摘要:
A method of production of dielectric powder containing as main ingredients Ti, Cu, and Ni, comprising a step of mixing an oxide of Ti and/or a compound forming an oxide of Ti by firing, an oxide of Cu and/or a compound forming an oxide of Cu by firing, and an oxide of Ni and/or a compound forming an oxide of Ni by firing to obtain a mixed powder, a step of calcining the mixed powder to obtain a calcined powder, a step of dry crushing the calcined powder to obtain dry crushed powder, and a step of wet crushing the dry crushed powder.
摘要:
A nickel-basis ferrite material, a sulfur content of ferrite powder in a raw material stage is in a range of from 300 ppm to 900 ppm on S basis and a chlorine content of the ferrite powder is not higher than 100 ppm on Cl basis, while a sulfur content of a ferrite sinter after burning is not higher than 100 ppm on S basis and a chlorine content of the ferrite sinter is not higher than 25 ppm on Cl basis. Furthermore, a ferrite material is constituted by an Ni ferrite material using a nickel compound as a raw material, the nickel compound having a specific surface area in a range of from 1.0 m2/g to 10 m2/g and a sulfur content in a range of from 100 ppm to 1,000 ppm on S basis.
摘要:
A ferrite composition includes a main component having 46.0 to 49.8 mol % of an iron oxide in terms of Fe2O3, 5.0 to 14.0 mol % of a copper oxide in terms of CuO and 8.0 to 32.0 mol % of a zinc oxide in terms of ZnO, and a remainder of the main component is composed of a nickel oxide; and as subcomponents, with respect to 100 wt % of the main component, 0.5 to 6.0 wt % of a silicon oxide in terms of SiO2 and 0.01 to 2.0 wt % of a boron oxide in terms of B2O3. Further, as a subcomponent, 0.01 to 0.17 wt % of potassium oxide in terms of K2O or 0.3 to 2.0 wt % of tin oxide in terms of SnO2 may be included.
摘要翻译:铁氧体组合物包括以Fe 2 O 3计的氧化铁为46.0〜49.8摩尔%,CuO为5.0〜14.0摩尔%的氧化铜,以ZnO计为8.0〜32.0摩尔%的氧化锌的主成分, 主要成分的剩余部分由氧化镍构成; 作为副成分,相对于100重量%的主成分,以SiO 2计为0.5〜6.0重量%的氧化硅,以B 2 O 3换算为0.01〜2.0重量%的氧化硼。 此外,作为副成分,可以包括以K 2 O计的氧化锡为0.01〜0.17重量%,以SnO 2为0.3〜2.0重量%的氧化锡。
摘要:
A dielectric ceramic composition comprises as a main component, Cu oxide, Si oxide and one selected from the group consisting of Zn oxide alone and a combination of Mg oxide and Zn oxide, as a subcomponent, a glass component including B oxide and at least one selected from the group consisting of Si oxide, Ba oxide, Ca oxide, Sr oxide, Li oxide and Zn oxide, and having a glass softening point is 750° C. or less, wherein a content of said glass component is 1.5 to 15 wt % with respect to 100 wt % of said main component. According to the present invention, a dielectric ceramic composition can be provided which is available to be sintered at low temperature (for example, 950° C. or lower) while comparatively decreasing contents of a glass component, which shows good properties (specific permittivity, loss Q value and insulation resistance), and which is available to perform cofiring different materials.
摘要:
A multilayer inductor component has a multilayer part having a plurality of magnetic layers laminated therein and a conductor part arranged within the multilayer part. The magnetic layers are formed from a ferrite material and an additive. The ferrite material contains Fe2O3, NiO, CuO, and ZnO. Fe2O3 is 30 to 45 mol %. NiO is 45 to 58 mol %. CuO is 6 to 10 mol %. ZnO is 0 to 3 mol %. The additive contains CoO. The content of CoO is 0.1 to 2.5 mass % with respect to the ferrite material as a whole. The multilayer inductor component has an impedance peak of 500 Ω or greater at an operating frequency of 1 GHz or higher.
摘要翻译:多层电感器部件具有层叠有多个磁性层的多层部分和布置在多层部分内的导体部分。 磁性层由铁素体材料和添加剂形成。 铁氧体材料含有Fe2O3,NiO,CuO和ZnO。 Fe 2 O 3为30〜45摩尔%。 NiO为45〜58摩尔%。 CuO为6〜10摩尔%。 ZnO为0〜3摩尔%。 添加剂含有CoO。 CoO的含量相对于铁素体材料整体为0.1〜2.5质量%。 多层电感器组件在1GHz或更高的工作频率下具有500Ω或更大的阻抗峰值。
摘要:
The present invention relates to a dielectric ceramic composition comprising a main component including at least one selected from barium titanate, strontium titanate and calcium titanate, and as a subcomponent, a glass component including an oxide of B, wherein a content of said glass component is 2 to 7 wt % with respect to 100 wt % of said main component. According to the present invention, there are provided a dielectric ceramic composition wherein a layer can be made thinner by relatively decreasing a content of the glass component, etc., as well as having good properties (specific permittivity, loss Q value and insulation resistance), and a complex electronic device such as a multilayer filter or a multilayer ceramic capacitor, which has a dielectric layer composed of the dielectric ceramic composition.
摘要:
A dielectric ceramic composition comprises as a main component, Cu oxide, Si oxide and one selected from the group consisting of Zn oxide alone and a combination of Mg oxide and Zn oxide, as a subcomponent, a glass component including B oxide and at least one selected from the group consisting of Si oxide, Ba oxide, Ca oxide, Sr oxide, Li oxide and Zn oxide, and having a glass softening point is 750° C. or less, wherein a content of said glass component is 1.5 to 15 wt % with respect to 100 wt % of said main component.According to the present invention, a dielectric ceramic composition can be provided which is available to be sintered at low temperature (for example, 950° C. or lower) while comparatively decreasing contents of a glass component, which shows good properties (specific permittivity, loss Q value and insulation resistance), and which is available to perform cofiring different materials.
摘要:
The present invention relates to a dielectric ceramic composition comprising a main component including at least one selected from barium titanate, strontium titanate and calcium titanate, and as a subcomponent, a glass component including an oxide of B, wherein a content of said glass component is 2 to 7 wt % with respect to 100 wt % of said main component. According to the present invention, there are provided a dielectric ceramic composition wherein a layer can be made thinner by relatively decreasing a content of the glass component, etc., as well as having good properties (specific permittivity, loss Q value and insulation resistance), and a complex electronic device such as a multilayer filter or a multilayer ceramic capacitor, which has a dielectric layer composed of the dielectric ceramic composition.
摘要:
In an inductor including a magnetic core on a top surface of a terminal table, a plurality of L-shaped conductors are inserted into the terminal table so that two ends of each of the L-shaped conductors are projecting from a side surface of the terminal table. The plurality of L-shaped conductors each have at least one stepped portion. One of the two ends which is on a higher level than the stepped portion acts as a winding terminal around which the wire is wound, and the other end which is on a lower level than the stepped portion acts as a mounting terminal used for mounting of the inductor. The winding terminal is projecting from a higher level of the side surface of the terminal table than the mounting terminal.
摘要:
For example, the reflector according to the present invention is a reflector made of glass for a projector which is composed of amorphous glass whose thermal expansion coefficient is 30 to 45×10−7/° C. and includes a reflective surface for reflecting light emitted from a light source and an opening for inserting a light source bulb or a conductor to the light source bulb, in which the opening is smoothed by heat-treating the surface thereof after opening-drilling, thus mechanical damage is removed from the processed part.