High performance kraft facing for fiberglass insulation
    5.
    发明申请
    High performance kraft facing for fiberglass insulation 审中-公开
    高性能牛皮纸面对玻璃纤维绝缘

    公开(公告)号:US20020182964A1

    公开(公告)日:2002-12-05

    申请号:US09867260

    申请日:2001-05-29

    发明人: James G. Snyder

    IPC分类号: B32B015/14

    摘要: A process for preparing a fiberglass insulation product, including the steps of: (a) providing a layer of kraft paper, (b) coating the kraft paper layer with from 2 to 10 pounds of HDPE or of polypropylene per 3000 square feet of the paper to form an HDPE-kraft laminate or a polypropylene-kraft laminate, (c) coating the HDPE-kraft or polypropylene-kraft laminate with from 3 to 10 pounds of LDPE per 3000 square feet of the HDPE-kraft laminate or polypropylene-kraft laminate to form an LDPE-HDPE-kraft laminate or an LDPE-polypropylene-kraft laminate, (d) adjusting the temperature of the LDPE-HDPE-kraft laminate or the LDPE-polypropylene-kraft laminate so that the LDPE becomes tacky while the HDPE or polypropylene remains solid, (e) providing a layer of fiberglass wool, and (f) contacting the LDPE layer of the LDPE-HDPE-kraft laminate or of the LDPE-polypropylene-kraft laminate with the fiberglass wool layer with pressure and cooling to bond the LDPE-HDPE-kraft laminate or LDPE-polypropylene-kraft laminate to the fiberglass wool layer to form a fiberglass insulation product.

    摘要翻译: 一种制备玻璃纤维绝缘产品的方法,包括以下步骤:(a)提供一层牛皮纸,(b)用每1000平方英尺纸张2至10磅HDPE或聚丙烯涂覆牛皮纸层 以形成HDPE-牛皮纸层压板或聚丙烯 - 牛皮纸层压材料,(c)用每1000平方英尺HDPE-牛皮纸层压板或聚丙烯 - 牛皮纸层压材料的3至10磅LDPE涂覆HDPE-牛皮纸或聚丙烯 - 牛皮纸层压板 以形成LDPE-HDPE-牛皮纸层压板或LDPE-聚丙烯 - 牛皮纸层压板,(d)调节LDPE-HDPE-牛皮纸层压板或LDPE-聚丙烯 - 牛皮纸层压板的温度,使得LDPE变粘,而HDPE或 聚丙烯保持固体,(e)提供一层玻璃纤维羊毛,和(f)将LDPE-HDPE-牛皮纸层压板或LDPE-聚丙烯 - 牛皮纸层压板的LDPE层与玻璃纤维棉绒层接触,压力和冷却键合 LDPE-HDPE-牛皮纸层压板或LDPE-聚丙基 将牛皮纸层压到玻璃纤维羊毛层以形成玻璃纤维绝缘产品。

    Nb3Ga multifilamentary superconducting wire and process for preparing the same
    8.
    发明申请
    Nb3Ga multifilamentary superconducting wire and process for preparing the same 失效
    Nb3Ga复丝超导线及其制备方法

    公开(公告)号:US20040028886A1

    公开(公告)日:2004-02-12

    申请号:US10397198

    申请日:2003-03-27

    摘要: By rapidly heating a precursor wire having a multifilamentary structure in which multiple composite cores in which a composite compound of an NbnullGa compound and Nb is embedded in Nb are embedded in Nb, Ta, Nb-base alloy or Tabase alloy as a matrix material to a temperature range of 1400 to 2100null C. in 2 seconds, quenching the precursor wire at a rate of 5000null C./second or larger, and subjecting the precursor wire to additional heat treatment at a temperature range of 600 to 850null C. for 1 to 400 hours, a superconducting wire having a multifilamentary structure in which multiple composite cores in which a composite compound containing Nb3Ga of a stoichiometric composition embedded in Nb are embedded in Nb, Ta, Nb-base alloy or Tabase alloy as a matrix material is obtained.