Method for recycling enzyme
    3.
    发明申请
    Method for recycling enzyme 有权
    回收酶的方法

    公开(公告)号:US20120070874A1

    公开(公告)日:2012-03-22

    申请号:US13137050

    申请日:2011-07-18

    IPC分类号: C12N9/96

    摘要: In saccharification of cellulose, chimeric β-glucosidase having a region exhibiting thermophilic bacteria-derived β-glucosidase activity and a module combinable to cellulose is used along with cellulosome, and at the completion of saccharification of cellulose, a cellulosic substrate is added to make the chimeric β-glucosidase and cellulosome attach to the cellulosic substrate for separation.

    摘要翻译: 在纤维素的糖化中,具有表现出嗜热细菌衍生的葡萄糖苷酶活性的区域的嵌合和葡糖苷酶以及可与纤维素组合的模块与纤维素体一起使用,并且在纤维素糖化完成时,将纤维素底物加入 使嵌合的β-葡糖苷酶和纤维素体附着到纤维素基质上进行分离。

    DIELECTRIC CERAMIC AND DIELECTRIC FILTER UTILIZING SAME
    4.
    发明申请
    DIELECTRIC CERAMIC AND DIELECTRIC FILTER UTILIZING SAME 审中-公开
    电介质陶瓷和电介质过滤器

    公开(公告)号:US20130127568A1

    公开(公告)日:2013-05-23

    申请号:US13813077

    申请日:2011-07-29

    IPC分类号: H01L41/09

    摘要: A dielectric ceramic includes a main crystal phase containing Ba, Nd and Ti; and a remainder, part of Ti contained in the main crystal phase being substituted with Al, a content of the Al contained in the main crystal phase to a total content of Al in the main crystal phase and the remainder being greater than or equal to 10% on Al2O3 basis. Accordingly, provided is a dielectric ceramic having a high relative permittivity ∈r, a high Qf value and a stable resonant-frequency temperature coefficient τf close to 0 ppm/° C. Also provided is a dielectric filter which is provided with the dielectric ceramic and in which a desired relative permittivity can be obtained with stability and a high Qf value can be obtained, and excellent performance capability can be maintained for a long period of time with stability in a place where wide temperature variations are encountered.

    摘要翻译: 电介质陶瓷包括含有Ba,Nd和Ti的主晶相; 剩下的是,主晶相中包含的部分Ti被Al取代,主晶相中包含的Al的含量相对于主晶相中的Al的总含量,余量大于或等于10 %Al2O3。 因此,提供了一种具有高相对介电常数Er,高Qf值和接近0ppm /℃的稳定谐振频率温度系数tauf的电介质陶瓷。还提供了一种介质滤波器,其设置有电介质陶瓷,并且 可以稳定地获得期望的相对介电常数,并且可以获得高Qf值,并且在遇到宽温度变化的地方具有稳定性的情况下可以长期保持优异的性能。

    Humidity-conditioning sheet
    5.
    发明授权
    Humidity-conditioning sheet 有权
    湿度调节片

    公开(公告)号:US08404032B2

    公开(公告)日:2013-03-26

    申请号:US12517370

    申请日:2007-12-10

    IPC分类号: B01D53/02

    摘要: A humidity-conditioning sheet 10 excellent in reversibility and responsiveness of a moisture adsorbing/desorbing ability of rapidly adsorbing moisture at high ambient humidity and conversely rapidly desorbing adsorbed moisture at low ambient humidity includes a sheet-shaped humidity-conditioning layer 7 formed by bonding together, with a thermoplastic resin powder 4, humidity-conditioning particles 3 which reversibly adsorb and desorb water vapor. The void ratio of the humidity-conditioning layer 7 is 5% or more. Since a ratio of voids 8 formed between the humidity-conditioning particles 3 is high, the voids 8 between the humidity-conditioning particles 3 can be used as water retention spaces for moisture adsorption and desorption, thereby achieving the high reversible moisture adsorbing/desorbing ability and excellent moisture adsorption/desorption responsiveness with the aid of not only the moisture adsorbing/desorbing ability inherent in the humidity-conditioning particles but also the moisture adsorbing/desorbing ability of the voids between the humidity-conditioning particles.

    摘要翻译: 在高环境湿度下快速吸附水分的水分吸附/解吸能力的可逆性和响应性优异的湿度调节片10,并且相反地在低环境湿度下快速解吸吸附的水分包括通过粘合在一起形成的片状调湿层7 ,热塑性树脂粉末4,可逆地吸附和解吸水蒸气的调湿颗粒3。 调湿层7的空隙率为5%以上。 由于调湿颗粒3之间形成的空隙8的比率高,所以调湿颗粒3之间的空隙8可以用作水分吸附和解吸的保水空间,从而获得高可逆的吸湿/解吸能力 并且借助于不仅调湿颗粒中固有的水分吸附/解吸能力以及调湿颗粒之间的空隙的水分吸附/解吸能力而具有优异的吸湿/解吸响应性。

    Semiconductor light emitting device member, method for manufacturing such semiconductor light emitting device member and semiconductor light emitting device using such semiconductor light emitting device member
    7.
    发明授权
    Semiconductor light emitting device member, method for manufacturing such semiconductor light emitting device member and semiconductor light emitting device using such semiconductor light emitting device member 有权
    半导体发光器件部件,这种半导体发光器件部件的制造方法和使用这种半导体发光器件的半导体发光器件

    公开(公告)号:US07859006B2

    公开(公告)日:2010-12-28

    申请号:US11816640

    申请日:2006-02-23

    IPC分类号: H01L33/00

    摘要: A semiconductor light-emitting device member excellent in transparency, light resistance, and heat resistance and capable of sealing a semiconductor light-emitting device without causing cracks and peeling even after a long-time use is provided wherein the semiconductor light-emitting device member contains (A) in a solid Si-nuclear magnetic resonance spectrum, at least one peak selected from (a) peaks whose peak top position is in an area of a chemical shift of −40 ppm to 0 ppm inclusive, and whose full width at half maximum is 0.3 ppm to 3.0 ppm inclusive, and (b) peaks whose peak top position is in an area of the chemical shift of −80 ppm or more and less than −40 ppm, and whose full width at half maximum is 0.3 ppm to 5.0 ppm inclusive, wherein (B) silicon content is 20 weight % or more and (C) silanol content is 0.1 weight % to 10 weight % inclusive.

    摘要翻译: 提供透明性,耐光性和耐热性优异的半导体发光元件,即使长时间使用也能够密封半导体发光元件而不引起裂纹和剥离的半导体发光元件,其中半导体发光元件 (A)在固体Si核磁共振谱中,至少一个峰选自(a)峰顶位置在-40ppm至0ppm的化学位移范围内的峰,并且其全宽为一半 最大值为0.3ppm〜3.0ppm,(b)峰顶位置在-80ppm以上且小于-40ppm的化学位移范围内,峰值全宽度为0.3ppm〜 5.0ppm,其中(B)硅含量为20重量%以上,(C)硅烷醇含量为0.1重量%〜10重量%。

    COATING COMPOSITION, METHOD FOR MAKING THE SAME, RESIN FORMING PRODUCT, AND METHOD FOR MAKING THE RESIN FORMING PRODUCT
    8.
    发明申请
    COATING COMPOSITION, METHOD FOR MAKING THE SAME, RESIN FORMING PRODUCT, AND METHOD FOR MAKING THE RESIN FORMING PRODUCT 审中-公开
    涂料组合物,其制备方法,树脂形成产品和制备树脂形成产品的方法

    公开(公告)号:US20100189993A1

    公开(公告)日:2010-07-29

    申请号:US11993710

    申请日:2006-06-26

    IPC分类号: B32B3/26 C08K7/26

    摘要: A coating composition excellent in coating characteristics and/or appearance of the coated surface is provided. The composition can provide a resin forming product excellent in dew condensation resistance, moisture conditioning effect, anti-fouling effect, cooling effect (moisture-releasing cooling effect, moisture-releasing endothermic properties), and/or endurance.The coating composition includes at least an inorganic porous material, a binder resin, and a solvent, wherein (1) the inorganic porous material contains at least one silicon compound; (2) the binder resin has (a) a solid hydroxyl value in the range of 5 mgKOH/g to 80 mgKOH/g and (b) a glass transition temperature (Tg) in the range of −5° C. to 40° C.; and (3) the solvent contains at least one organic solvent.

    摘要翻译: 提供涂布表面的涂布特性和/或外观优异的涂料组合物。 该组合物可以提供耐结露性,湿度调节效果,防污效果,冷却效果(除湿降温效果,吸湿释放性))和/或耐久性优异的树脂形成品。 涂料组合物至少包括无机多孔材料,粘合剂树脂和溶剂,其中(1)无机多孔材料含有至少一种硅化合物; (2)粘合剂树脂具有(a)5mgKOH / g至80mgKOH / g范围内的固体羟基值和(b)-5℃至40℃范围内的玻璃化转变温度(Tg) C。; 和(3)溶剂含有至少一种有机溶剂。

    (Meth)acrylic film, and making film and receptor sheet using the same
    9.
    发明授权
    (Meth)acrylic film, and making film and receptor sheet using the same 有权
    (甲基)丙烯酸膜,并使用其制造膜和受体片

    公开(公告)号:US07691948B2

    公开(公告)日:2010-04-06

    申请号:US10569113

    申请日:2004-09-09

    摘要: To provide a film having high tensile strength and elongation characteristics. A methacrylic film formed of (A) a carboxyl group-containing (meth)acrylic polymer having a glass transition temperature (Tg) of 0° C. or higher and a weight-average molecular weight of 10,000 or more obtained by copolymerizing a composition containing a monoethylenically unsaturated monomer as a main component and an unsaturated monomer having a carboxyl group, and (B) an amino group-containing (meth)acrylic polymer having a glass transition temperature (Tg) of 0° C. or lower and a weight-average molecular weight of 10,000 or more obtained by copolymerizing a composition containing a monoethylenically unsaturated monomer as a main component and an unsaturated monomer having an amino group, wherein a mixing ratio of the component (A) to the component (B) is from 10:90 to 90:10 in terms of a weight ratio.

    摘要翻译: 提供具有高拉伸强度和伸长特性的薄膜。 由(A)具有玻璃化转变温度(Tg)为0℃以上的含羧基(甲基)丙烯酸系聚合物,重均分子量为10000以上的甲基丙烯酸系膜形成的共聚物,其含有 作为主要成分的单烯属不饱和单体和具有羧基的不饱和单体,(B)玻璃化转变温度(Tg)为0℃以下的含氨基(甲基)丙烯酸系聚合物, 通过共聚含有单烯属不饱和单体作为主要成分的组合物和具有氨基的不饱和单体得到的平均分子量为10,000以上,其中,成分(A)与成分(B)的混合比例为10: 90〜90:10。

    HUMIDITY-CONDITIONING SHEET
    10.
    发明申请
    HUMIDITY-CONDITIONING SHEET 有权
    湿度调节表

    公开(公告)号:US20100005968A1

    公开(公告)日:2010-01-14

    申请号:US12517370

    申请日:2007-12-10

    IPC分类号: B01D53/02 B01D53/22

    摘要: A humidity-conditioning sheet 10 excellent in reversibility and responsiveness of a moisture adsorbing/desorbing ability of rapidly adsorbing moisture at high ambient humidity and conversely rapidly desorbing adsorbed moisture at low ambient humidity includes a sheet-shaped humidity-conditioning layer 7 formed by bonding together, with a thermoplastic resin powder 4, humidity-conditioning particles 3 which reversibly adsorb and desorb water vapor. The void ratio of the humidity-conditioning layer 7 is 5% or more. Since a ratio of voids 8 formed between the humidity-conditioning particles 3 is high, the voids 8 between the humidity-conditioning particles 3 can be used as water retention spaces for moisture adsorption and desorption, thereby achieving the high reversible moisture adsorbing/desorbing ability and excellent moisture adsorption/desorption responsiveness with the aid of not only the moisture adsorbing/desorbing ability inherent in the humidity-conditioning particles but also the moisture adsorbing/desorbing ability of the voids between the humidity-conditioning particles.

    摘要翻译: 在高环境湿度下快速吸附水分的水分吸附/解吸能力的可逆性和响应性优异的湿度调节片10,并且相反地在低环境湿度下快速解吸吸附的水分包括通过粘合在一起形成的片状调湿层7 ,热塑性树脂粉末4,可逆地吸附和解吸水蒸气的调湿颗粒3。 调湿层7的空隙率为5%以上。 由于调湿颗粒3之间形成的空隙8的比率高,所以调湿颗粒3之间的空隙8可以用作水分吸附和解吸的保水空间,从而获得高可逆的吸湿/解吸能力 并且借助于不仅调湿颗粒中固有的水分吸附/解吸能力以及调湿颗粒之间的空隙的水分吸附/解吸能力而具有优异的吸湿/解吸响应性。