Brazing paste
    8.
    发明授权
    Brazing paste 失效
    钎焊膏

    公开(公告)号:US4919731A

    公开(公告)日:1990-04-24

    申请号:US308450

    申请日:1989-02-10

    摘要: The present invention provides an electronic component part with terminal pins very closely and very strongly bonded to a high thermal conductivity ceramics circuit board and a method for simply and continuously manufacturing electronic component parts, with a high operability, each with terminal pins bonded to a high thermal conductivity ceramics circuit board. According to the present invention, an electronic component part is provided in which terminal pins are bonded to a high thermal conductivity ceramics circuit board by a brazing metal, containing at least one kind of Group IVa elements. In another aspect of the present invention a method is provided for manufacturing electronic component parts, which comprises the step of attaching terminal pins to a high thermal conductivity ceramics circuit board by a brazing paste layer comprised of brazing metal powder containing at least one kind of Group IVa elements, an acrylic binder with a carboxylic group as a substituent group and organic solvent, and heating the resultant structure in an atmosphere containing nitrogen as a principal element so that terminal pins are firmly bonded to a circuit board.

    Method of joining Ni-base heat resisting alloys
    9.
    发明授权
    Method of joining Ni-base heat resisting alloys 失效
    连接Ni基耐热合金的方法

    公开(公告)号:US4681251A

    公开(公告)日:1987-07-21

    申请号:US782163

    申请日:1985-10-02

    CPC分类号: B23K35/004 B23K35/286

    摘要: There is disclosed a method of joining Ni-base heat-resisting alloys which comprises forming, under an inert atmosphere, an aluminum layer on at least surfaces to be joined of a constructional member which has been divided into a plural number of parts composed of a Ni-base heat-resisting alloy reinforced by a .gamma.' phase in Ni.sub.3 Al system, followed by heating the parts so that said aluminum is dispersed in said Ni-base heat-resisting alloys, the joining portion (joint) contains substantially no .beta.-NiAl phase and a .gamma.'-Ni.sub.3 Al phase is dispersed therein to join the parts. The joint provided by the method according to the present invention has been improved in its strength and corrosion resistance at a high temperature. Further, the method according to the present invention can be carried out with a high degree of freedom in supplying a joining filler metal.

    摘要翻译: 公开了一种接合Ni基耐热合金的方法,其包括在惰性气氛下在至少被划分成多个部分的结构部件的表面上形成铝层的铝层 Ni3Al体系中由γ'相增强的Ni基耐热合金,然后加热部件使得所述铝分散在所述Ni基耐热合金中,所述接合部分(接头)基本上不含β-NiAl 相和γ'-Ni3Al相分散在其中以连接部件。 通过根据本发明的方法提供的接头在高温下的强度和耐腐蚀性得到改善。 此外,根据本发明的方法可以在供给接合填充金属时具有高自由度地进行。