摘要:
An internal gear manufacturing method capable of manufacturing time reduction and easy core removal, and a metallic glass internal gear manufactured thereby. A carbon core formed into a shape of an external gear is arranged in a thin, long tubular mold of a length equal thereto with a space extending longitudinally therealong. A molten metal material is pressure-injected under a temperature higher than a melting point thereof into the space between the mold and the core. The molten metal material is resolidified by rapid cooling at or above a critical cooling rate thereof together with the mold and the core. After resolidification of the molten metal material, the core is removed by pulverization or dissolution. Along internal gear formed of the resolidified metal material is cut into a plurality of segments of a prescribed length.
摘要:
An internal gear manufacturing method capable of manufacturing time reduction and easy core removal, and a metallic glass internal gear manufactured thereby. A carbon core formed into a shape of an external gear is arranged in a thin, long tubular mold of a length equal thereto with a space extending longitudinally therealong. A molten metal material is pressure-injected under a temperature higher than a melting point thereof into the space between the mold and the core. The molten metal material is resolidified by rapid cooling at or above a critical cooling rate thereof together with the mold and the core. After resolidification of the molten metal material, the core is removed by pulverization or dissolution. Along internal gear formed of the resolidified metal material is cut into a plurality of segments of a prescribed length.
摘要:
A metal-made high-precision gear and a gear mechanism are disclosed. The precision gear is made of a novel material which does not exist in conventional materials for precision gears, including resins and tool steels, has high hardness, strength and excellent surface smoothness, and is superior in workability. In the precision gear which is formed of an amorphous metal alloy having a ternary, quaternary or higher composition containing iron group elements, such as Fe, Co, Ni, and Cu, Ti, Zr, Hf, as the principal elements, the precision gear whose module is 0.2 or less is made of the amorphous metal alloy having a disordered structure which does not have a fixed regularity and whose XRD pattern is a halo pattern, namely exhibits a broad peak.
摘要:
A metallic material containing both a second constituent and a third constituent having positive and negative heats of mixing relative to a first constituent, respectively, and including a compound, an alloy or a nonequilibrium alloy having a melting point that is higher than the solidifying point of a metal bath made of the first constituent is placed in the metal bath. The metal bath is controlled to a temperature lower than a minimum value of a liquidus temperature within a range of compositional variations in which the amount of the third constituent in the metallic material decreases down to a point where the metallic material becomes substantially the second constituent so that the third constituent is selectively dissolved into the metal bath.
摘要:
A sputtering target for producing a metallic glass membrane characterized in comprising a structure obtained by sintering atomized powder having a composition of a ternary compound system or greater with at least one or more metal elements selected from Pd, Zr, Fe, Co, Cu and Ni as its main component (component of greatest atomic %), and being an average grain size of 50 μm or less. The prepared metallic glass membrane can be used as a substitute for conventional high-cost bulk metallic glass obtained by quenching of molten metal. This sputtering target for producing the metallic glass membrane is also free from problems such as defects in the metallic glass membrane and unevenness of composition, has a uniform structure, can be produced efficiently and at low cost, and does not generate many nodules or particles. Further provided is a method for manufacturing such a sputtering target for forming the metallic glass membrane.
摘要:
An arc melting furnace apparatus is provided which reduces an operation burden on a worker and shortens working hours. An arc melting furnace apparatus 1 includes a housing 2 having formed therein a melting chamber 2a, a hearth 4 provided within the melting chamber 2a and having a recessed portion 4a, and a heating mechanism 10 for heating and melting a metal material supplied into the recessed portion 4 to generate an alloy ingot. The apparatus comprises a turning member 23 rotatably supported on a supporting member 21 standing within the melting chamber 2a, a perimeter edge of the turning member 23 rotating and moving along the inner surface of the recessed portion 4a to lift the alloy ingot generated in the recessed portion 4a above the hearth 4 and turn it over, and a resilient turn-over assisting member 24 provided above an upper end of the recessed portion 4a. Further, the turn-over assisting member 24 is arranged to flex by a predetermined amount when the alloy ingot abuts it, and to return to its original state from the flexed state so that the alloy ingot is urged to drop into the recessed portion 4a.
摘要:
A magnetic recording medium 1 includes a substrate 11; and a metallic glassy layer 12 that is arranged on the substrate 11 and has a plurality of convex portions 12A and concave portions 12B. The metallic glassy layer 12 has a chemical composition represented by any one of the formulae (1) to (3): FemPtnSixByPz (wherein, 20
摘要:
A method of coloring a surface of a zirconium-based metallic glass component that includes the step of imparting interference colors by carrying out an anodizing process using an alkaline solution to form a film having a thickness of 300 nm or less on the surface of the zirconium-based metallic glass component.
摘要:
A sputtering target for producing a metallic glass membrane characterized in comprising a structure obtained by sintering atomized powder having a composition of a ternary compound system or greater with at least one or more metal elements selected from Pd, Zr, Fe, Co, Cu and Ni as its main component (component of greatest atomic %), and being an average grain size of 50 μm or less. The prepared metallic glass membrane can be used as a substitute for conventional high-cost bulk metallic glass obtained by quenching of molten metal. This sputtering target for producing the metallic glass membrane is also free from problems such as defects in the metallic glass membrane and unevenness of composition, has a uniform structure, can be produced efficiently and at low cost, and does not generate many nodules or particles. Further provided is a method for manufacturing such a sputtering target for forming the metallic glass membrane.
摘要:
An aluminum base alloy is produced by supercooling a molten alloy composed mainly of aluminum. The molten alloy contains an element capable of forming a quasicrystalline phase, an element which aids formation of the quasicrystals, and an element which stabilizes a supercooled state of the molten alloy and delays crystallization of a crystalline phase, and is composed of a mixed composition of a fine amorphous phase and an aluminum crystalline phase or an aluminum supersaturated solid solution phase, or a single phase of only an amorphous phase.