METHODS OF USING BIOBASED LATEX BINDERS FOR IMPROVED PRINTING PERFORMANCE
    1.
    发明申请
    METHODS OF USING BIOBASED LATEX BINDERS FOR IMPROVED PRINTING PERFORMANCE 有权
    使用生物化的LATEX粘合剂改进印刷性能的方法

    公开(公告)号:US20120263894A1

    公开(公告)日:2012-10-18

    申请号:US13514635

    申请日:2010-12-17

    IPC分类号: B32B27/10 B41M5/52

    摘要: The invention therefore provides a method of improving print performance in a paper product comprising applying a coating composition comprising (i) a pigment and (ii) a starch dispersion of discrete crosslinked native starch particles in an aqueous liquid, wherein the particle size of the starch particles in the starch dispersion ranges from about 40 nm to about 400 μm, to the paper product, wherein the print performance of the paper product is improved. In one embodiment, the coating composition comprises a solids content of from 5 to about 75% weight and comprises (i) about 100 parts by weight of pigment, and (ii) about 1 to about 300 parts by weight of starch, all based on dry weight.

    摘要翻译: 因此,本发明提供了一种提高纸产品印刷性能的方法,包括涂覆一种涂料组合物,该涂料组合物包含(i)颜料和(ii)在水性液体中的离散交联天然淀粉颗粒的淀粉分散体,其中淀粉的粒度 淀粉分散体中的颗粒的范围为约40nm至约400μm,其中纸产品的印刷性能得到改善。 在一个实施方案中,涂料组合物包含5至约75重量%的固体含量,并包含(i)约100重量份的颜料,和(ii)约1至约300重量份的淀粉,全部基于 净重。

    Antistatic gloves and process for making same
    5.
    发明申请
    Antistatic gloves and process for making same 审中-公开
    防静电手套及其制作方法

    公开(公告)号:US20080306200A1

    公开(公告)日:2008-12-11

    申请号:US11811641

    申请日:2007-06-11

    IPC分类号: C08G71/04 C08K3/22 C08K3/30

    摘要: The present invention is directed to antistatic elastomeric articles and methods of making the same. The articles can be single layered or multilayered. The single layered articles possess desirable antistatic properties and desirable properties of comfort and feel. The multilayered articles have an outermost layer/surface that possesses desirable antistatic properties and an innermost layer/surface that exhibits desirable properties of comfort and feel. In preferred embodiments, the elastomeric articles are made form a nitrile/natural rubber blend. Articles of the present invention have antistatic properties measured as having a surface resistivity below about 1014 Ω/sq and a static decay time of less than about 60 seconds.

    摘要翻译: 本发明涉及抗静电弹性体制品及其制备方法。 文章可以是单层或多层。 单层制品具有理想的抗静电性能和舒适感的理想特性。 多层制品具有具有所需抗静电性能的最外层/表面和表现出所需舒适性和感觉性质的最内层/表面。 在优选的实施方案中,弹性制品由腈/天然橡胶共混物制成。 本发明的制品具有测量为具有低于约1014Ω/ sq的表面电阻率和小于约60秒的静态衰减时间的抗静电性能。