公开(公告)号:US08859703B2
公开(公告)日:2014-10-14
申请号:US13338304
申请日:2011-12-28
申请人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
发明人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
IPC分类号: C08F10/02 , B29C47/00 , C08F10/00 , C08F210/16 , C08F110/02
CPC分类号: C08F10/00 , B29C47/92 , B29C2947/922 , B29C2947/924 , B29C2947/92514 , B29C2947/92542 , B29C2947/92695 , B29C2947/92714 , B29C2947/92895 , C08F10/02 , C08F110/02 , C08F210/16 , C08F2400/02 , C08F4/6567 , C08F4/6557 , C08F2/001 , C08F2500/07 , C08F2500/05 , C08F2500/12 , C08F210/08
摘要: Disclosed is a bimodal Ziegler-Natta catalyzed polyethylene, having a density of from 0.930 g/cc to 0.960 g/cc, and a molecular weight distribution of from 10 to 25, wherein an article formed therefrom has a PENT of at least 1500. Also disclosed is a method of preparing a tubular article including obtaining a bimodal polyethylene having a density of from 0.930 g/cc to 0.960 g/cc and a molecular weight distribution of from 10 to 25, and processing the polyethylene under conditions where a specific energy input (SEI) is less than 300 kW·h/ton, and wherein the article has a PENT of at least 1500. Further disclosed is a method for controlling the degradation of polyethylene including polymerizing ethylene monomer, recovering polyethylene, extruding the polyethylene, and controlling the degradation of polyethylene by measuring the SEI to the extruder and adjusting throughput and/or gear suction pressure keep SEI less than 300 kW·h/ton, and forming an article.
摘要翻译: 公开了一种双峰型齐格勒 - 纳塔催化聚乙烯,其密度为0.930g / cc至0.960g / cc,分子量分布为10至25,其中由其形成的制品具有至少1500的PENT。另外 公开了一种制备管状制品的方法,包括获得密度为0.930g / cc至0.960g / cc和分子量分布为10至25的双峰聚乙烯,并在特定能量输入条件下处理聚乙烯 (SEI)小于300kW·h / ton,其中制品的PENT为至少1500.另外公开了一种控制聚乙烯降解的方法,包括聚合乙烯单体,回收聚乙烯,挤出聚乙烯,控制 通过测量SEI到挤出机并调整产量和/或齿轮吸入压力,聚乙烯的降解使SEI小于300kW·h / ton,形成物品。
-
公开(公告)号:US20120091621A1
公开(公告)日:2012-04-19
申请号:US13338304
申请日:2011-12-28
申请人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
发明人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
CPC分类号: C08F10/00 , B29C47/92 , B29C2947/922 , B29C2947/924 , B29C2947/92514 , B29C2947/92542 , B29C2947/92695 , B29C2947/92714 , B29C2947/92895 , C08F10/02 , C08F110/02 , C08F210/16 , C08F2400/02 , C08F4/6567 , C08F4/6557 , C08F2/001 , C08F2500/07 , C08F2500/05 , C08F2500/12 , C08F210/08
摘要: Disclosed is a bimodal Ziegler-Natta catalyzed polyethylene, having a density of from 0.930 glee to 0.960 glee, and a molecular weight distribution of from 10 to 25, wherein an article formed therefrom has a PENT of at least 1500. Also disclosed is a method of preparing a tubular article including obtaining a bimodal polyethylene having a density of from 0.930 glee to 0.960 Wee and a molecular weight distribution of from 10 to 25, and processing the polyethylene under conditions where a specific energy input (SET) is less than 300 kW.h/ton, and wherein the article has a PENT of at least 1500. Further disclosed is a method for controlling the degradation of polyethylene including polymerizing ethylene monomer, recovering polyethylene, extruding the polyethylene, and controlling the degradation of polyethylene by measuring the SEI to the extruder and adjusting throughput and/or gear suction pressure keep SEI less than 300 kW.h/ton, and forming an article.
摘要翻译: 公开了一种双峰型齐格勒 - 纳塔催化聚乙烯,其密度为0.930gle-0.960glee,分子量分布为10-25,其中由其形成的制品具有至少为1500的PENT。还公开了一种方法 制备管状制品,包括获得密度为0.930glee至0.960ee的分子量分布为10至25的双峰聚乙烯,并且在比能量输入(SET)小于300kW的条件下处理聚乙烯 h / ton,并且其中制品具有至少1500的PENT。还公开了一种控制聚乙烯降解的方法,包括聚合乙烯单体,回收聚乙烯,挤出聚乙烯,并通过测量SEI来控制聚乙烯的降解 到挤出机并调节产量和/或齿轮吸入压力使SEI小于300kW.h / ton,并形成物品。
-
公开(公告)号:US20100267909A1
公开(公告)日:2010-10-21
申请号:US12777553
申请日:2010-05-11
申请人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
发明人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian B. Cole , Stan Biesert , Vincent Barre , Ruby L. Curtis , Son Nguyen , Danielle Childress
IPC分类号: C08F4/50 , C08F110/02 , C08F4/42
CPC分类号: C08F10/00 , B29C47/92 , B29C2947/922 , B29C2947/924 , B29C2947/92514 , B29C2947/92542 , B29C2947/92695 , B29C2947/92714 , B29C2947/92895 , C08F10/02 , C08F110/02 , C08F210/16 , C08F2400/02 , C08F4/6567 , C08F4/6557 , C08F2/001 , C08F2500/07 , C08F2500/05 , C08F2500/12 , C08F210/08
摘要: Disclosed is a bimodal Ziegler-Natta catalyzed polyethylene, having a density of from 0.930 g/cc to 0.960 g/cc, and a molecular weight distribution of from 10 to 25, wherein an article formed therefrom has a PENT of at least 1500. Also disclosed is a method of preparing a tubular article including obtaining a bimodal polyethylene having a density of from 0.930 g/cc to 0.960 g/cc and a molecular weight distribution of from 10 to 25, and processing the polyethylene under conditions where a specific energy input (SEI) is less than 300 kW·h/ton, and wherein the article has a PENT of at least 1500. Further disclosed is a method for controlling the degradation of polyethylene including polymerizing ethylene monomer, recovering polyethylene, extruding the polyethylene, and controlling the degradation of polyethylene by measuring the SEI to the extruder and adjusting throughput and/or gear suction pressure keep SEI less than 300 kW·h/ton, and forming an article.
摘要翻译: 公开了一种双峰型齐格勒 - 纳塔催化聚乙烯,其密度为0.930g / cc至0.960g / cc,分子量分布为10至25,其中由其形成的制品具有至少1500的PENT。另外 公开了一种制备管状制品的方法,包括获得密度为0.930g / cc至0.960g / cc和分子量分布为10至25的双峰聚乙烯,并在特定能量输入条件下处理聚乙烯 (SEI)小于300kW·h / ton,其中制品的PENT为至少1500.另外公开了一种控制聚乙烯降解的方法,包括聚合乙烯单体,回收聚乙烯,挤出聚乙烯,控制 通过测量SEI到挤出机并调整产量和/或齿轮吸入压力,聚乙烯的降解使SEI小于300kW·h / ton,形成物品。
-
公开(公告)号:US08110644B2
公开(公告)日:2012-02-07
申请号:US12777553
申请日:2010-05-11
申请人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian Cole , Stan Biesert , Vincent Barre , Ruby Curtis , Son Nguyen , Danielle Childress
发明人: Tim Coffy , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian Cole , Stan Biesert , Vincent Barre , Ruby Curtis , Son Nguyen , Danielle Childress
IPC分类号: C08F110/02 , C08F4/42
CPC分类号: C08F10/00 , B29C47/92 , B29C2947/922 , B29C2947/924 , B29C2947/92514 , B29C2947/92542 , B29C2947/92695 , B29C2947/92714 , B29C2947/92895 , C08F10/02 , C08F110/02 , C08F210/16 , C08F2400/02 , C08F4/6567 , C08F4/6557 , C08F2/001 , C08F2500/07 , C08F2500/05 , C08F2500/12 , C08F210/08
摘要: Disclosed is a bimodal Ziegler-Natta catalyzed polyethylene, having a density of from 0.930 g/cc to 0.960 g/cc, and a molecular weight distribution of from 10 to 25, wherein an article formed therefrom has a PENT of at least 1500. Also disclosed is a method of preparing a tubular article including obtaining a bimodal polyethylene having a density of from 0.930 g/cc to 0.960 g/cc and a molecular weight distribution of from 10 to 25, and processing the polyethylene under conditions where a specific energy input (SEI) is less than 300 kW·h/ton, and wherein the article has a PENT of at least 1500. Further disclosed is a method for controlling the degradation of polyethylene including polymerizing ethylene monomer, recovering polyethylene, extruding the polyethylene, and controlling the degradation of polyethylene by measuring the SEI to the extruder and adjusting throughput and/or gear suction pressure keep SEI less than 300 kW·h/ton, and forming an article.
摘要翻译: 公开了一种双峰型齐格勒 - 纳塔催化聚乙烯,其密度为0.930g / cc至0.960g / cc,分子量分布为10至25,其中由其形成的制品具有至少1500的PENT。另外 公开了一种制备管状制品的方法,包括获得密度为0.930g / cc至0.960g / cc和分子量分布为10至25的双峰聚乙烯,并在特定能量输入条件下处理聚乙烯 (SEI)小于300kW·h / ton,其中制品的PENT为至少1500.另外公开了一种控制聚乙烯降解的方法,包括聚合乙烯单体,回收聚乙烯,挤出聚乙烯,控制 通过测量SEI到挤出机并调整产量和/或齿轮吸入压力,聚乙烯的降解使SEI小于300kW·h / ton,形成物品。
-
公开(公告)号:US20080051538A1
公开(公告)日:2008-02-28
申请号:US11774255
申请日:2007-07-06
申请人: TIM COFFY , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian Cole , Stan Beisert , Vincent Barre , Ruby Curtis , Son Nguyen , Danielle Childress
发明人: TIM COFFY , Steven Gray , David Knoeppel , Cyril Chevillard , David Rauscher , Carlos Corleto , Gerhard Guenther , Brian Cole , Stan Beisert , Vincent Barre , Ruby Curtis , Son Nguyen , Danielle Childress
IPC分类号: C08F4/52
CPC分类号: C08F10/00 , B29C48/92 , B29C2948/922 , B29C2948/924 , B29C2948/92514 , B29C2948/92542 , B29C2948/92695 , B29C2948/92714 , B29C2948/92895 , C08F10/02 , C08F110/02 , C08F210/16 , C08F2400/02 , C08F4/6567 , C08F4/6557 , C08F2/001 , C08F2500/07 , C08F2500/05 , C08F2500/12 , C08F210/08
摘要: Disclosed is a bimodal Ziegler-Natta catalyzed polyethylene, having a density of from 0.930 g/cc to 0.960 g/cc, and a molecular weight distribution of from 10 to 25, wherein an article formed therefrom has a PENT of at least 1500. Also disclosed is a method of preparing a tubular article including obtaining a bimodal polyethylene having a density of from 0.930 g/cc to 0.960 g/cc and a molecular weight distribution of from 10 to 25, and processing the polyethylene under conditions where a specific energy input (SEI) is less than 300 kW.h/ton, and wherein the article has a PENT of at least 1500. Further disclosed is a method for controlling the degradation of polyethylene including polymerizing ethylene monomer, recovering polyethylene, extruding the polyethylene, and controlling the degradation of polyethylene by measuring the SEI to the extruder and adjusting throughput and/or gear suction pressure keep SEI less than 300 kW.h/ton, and forming an article.
摘要翻译: 公开了一种双峰型齐格勒 - 纳塔催化聚乙烯,其密度为0.930g / cc至0.960g / cc,分子量分布为10至25,其中由其形成的制品具有至少1500的PENT。另外 公开了一种制备管状制品的方法,包括获得密度为0.930g / cc至0.960g / cc和分子量分布为10至25的双峰聚乙烯,并在特定能量输入条件下处理聚乙烯 (SEI)小于300kW.h / ton,并且其中该制品具有至少1500的PENT。还公开了一种控制聚乙烯降解的方法,包括聚合乙烯单体,回收聚乙烯,挤出聚乙烯和控制 通过测量SEI到挤出机并调节产量和/或齿轮吸入压力,聚乙烯的降解使SEI小于300kW.h / ton,形成物品。
-
公开(公告)号:US20070007681A1
公开(公告)日:2007-01-11
申请号:US11267984
申请日:2005-11-07
申请人: Cyril Chevillard , Son Nguyen , Gerhard Guenther , Vincent Barre
发明人: Cyril Chevillard , Son Nguyen , Gerhard Guenther , Vincent Barre
IPC分类号: B29C45/76
CPC分类号: B29C48/10 , B29C48/18 , B29C48/92 , B29C49/04 , B29C2948/92047 , B29C2948/922 , B29C2948/92314 , B29K2023/06 , B29K2023/0625 , B29K2023/0633 , B29K2023/0641 , B29K2023/065 , B29K2105/0008 , B29K2105/0032 , B29K2105/0044 , B29K2105/005
摘要: Improving polyethylene film properties may be accomplished by measuring the specific energy input (SEI) to the extruder and then adjusting a process parameter in response to a change in the SEI and/or by introducing both a free radical initiator and an alkali earth metal stearate into the polymerization. Alternatively or in addition thereto, selecting the optimum free radical initiator for a particular polyethylene resin polymerized in the presence of a selected catalyst between two resin properties may be accomplished by examining the ratio of: % variation in a first property % variation in a second property of polyethylene resins individually made with each free radical initiator under consideration. The free radical initiator may be oxygen, peroxides, peroxyketals, peroxyesters, and/or dialkyl peroxides.
-
公开(公告)号:US20070007680A1
公开(公告)日:2007-01-11
申请号:US11174815
申请日:2005-07-05
IPC分类号: B29C45/76
CPC分类号: B29C48/10 , B29C48/18 , B29C48/92 , B29C49/04 , B29C2948/92047 , B29C2948/922 , B29C2948/92314 , B29K2023/06 , B29K2023/0625 , B29K2023/0633 , B29K2023/0641 , B29K2023/065 , B29K2105/0008 , B29K2105/0032 , B29K2105/0044 , B29K2105/005
摘要: The rheology of polyethylene resin may be controlled by measuring the specific energy input (SEI) to the extruder and then adjusting a process parameter in response to a change in the SEI and/or by introducing both a free radical initiator and an alkali earth metal stearate into the polymerization. Indeed, the process parameter changed in response to the SEI measurement may be adjusting the proportion of free radical initiator, adjusting the proportion of alkali earth metal stearate, or both. The free radical initiator may be a peroxide, and the alkali earth metal stearate may be calcium stearate.
摘要翻译: 聚乙烯树脂的流变学可以通过测量挤出机的比能量输入(SEI)来控制,然后响应于SEI的变化调整工艺参数和/或通过引入自由基引发剂和碱土金属硬脂酸酯 进入聚合。 实际上,响应于SEI测量而改变的工艺参数可以调节自由基引发剂的比例,调节硬脂酸碱土金属的比例,或两者。 自由基引发剂可以是过氧化物,碱土金属硬脂酸酯可以是硬脂酸钙。
-
公开(公告)号:US20160373394A1
公开(公告)日:2016-12-22
申请号:US15257604
申请日:2016-09-06
申请人: G. Roger Lee , Son Nguyen , Beau F. Mersereau , John A. Dragseth
发明人: G. Roger Lee , Son Nguyen , Beau F. Mersereau , John A. Dragseth
CPC分类号: H04L51/22 , G06F3/04842 , G06F16/93 , G06Q10/00
摘要: A computer-implemented document management method is discussed. The method includes displaying in a messaging application a plurality of folders for storing electronic mail messages, analyzing content one or more of the electronic mail messages to locate identifiers associated with matters in a document management system, and generating a user-selectable object that, when selected, automatically causes the generation of a document management display for a user of the messaging application.
摘要翻译: 讨论了计算机实现的文档管理方法。 该方法包括在消息应用程序中显示用于存储电子邮件消息的多个文件夹,分析内容中的一个或多个电子邮件消息以定位与文档管理系统中的事项相关联的标识符,以及生成用户可选择的对象, 自动导致为消息应用程序的用户生成文档管理显示。
-
公开(公告)号:US08720476B2
公开(公告)日:2014-05-13
申请号:US12848547
申请日:2010-08-02
申请人: Tan Lee , Son Nguyen , Dung Tran , Scott Lee
发明人: Tan Lee , Son Nguyen , Dung Tran , Scott Lee
IPC分类号: B25B27/24
CPC分类号: E21B33/061 , E21B33/062 , Y10T137/6109
摘要: An apparatus for engaging and moving a ram block. In some embodiments, the apparatus, or ram block changer, includes a support bracket coupled to a blowout preventer and an articulated arm releasably coupled to the ram block. The ram block changer may further include a pivot coupling assembly having a first axis of rotation. The pivot coupling assembly extends through the support bracket and the articulated arm, wherein the articulated arm is rotatable about the first axis of rotation relative to the support bracket. The articulated arm may include a first member receiving the pivot coupling assembly therethrough, a second member coupled to the ram block, and a second pivot coupling assembly having a second axis of rotation spaced apart from the first axis of rotation and extending through the first and second members. The second member is rotatable about the second axis of rotation relative to the first member.
摘要翻译: 一种用于接合和移动冲压块的装置。 在一些实施例中,装置或压头块更换器包括联接到防喷器和可释放地联接到压头块的铰接臂的支撑支架。 压头块更换器还可以包括具有第一旋转轴线的枢转联接组件。 枢转联接组件延伸穿过支撑托架和铰接臂,其中铰接臂相对于支撑托架绕第一旋转轴线旋转。 所述铰接臂可以包括接收通过其的枢转联接组件的第一构件,联接到所述滑块的第二构件和第二枢转联接组件,所述第二枢转联接组件具有与所述第一旋转轴线间隔开的第二旋转轴线并延伸穿过所述第一和 第二名成员 第二构件可相对于第一构件围绕第二旋转轴线旋转。
-
公开(公告)号:US08598898B2
公开(公告)日:2013-12-03
申请号:US12898528
申请日:2010-10-05
申请人: Chinsong Sul , Min-Kyu Kim , Son Nguyen
发明人: Chinsong Sul , Min-Kyu Kim , Son Nguyen
IPC分类号: G01R31/3187
CPC分类号: G01R31/31716
摘要: Embodiments of the invention are generally directed to testing of high-speed input-output devices. An embodiment of a high-speed input-output apparatus includes a transmitter and a receiver, and a loop-back connection from an output of the transmitter to an input of the receiver, the loop-back connection including a first connector and a second connector for transmission of differential signals. The apparatus further includes a first inductor having a first terminal and a second terminal and second inductor having a first terminal and a second terminal, the first terminal of the first inductor being connected to the first connector and the first terminal of the second inductor being connected to the second connector, the second terminal of the first inductor and the second terminal of the second inductor providing a test access port for direct current testing of the apparatus.
摘要翻译: 本发明的实施例通常涉及高速输入 - 输出设备的测试。 高速输入输出设备的实施例包括发射器和接收器以及从发射器的输出到接收器的输入的环回连接,所述环回连接包括第一连接器和第二连接器 用于传输差分信号。 该装置还包括具有第一端子和第二端子的第一电感器和具有第一端子和第二端子的第二电感器,第一电感器的第一端子连接到第一连接器,并且第二电感器的第一端子被连接 到第二连接器,第一电感器的第二端子和第二电感器的第二端子提供用于设备的直流测试的测试访问端口。
-
-
-
-
-
-
-
-
-