Sheet metal member, method of manufacturing same, and heat radiation
plate
    1.
    发明授权
    Sheet metal member, method of manufacturing same, and heat radiation plate 失效
    钣金件,其制造方法和散热板

    公开(公告)号:US6139975A

    公开(公告)日:2000-10-31

    申请号:US230494

    申请日:1999-01-26

    摘要: In a method of manufacturing a sheet member comprising: obtaining a sintered compact by sintering a sheet-like compact having a reduced-thickness portion and an enlarged-thickness portion; and then repressing the sintered compact into a sheet member, a difference in density between the reduced-thickness portion and the enlarged-thickness portion of the sintered compact after repressing is adjusted to be in a range of .+-.1.5%. By doing so, the accuracy of flatness is enhanced and the amount of distortion, which would otherwise remain in the sheet member, is reduced because the sheet member is formed by sintering the sheet-like compact. In addition, the deformation caused by heating is greatly restricted. Accordingly, the prospect of the sheet member of the present invention is bright as a heat dissipating plate.

    摘要翻译: PCT No.PCT / JP98 / 02591 Sec。 371日期1999年1月26日 102(e)日期1999年1月26日PCT提交1998年6月12日PCT公布。 第WO98 / 56526号公报 日期:1998年12月17日在制造片材的方法中,包括:通过烧结具有厚度减小的部分和扩大厚度部分的片状压块来获得烧结体; 然后将烧结体压制成片状部件,将压制后的烧结体的厚度减薄部与扩大部分的密度差调整为±1.5%的范围。 通过这样做,由于片材通过烧结片状压块而形成,因此平坦度的精度提高,否则残留在片状构件中的变形量减少。 此外,加热引起的变形受到很大限制。 因此,作为散热板,本发明的片材的前景是明亮的。

    Process for producing connecting rod
    4.
    发明授权
    Process for producing connecting rod 失效
    连杆生产工艺

    公开(公告)号:US5905939A

    公开(公告)日:1999-05-18

    申请号:US888010

    申请日:1997-07-03

    摘要: There is provided a connecting rod including a connecting rod body and a cap having excellent alignment properties, and a method of producing such a connecting rod. A connecting rod body and a cap are produced through the steps of molding green compacts respectively corresponding to the connecting rod body and the cap; sintering and unifying both the green compacts; forging the resultant sintered product in a mold; and fracturing the resultant forged product. The green compact corresponding to the cap and/or the green compact corresponding to the connecting rod body includes opposite circumferential end faces formed with one or more projection. A clearance c is formed between both circumferential end faces of the sintered product due to the projection. With this clearance c, both the circumferential end faces are formed with recesses and projections which are fitted to each other during the forging process and which are relatively large and thus have large biting amounts. During the fracturing process, the recesses and the projections are separated into two pieces.

    摘要翻译: 提供了一种连杆,包括具有优良对准性能的连杆主体和盖,以及制造这种连杆的方法。 通过分别对应于连杆主体和盖的成型压坯的步骤来制造连杆体和盖, 烧结并统一生坯; 将所得烧结产品锻造在模具中; 并破碎所得的锻造产品。 对应于与连杆主体相对应的盖和/或生坯的生坯具有形成有一个或多个突起的相对的周向端面。 由于突起,在烧结体的两个周向端面之间形成有间隙c。 利用该间隙c,两个周向端面形成有在锻造过程中彼此相配合并且相对较大并因此具有大的咬入量的凹部和突起。 在压裂过程中,凹槽和突起被分成两部分。

    Forming die assembly for microcomponents
    6.
    发明授权
    Forming die assembly for microcomponents 有权
    微型组件模具组装

    公开(公告)号:US09492867B2

    公开(公告)日:2016-11-15

    申请号:US13279759

    申请日:2011-10-24

    CPC分类号: B22F3/03 B30B11/02 B30B15/302

    摘要: A forming die assembly for microcomponents includes a forming die and a punch. The forming die is formed with a cavity, a punch hole connected to the cavity, and a supply path for supplying a raw material with a metal powder and a binder having plasticity. The supply path is connected to the cavity so as to have a gate therebetween and is used for supplying the raw material into the cavity. The punch is slidably inserted into the punch hole, and it opens and closes the gate by reciprocatory sliding. The punch closes the gate and compresses the raw material in the cavity into a green compact by sliding in the direction of the cavity.

    摘要翻译: 用于微型部件的成型模具组件包括成形模具和冲头。 成形模具形成有空腔,连接到空腔的冲孔和用于向原材料供应金属粉末和具有可塑性的粘合剂的供给路径。 供给路径连接到空腔,以便在其间具有栅极,并且用于将原料供应到空腔中。 冲头可滑动地插入冲孔,并且通过往复滑动打开和关闭门。 打孔器关闭门,并通过沿空腔的方向滑动将空腔中的原料压缩成绿色压块。

    Production method for fluid dynamic pressure sintered bearing
    7.
    发明申请
    Production method for fluid dynamic pressure sintered bearing 审中-公开
    流体动压烧结轴承的生产方法

    公开(公告)号:US20070212248A1

    公开(公告)日:2007-09-13

    申请号:US11709802

    申请日:2007-02-23

    IPC分类号: B22F3/24

    摘要: A production method for a fluid dynamic pressure sintered bearing includes: preparing a sintered bearing having a porosity of 8 to 20 vol % as a material; and controlling at least one of an overall length, an outer diameter, and an inner diameter of the sintered bearing by repressing the sintered bearing. The production method further includes: forming grooves for generating a fluid dynamic pressure on a bearing surface of the sintered bearing by performing repressing and plastic working on the sintered bearing; and sealing pores exposed on the bearing surface by infiltrating a resin into at least the pores; and barreling entire surface of the sintered bearing by magnetic barreling or electromagnetic barreling.

    摘要翻译: 一种流体动态压力烧结轴承的制造方法,其特征在于,具有:制作孔隙率为8〜20体积%的烧结轴承作为材料; 以及通过压制所述烧结轴承来控制所述烧结轴承的总长度,外径和内径中的至少一个。 该制造方法还包括:通过在烧结轴承上进行压制和塑性加工,形成用于在烧结轴承的支承表面上产生流体动压的槽; 以及通过将树脂渗透到至少孔中来密封暴露在轴承表面上的孔; 并通过磁力滚筒或电磁滚筒来滚动烧结轴承的整个表面。

    Forming die assembly for microcomponents
    8.
    发明授权
    Forming die assembly for microcomponents 有权
    微型组件模具组装

    公开(公告)号:US08851872B2

    公开(公告)日:2014-10-07

    申请号:US13279839

    申请日:2011-10-24

    摘要: A forming die assembly for microcomponents includes a forming die, a plunger, and a punch. The forming die is formed with a cavity, a storage portion for storing a raw material with a metal powder and a binder having plasticity, and a punch hole that connects the cavity and the storage portion so as to form a gate therebetween. The plunger is formed so as to be slidably inserted into the storage portion and to fill the raw material stored in the storage portion into the cavity through the punch hole. The punch is slidably inserted into the plunger in the sliding direction of the plunger and opens and closes the gate by reciprocatory sliding. The punch closes the gate and compresses the raw material in the cavity into a green compact by sliding in the direction of the cavity.

    摘要翻译: 用于微型部件的成型模具组件包括成型模具,柱塞和冲头。 成形模具形成有空腔,用于存储具有金属粉末的原材料和具有可塑性的粘合剂的存储部分,以及连接空腔和存储部分以在其间形成闸门的冲孔。 柱塞被形成为可滑动地插入存储部分中,并且通过冲孔将存储在存储部分中的原料填充到空腔中。 冲头在柱塞的滑动方向上可滑动地插入柱塞中,并通过往复运动打开和关闭门。 打孔器关闭门,并通过沿空腔的方向滑动将空腔中的原料压缩成绿色压块。

    THERMOELECTRIC CONVERTING MODULE AND MANUFACTURING METHOD THEREOF
    9.
    发明申请
    THERMOELECTRIC CONVERTING MODULE AND MANUFACTURING METHOD THEREOF 审中-公开
    热电转换模块及其制造方法

    公开(公告)号:US20130061901A1

    公开(公告)日:2013-03-14

    申请号:US13606418

    申请日:2012-09-07

    IPC分类号: H01L35/32 H01L35/14 H01L35/34

    CPC分类号: H01L35/08 H01L35/22

    摘要: Provided is a high temperature thermoelectric converting module including a plurality of p type thermoelectric elements; a plurality of n type thermoelectric elements; a plurality of electrodes; and a lead line. The plurality of p type thermoelectric elements, the plurality of n type thermoelectric elements, and the plurality of electrodes are electrically serially connected to each other, a pair of connecting lines that connects the lead line to one of the plurality of electrodes to output to the outside is further included, at least one electrode which is disposed at the high temperature side and the plurality of p type and n type thermoelectric elements are bonded with an intermediate layer therebetween. The plurality of p type and n type thermoelectric elements contain silicon as a component and the intermediate layer is formed as a layer containing aluminum and silicon and components other than silicon of the thermoelectric elements.

    摘要翻译: 提供一种包括多个p型热电元件的高温热电转换模块; 多个n型热电元件; 多个电极; 和引导线。 多个p型热电元件,多个n型热电元件和多个电极彼此电连接,一对连接线,其将引线连接到多个电极中的一个以输出到 还包括外部,设置在高温侧的至少一个电极和多个p型和n型热电元件在其间具有中间层。 多个p型和n型热电元件含有硅作为组分,并且中间层形成为含有铝和硅的层以及除了热电元件的硅以外的成分。

    Production method of electrode for cold cathode fluorescent lamp
    10.
    发明授权
    Production method of electrode for cold cathode fluorescent lamp 失效
    冷阴极荧光灯电极的制作方法

    公开(公告)号:US07666348B2

    公开(公告)日:2010-02-23

    申请号:US11429178

    申请日:2006-05-08

    IPC分类号: B22F3/12

    摘要: A production method includes: preparing a metal powder composed of one of Mo and W, and a binder composed of a thermoplastic resin and a wax; mixing the metal powder and 40 to 60 volume % of the binder with respect to the metal powder into a mixed powder; and heating and kneading the mixed powder into a raw material. The production method further includes: supplying a predetermined of the raw material in a hole of a die; and compacting the raw material into a cup-shaped green compact by pressing the raw material by a punch, the cup-shaped green compact having a cylindrical portion, a bottom formed at one end portion thereof, and an opening formed at another end portion thereof. The production method further includes: ejecting the cup-shaped green compact from the hole of the die; removing the binder from the ejected cup-shaped green compact by heating; and sintering the cup-shaped green compact by heating the green compact and diffusion-bonding particles of the green compact.