    摘要: A method of making a transistor having first and second electrodes, a semiconductive layer, and a dielectric layer; said semiconductive layer comprising a semiconductive polymer and said dielectric layer comprising an insulating polymer; characterised in that said method comprises the steps of: (i) depositing on the first electrode a layer of a solution containing material for forming the semiconductive layer and material for forming the dielectric layer; and (ii) optionally curing the layer deposited in step (i); wherein, in step (i), the solvent drying time, the temperature of the first electrode and the weight ratio, of (material for forming the dielectric layer): (material for forming the semiconductive layer) in the solution are selected so that the material for forming the semiconductive layer and the material for forming the dielectric layer phase separate by self-organisation to form an interface between the material for forming the semiconductive layer and the material for forming the dielectric layer.

    摘要翻译: 一种制造具有第一和第二电极的晶体管的方法,半导体层和电介质层; 所述半导体层包括半导体聚合物,所述介电层包含绝缘聚合物; 其特征在于所述方法包括以下步骤:(i)在第一电极上沉积含有用于形成半导体层的材料的溶液层和用于形成介电层的材料; 和(ii)任选地固化在步骤(i)中沉积的层; 其中,在步骤(i)中,选择溶液中的(用于形成介电层的材料)的溶剂干燥时间,第一电极的温度和重量比:(用于形成半导体层的材料),使得 用于形成半导体层的材料和用于形成电介质层相的材料通过自组织分离,以在用于形成半导体层的材料和用于形成电介质层的材料之间形成界面。

    Functionalised graphene oxide
    8.
    发明授权
    Functionalised graphene oxide 有权
    官能化石墨烯氧化物

    公开(公告)号:US09156701B2

    公开(公告)日:2015-10-13

    申请号:US12735328

    申请日:2009-01-03

    摘要: A functionalised graphene oxide and a method of making a functionalized graphene oxide comprising: (i) oxidizing graphite to form graphite oxide wherein the graphene sheets which make up the graphite independently of each other have a basal plane fraction of carbon atoms in the sp2-hybridised state between 0.1 and 0.9, wherein the remainder fraction comprises sp3-hybridised carbon atoms which are bonded to oxygen groups selected from hydroxyl and/or epoxy and/or carboxylic acid; and (ii) exfoliating and in-situ functionalizing the graphite oxide surface with one or more functional groups such that fictionalization of the surface is effected at a concentration greater than one functional group per 100 carbon atoms and less than one functional group per six carbon atoms. The functionalized graphene oxide is dispersible at high concentrations in appropriate solvents without aggregating or precipitating over extended periods at room temperature.

    摘要翻译: 一种官能化石墨烯氧化物和制备官能化石墨烯氧化物的方法,包括:(i)氧化石墨以形成氧化石墨,其中组成石墨的石墨烯片彼此独立地具有sp2杂交中的碳原子的基础面部分 状态在0.1和0.9之间,其中剩余部分包含与选自羟基和/或环氧基和/或羧酸的氧基团键合的sp3杂化的碳原子; 和(ii)用一个或多个官能团对石墨氧化物表面进行去角质和原位官能化,使得表面的虚拟化以每100个碳原子大于一个官能团的浓度和每六个碳原子少于一个官能团 。 功能化石墨烯氧化物可以在适当的溶剂中以高浓度分散,而不会在室温下长时间聚集或沉淀。

    FUNCTIONALISED GRAPHENE OXIDE
    10.
    发明申请
    FUNCTIONALISED GRAPHENE OXIDE 有权
    功能性石墨氧化物

    公开(公告)号:US20110052813A1

    公开(公告)日:2011-03-03

    申请号:US12735328

    申请日:2009-01-03

    IPC分类号: C07C309/14 B05D5/00

    摘要: A functionalised graphene oxide and a method of making a functionalised graphene oxide comprising: (i) oxidizing graphite to form graphite oxide wherein the graphene sheets which make up the graphite independently of each other have a basal plane fraction of carbon atoms in the sp2-hybridised state between 0.1 and 0.9, wherein the remainder fraction comprises sp3-hybridised carbon atoms which are bonded to oxygen groups selected from hydroxyl and/or epoxy and/or carboxylic acid; and (ii) exfoliating and in-situ functionalizing the graphite oxide surface with one or more functional groups such that functionalisation of the surface is effected at a concentration greater than one functional group per 100 carbon atoms and less than one functional group per six carbon atoms. The functionalised graphene oxide is dispersible at high concentrations in appropriate solvents without aggregating or precipitating over extended periods at room temperature.