摘要:
The use of an aqueous polyurethane dispersion adhesive is described for producing biodisintegratable composite foils where at least two substrates are adhesive-bonded to one another with use of the polyurethane dispersion adhesive, where at least one of the substrates is a biodisintegrable polymer foil. At least 60% by weight of the polyurethane is composed of diisocyanates, polyesterdiols, and at least one bifunctional carboxylic acid selected from dihydroxycarboxylic acids and diaminocarboxylic acids.
摘要:
A method for producing biodisintegratable composite foils with an aqueous polyurethane dispersion adhesive. The method involves adhesive-bonding a first substrate to a second substrate with use of the aqueous polyurethane dispersion adhesive. At least one of the first substrate and the second substrate is made of a biodisintegratable polymer foil, and at least 60% by weight of the polyurethane contains diisocyanates, polyesterdiols, and bifunctional carboxylic acids. The bifunctional carboxylic acids are dihydroxycarboxylic acids or diaminocarboxylic acids.
摘要:
The invention relates to a sealing mass with low density and improved tensile strength on the basis of sulfur-containing polymers such as on the basis of polysulfide, polyether or/and polytioether that has a density of not more than 1.3 g/cm3 according to ISO 2781 and a tensile strength of at least 1.9 N/mm2 according to ISO 37 after curing. The invention further relates to a ground mass based on sulfur-containing polymers for producing a sealing mass that comprises at least one long-chain linear polymer and at least one short-chain branched polymer having a content in trifunctional molecules, or/and at least one multifunctional cross-linker with a number of functional groups n≧3. The invention further relates to a method for producing a sealing mass according to which at least one base polymer is mixed with at least one adhesion promoter and the at least one light filler, especially hollow filler, is added, a vacuum with a remaining pressure of less than 50 mbar being maintained during incorporation of the light filler.
摘要翻译:本发明涉及一种基于含硫聚合物,例如基于多硫化物,聚醚或/和聚氧乙烯醚的密度不超过1.3g / cm 2的低密度和改进的拉伸强度的密封块, 3和根据ISO 37固化后的抗拉强度至少为1.9N / mm 2。 本发明还涉及一种基于含硫聚合物的研磨物质,用于生产包含至少一种长链线性聚合物和至少一种具有三官能分子含量的至少一种短链支化聚合物的密封块,或至少 一个具有多个官能团n> = 3的多功能交联剂。 本发明还涉及一种用于生产密封块的方法,根据该方法,将至少一种基础聚合物与至少一种粘合促进剂混合,并加入至少一种轻填料,特别是中空填料, 在掺入轻填料的过程中维持小于50毫巴。
摘要:
An adhesive comprising a polymer obtainable by free-radical addition polymerization of ethylenically unsaturated compounds (monomers) and synthesized from at least 60% by weight of principal monomers selected from C1 to C20 alkyl (meth)acrylates, vinyl esters of carboxylic acids containing up to 20 carbon atoms, vinylaromatics having up to 20 carbon atoms, ethylenically unsaturated nitrites, vinyl halides, vinyl ethers of alcohols containing 1 to 10 carbon atoms, aliphatic hydrocarbons having 2 to 4 carbon atoms and one or two double bonds, and mixtures of these monomers, and from more than 1% by weight of monomers containing at least two nonconjugated polymerizable vinyl groups.
摘要:
Described is paper or cardboard packaging produced from mineral oil contaminated, recycled paper, wherein the packaging includes a barrier layer obtainable by applying an aqueous polymeric dispersion comprising a copolymer obtainable by emulsion polymerization of C1-C4 alkyl(meth)acrylates, acid monomers, e.g., acrylic acid or methacrylic acid, 0-20 wt % of acrylonitrile and 0 to 10 wt % of further monomers, wherein the glass transition temperature of the copolymer is in the range from +10 to +45° C. The barrier layer may be situated on one of the surfaces of the packaging or form one of multiple layers of a multilayered packaging coating or be situated as a coating on one side of an inner bag situated within the packaging.
摘要:
A pressure-sensitive adhesive comprising a polymer obtainable by free-radical polymerization and synthesized from a) 70% to 99% by weight of n-butyl acrylate b) 1% to 30% by weight of ethylhexyl acrylate c) 0 to 5% by weight of an ethylenically unsaturated acid d) 0 to 20% by weight of at least one further monomer, for which vinyl acetate is excluded.
摘要:
Paper or cardboard packaging produced from recycled paper contaminated by mineral oil, where the packaging includes a barrier layer obtained by applying an aqueous polymeric dispersion containing a mixture of at least two polymers A and B. Polymer A is obtained by emulsion polymerization of C1-C4 alkyl(meth)acrylates, acid monomers, e.g., acrylic acid or methacrylic acid, 0-20 wt % of acrylonitrile and 0-10 wt % of further monomers, where the glass transition temperature of copolymer A is greater than +45° C. and the glass transition temperature of polymer B is less than +10° C. The mean value calculated from the glass transition temperatures of the individual polymers is +10 to +45° C. The barrier layer may be situated on one of the surfaces of the packaging or form one of multiple layers of a multilayered packaging coating or be situated as a coating on one side of an inner bag situated within the packaging.
摘要:
The use of polyelectrolyte complexes is described, for providing an oxygen barrier to packaging materials made of polymer foils. Polymeric components of the polyelectrolyte complex are applied in polymerized form to the polymer foil. The polymer foil is either coated with an aqueous dispersion comprising a dispersed polyelectrolyte complex previously produced by water-in-water emulsion polymerization, or is coated with a composition comprising a polyelectrolyte complex produced from anionic polymer and from cationic surfactant, or the polymer foil is coated with at least three alternating layers, where respectively one of two adjacent layers comprises an anionic polyelectrolyte component and the other of two adjacent layers comprises a cationic polyelectrolyte component, and polyelectrolyte complexes form at the opposite, adjacent interfaces of the alternating layers.
摘要:
An adhesive comprising A) a polymer obtainable by free-radical addition polymerization and synthesized from at least 60% by weight of principal monomers selected from C1 to C20 alkyl(meth)acrylates, vinyl esters of carboxylic acids containing up to 20 carbon atoms, vinylaromatics having up to 20 carbon atoms, ethylenically unsaturated nitriles, vinyl halides, vinyl ethers of alcohols containing 1 to 10 carbon atoms, aliphatic hydrocarbons having 2 to 8 carbon atoms and one or two double bonds, and mixtures of these monomers, and B) an aminotriazine resin.
摘要:
A pressure sensitive adhesive comprising an aqueous dispersion of a polymer, said dispersion comprising, besides the polymer, silicon compounds selected from polymeric silicates, water-soluble alkali metal silicates (waterglass), silanes, and silicones obtainable from the silanes by condensation.