Abstract:
Described is a polyethylene composition comprising at least one polyethylene having a crystallinity of less than 60, or 55, or 50% and within a range from 0.2 wt % to 15 wt % of cyclic-olefin copolymer and within a range from 0.2 wt % to 15 wt % of hydrocarbon resin, by weight of the polyethylene composition. The polyethylene compositions can be formed into useful articles such as films and injection molded and thermoformed articles.
Abstract:
A functionalized polyolefin and a tire tread composition comprising the functionalized polyolefin is described. The functionalized polyolefin comprises a vinyl/vinylidene-terminated polyolefin in which the vinyl/vinylidene terminus is functionalized with an alkoxysilane or an alkylsilane and optionally having ether, hydroxyl and/or amine functionality. The invention is also directed to the synthesis of vinyl/vinylidene-terminated polyolefins, functionalization at the vinyl/vinylidene terminus with an alkoxysilane or an alkylsilane and optionally having ether, hydroxyl and/or amine functionality.
Abstract:
A polymer obtained by a solution polymerization process comprising within a range from 0.5 to 20 wt % of cyclic olefin derived units, within a range from 0 wt % to 15 wt % C4 to C12 α-olefin derived units, the remainder being ethylene derived units; and having a Mw/Mn of less than 2.5; a weight average molecular weight (Mw) within a range from 80,000 to 300,000 g/mole; and a g′ value of greater than 0.95. The polymer may be formed in a solution polymerization process comprising combining in a solution cyclic olefins, ethylene, hydrogen and optionally C4 to C12 α-olefins with a single-site catalyst to form the polymer, wherein the single-site catalyst is most preferably selected from unsymmetrical Group 4 bis-bridged cyclopentadienyl metallocenes.
Abstract:
A tire tread composition is disclosed. The tire tread composition includes components, by weight of the composition, within the range from: 5 to 75 wt % of a diene elastomer; 0 to 40 wt % of processing oil; 20 to 80 wt % of filler; a curative agent; and 5 to 30 wt % of a propylene-ethylene-diene terpolymer containing from 2 wt % to 40 wt % of ethylene and/or C4-C20 α-olefins derived units, from 0.5 to 10 wt % of diene derived units, and having a heat of fusion, as determined by DSC, of from 0 J/g to 80 J/g.
Abstract:
A polyolefin-polybutadiene block-copolymer and a tire tread composition comprising the polyolefin-polybutadiene block-copolymer, the composition comprising, by weight of the composition, within the range from 15 to 60 wt % of a styrenic copolymer, processing oil, filler, a curative agent, and from 4 to 20 wt % of a polyolefin-polybutadiene block-copolymer, wherein the polyolefin-polybutadiene block-copolymer is a block copolymer having the general formula PO-XL-fPB; where “PO” is a polyolefin block having a weight average molecular weight within the range from 1000 to 150,000 g/mole, the “fPB” is a functionalized polar polybutadiene block having a weight average molecular weight within the range from 500 to 30,000 g/mole, and “XL” is a cross-linking moiety that covalently links the PO and fPB blocks; and wherein the maximum Energy Loss (Tangent Delta) of the immiscible polyolefin domain is a temperature within the range from −30° C. to 10° C.
Abstract:
A graft copolymer comprising polyolefin and engineering thermoplastic components, wherein the thermoplastic component is a polymer comprising heteroatoms or heteroatom containing moieties in its backbone and phenyl or substituted phenyl groups, the polyolefin component covalently bound to the engineering thermoplastic component. The graft copolymer is the reaction product of an engineering thermoplastic having at least one phenylene in the polymer backbone, and a vinyl/vinylidene terminated polyolefin having a weight average molecular weight of at least 300 g/mole, wherein the vinyl/vinylidene terminated polyolefin is selected from polyethylenes, polypropylenes, ethylene-propylene copolymers, polyisobutylenes, polydienes, propylene-based elastomers, ethylene-based plastomers, and combinations thereof.
Abstract:
Disclosed herein is a method to stabilize a poly(arylene ether) comprising combining a neat or diluted poly(arylene ether) with a vinyl or vinylidene-terminated polyolefin at a temperature of at least 80° C. to form heated reaction components; combining a Brφnsted acid or Lewis acid with the heated reaction components; and isolating a polyolefin-poly(arylene ether) copolymer composition.
Abstract:
Rubber compounds may comprise: an epoxidized polypentenamer rubber (CPR) and/or a hydrolyzed epoxidized CPR; and a filler comprising silica particles. One nonlimiting example is rubber compound comprising: phr to 90 phr of a styrene-butadiene rubber (SBR), a natural rubber (NR), and/or a butadiene rubber (BR); 10 phr to 50 phr of a epoxidized CPR and/or a hydrolyzed epoxidized CPR; and 10 phr to 200 phr of a filler comprising silica particles, wherein the SBR, the NR, the BR, the epoxidized CPR, and the hydrolyzed epoxidized CPR combined equal 100 parts. Rubber compounds comprising epoxidized CPR and/or a hydrolyzed epoxidized CPR; and a filler comprising silica particles may be useful in tire compositions.
Abstract:
A film, preferably, a multi-layered film, comprising a polymer composition, wherein the polymer composition comprises: within a range from 1 wt % to 25 wt % of a cyclic olefin copolymer based on the weight of the polymer composition, and within a range from 75 wt % to 99 wt % (the remainder of material) of a polyethylene based on the weight of the polymer composition, wherein the cyclic olefin copolymer has a glass transition temperature (Tg) of at least 80° C. The films may be used in shrink packaging application.
Abstract:
A polymer obtained by a solution polymerization process comprising within a range from 0.5 to 20 wt % of cyclic olefin derived units, within a range from 0 wt % to 15 wt % C4 to C12 α-olefin derived units, the remainder being ethylene derived units; and having a Mw/Mn of less than 2.5; a weight average molecular weight (Mw) within a range from 80,000 to 300,000 g/mole; and a g′ value of greater than 0.95. The polymer may be formed in a solution polymerization process comprising combining in a solution cyclic olefins, ethylene, hydrogen and optionally C4 to C12 α-olefins with a single-site catalyst to form the polymer, wherein the single-site catalyst is most preferably selected from unsymmetrical Group 4 bis-bridged cyclopentadienyl metallocenes.