摘要:
A treatment method includes the steps of: Providing an initial supply of an ammonium octamolybdate precursor powder having a bi-modal particle size distribution; applying a quantity of solvent to the initial supply of ammonium octamolybdate precursor powder to form a moistened intermediate powder; and allowing the moistened intermediate powder to adsorb the applied solvent over a time period, the quantity of solvent applied and the time period being sufficient to form a treated ammonium octamolybdate powder composition having a substantially uni-modal particle size distribution.
摘要:
A coated article system includes a substrate and a surface coating on the substrate. The surface coating is formed by depositing individual particles of a composite metal powder with sufficient energy to cause the composite metal powder to bond with the substrate and form the surface coating. The composite metal powder includes a substantially homogeneous dispersion of molybdenum and molybdenum disulfide sub-particles that are fused together to form the individual particles of the composite metal powder.
摘要:
Molybdenum disulfide powders include substantially spherically-shaped particles of molybdenum disulfide that are formed from agglomerations of generally flake-shaped sub-particles. The molybdenum disulfide powders are flowable and exhibit uniform densities. Methods for producing a molybdenum disulfide powder may include the steps of: Providing a supply of molybdenum disulfide precursor material; providing a supply of a liquid; providing a supply of a binder; combining the molybdenum disulfide precursor material with the liquid and the binder to form a slurry; feeding the slurry into a stream of hot gas; and recovering the molybdenum disulfide powder, the molybdenum disulfide powder including substantially spherically-shaped particles of molybdenum disulfide formed from agglomerations of generally flake-shaped sub-particles.
摘要:
A friction material composition may include an abrasive, a filler, a binder, and a spherical molybdenum disulfide powder. The spherical molybdenum disulfide powder is made up of molybdenum disulfide sub-particles that are agglomerated together to form individual, substantially spherically-shaped agglomerated particles of at least about 90% by weight molybdenum disulfide.
摘要:
A method of producing a compacted article according to one embodiment may involve the steps of: Providing a copper/molybdenum disulfide composite powder including a substantially homogeneous dispersion of copper and molybdenum disulfide sub-particles that are fused together to form individual particles of the copper/molybdenum disulfide composite powder; and compressing the copper/molybdenum disulfide composite powder under sufficient pressure to cause the copper/molybdenum disulfide composite powder to behave as a nearly solid mass.
摘要:
A method of producing a compacted article according to one embodiment may involve the steps of: Providing a copper/molybdenum disulfide composite powder including a substantially homogeneous dispersion of copper and molybdenum disulfide sub-particles that are fused together to form individual particles of the copper/molybdenum disulfide composite powder; and compressing the copper/molybdenum disulfide composite powder under sufficient pressure to cause the copper/molybdenum disulfide composite powder to behave as a nearly solid mass.
摘要:
A treatment method includes the steps of: Providing an initial supply of an ammonium octamolybdate precursor powder having a bi-modal particle size distribution; applying a quantity of solvent to the initial supply of ammonium octamolybdate precursor powder to form a moistened intermediate powder; and allowing the moistened intermediate powder to adsorb the applied solvent over a time period, the quantity of solvent applied and the time period being sufficient to form a treated ammonium octamolybdate powder composition having a substantially uni-modal particle size distribution.
摘要:
A method for producing a metal article may include: Producing a supply of a composite metal powder by: providing a supply of molybdenum metal powder; providing a supply of a sodium compound; combining the molybdenum metal powder and the sodium compound with a liquid to form a slurry; feeding the slurry into a stream of hot gas; and recovering the composite metal powder; and consolidating the composite metal powder to form the metal article, the metal article comprising a sodium/molybdenum metal matrix. Also disclosed is a metal article produced accordance with this method.
摘要:
A friction material composition may include an abrasive, a filler, a binder, and a spherical molybdenum disulfide powder. The spherical molybdenum disulfide powder is made up of molybdenum disulfide sub-particles that are agglomerated together to form individual, substantially spherically-shaped agglomerated particles of at least about 90% by weight molybdenum disulfide.
摘要:
Molybdenum disulfide powders include substantially spherically-shaped particles of molybdenum disulfide that are formed from agglomerations of generally flake-shaped sub-particles. The molybdenum disulfide powders are flowable and exhibit uniform densities. Methods for producing a molybdenum disulfide powder may include the steps of: Providing a supply of molybdenum disulfide precursor material; providing a supply of a liquid; providing a supply of a binder; combining the molybdenum disulfide precursor material with the liquid and the binder to form a slurry; feeding the slurry into a stream of hot gas; and recovering the molybdenum disulfide powder, the molybdenum disulfide powder including substantially spherically-shaped particles of molybdenum disulfide formed from agglomerations of generally flake-shaped sub-particles.