial direction of a tire from the bead part 19 to be coupled to a ground contact edge region of a tread part 13, the side wall 16 comprising a two-layer structure of an internal layer rubber 27 and an outer layer rubber 26, characterized in that on the circumference of unilateral or bilateral part of the tire 10, the rim strip 19 and either the internal layer rubber 27 or the external layer rubber 26 of the side wall 16 are formed into a continuous conductive path by a conductive rubber material, only the conductive path is used as a conducting path of the tire, and members other than the conductive path are selected and used from a conductive rubber material or a nonconductive rubber material.

    摘要翻译: 可以根据现有方法制造而不需要特殊的轮胎制造步骤而不需要添加材料构件和制造步骤的充气轮胎具有优异的滚动阻力和湿润特性,并且具有导电性。 充气轮胎10具有与胎圈部11的轮辋条19接触并且从胎圈部19沿轮胎的径向向外延伸的侧壁16,以与胎面部13的接地接触边缘区域连接, 侧壁16包括内层橡胶27和外层橡胶26的两层结构,其特征在于,在轮胎10的单边或双边部分的周边上,轮缘条19和内层橡胶27 或侧壁16的外层橡胶26通过导电橡胶材料形成为连续的导电路径,仅将导电路径用作轮胎的导电路径,并且选择并使用除导电路径之外的构件 导电橡胶材料或非导电橡胶材料。

    Pneumatic tire
    67.
    发明授权
    Pneumatic tire 有权
    气动轮胎

    公开(公告)号:US08353324B2

    公开(公告)日:2013-01-15

    申请号:US12444405

    申请日:2006-10-11

    申请人: Norihiko Nakamura

    发明人: Norihiko Nakamura

    IPC分类号: B60C19/08

    摘要: A pneumatic tire that can be manufactured according to the conventional method without requiring special tire manufacturing steps and without needing addition of material members and production steps, and having excellent rolling resistance and wet properties, and having conductivity is to be provided. A pneumatic tire 10 comprises a carcass 14, a rim strip 19, and a wing 24 in which one edge thereof is contacted with the carcass 14 and the other edge thereof is exposed to the surface of a ground contact edge region of a tread part 13, wherein a carcass ply 14 contacting the rim strip 19 and the wing 24 has a conductive ply 14X and a nonconductive ply 14Y on the circumference of the tire, and the conductive ply 14X and the rim strip and the wing form a continuous conductive path comprising a conductive rubber material, only the conductive path is used as a conducting path of the tire, and members other than the conducting path are selected and used from a conductive rubber material or a nonconductive rubber material.

    摘要翻译: 可以提供可以根据常规方法制造的充气轮胎,而不需要特殊的轮胎制造步骤,并且不需要添加材料构件和制造步骤,并且具有优异的滚动阻力和湿性能,并且具有导电性。 充气轮胎10包括胎体14,轮辋条19和翼24,其中一个边缘与胎体14接触,另一个边缘暴露于胎面部13的接地边缘区域的表面 其中接触边缘带19和机翼24的胎体帘布层14在轮胎的圆周上具有导电帘布层14X和非导电帘布层14Y,并且导电层14X和轮缘条和翼形成连续导电路径,包括 导电橡胶材料,仅使用导电路径作为轮胎的导电路径,并且从导电橡胶材料或非导电橡胶材料中选择并使用导电路径以外的构件。

    AMMONIA SYNTHESIS PROCESS
    68.
    发明申请
    AMMONIA SYNTHESIS PROCESS 失效
    氨基酸合成方法

    公开(公告)号:US20110286907A1

    公开(公告)日:2011-11-24

    申请号:US13143619

    申请日:2009-12-22

    IPC分类号: C01C1/04

    摘要: The invention provides a process for efficient synthesis of ammonia. The process includes a water-splitting step in which water is decomposed to obtain a first source gas comprising hydrogen and oxygen, a first oxygen removal step in which the oxygen contained in the first source gas is at least partially separated and removed by an oxygen separating membrane or hydrogen separating membrane to obtain a second source gas having a lower oxygen concentration than the first source gas, a second oxygen removal step in which the oxygen in the second source gas is reacted with hydrogen to produce water for removal, or is adsorbed onto an adsorption medium for removal, to obtain a third source gas having a lower oxygen concentration than the second source gas, and an ammonia synthesis step in which the hydrogen in the third source gas is reacted with nitrogen to synthesize ammonia.

    摘要翻译: 本发明提供了一种有效合成氨的方法。 该方法包括水分解步骤,其中水被分解以获得包含氢和氧的第一源气体,第一氧除去步骤,其中通过氧分离将至少部分地分离和除去第一源气体中所含的氧 膜或氢分离膜,以获得具有比第一源气体低的氧浓度的第二源气体;第二氧除去步骤,其中第二源气体中的氧与氢反应以产生除去水或吸附到 用于除去的吸附介质,以获得具有比第二源气体低的氧浓度的第三源气体,以及氨合成步骤,其中第三源气体中的氢与氮反应以合成氨。

    TIN-PLATED STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME
    69.
    发明申请
    TIN-PLATED STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME 审中-公开
    镀锡钢板及其制造方法

    公开(公告)号:US20110168563A1

    公开(公告)日:2011-07-14

    申请号:US13003091

    申请日:2009-07-02

    IPC分类号: C25D11/36 C25D7/00 C25D5/10

    摘要: A tin-plated steel sheet includes a steel sheet; an Sn-containing plating layer in which the mass per unit area of Sn is 0.05 to 20 g/m2 disposed on at least one surface of the steel sheet; a first chemical conversion coating which contains P and Sn, in which the mass per unit area of P is 0.3 to 10 mg/m2, disposed on the Sn-containing plating layer; and a second chemical conversion coating which contains P and Al, in which the mass per unit area of P is 1.2 to 10 mg/m2 and the mass per unit area of Al is 0.24 to 8.7 mg/m2, disposed on the first chemical conversion coating.

    摘要翻译: 镀锡钢板包括钢板; 设置在钢板的至少一个表面上的Sn的单位面积质量为0.05〜20g / m 2的含Sn镀层; 设置在含Sn镀层上的含有P和Sn的第一化学转化膜,其中P的单位面积质量为0.3〜10mg / m 2; 以及含有P和Al的第二化学转化膜,其中P的单位面积质量为1.2〜10mg / m 2,Al的单位面积质量为0.24〜8.7mg / m 2,配置在第一化学转化 涂层。