RUBBER COMPOSITION FOR TIRES AND PNEUMATIC TIRE
    12.
    发明申请
    RUBBER COMPOSITION FOR TIRES AND PNEUMATIC TIRE 有权
    轮胎和气胎的橡胶组合物

    公开(公告)号:US20150175781A1

    公开(公告)日:2015-06-25

    申请号:US14415501

    申请日:2012-08-02

    IPC分类号: C08L7/00

    摘要: The present invention provides rubber compositions for tires which are capable of improving handling stability, fuel efficiency, and processability while sufficiently reducing the dependence on petroleum resources, and pneumatic tires including tire components (e.g. bead apex) formed from the rubber compositions for tires. The present invention relates to rubber compositions for tires, containing a rubber component and a naturally derived phenolic resin.

    摘要翻译: 本发明提供轮胎用橡胶组合物,其能够在充分降低对石油资源的依赖性的同时提高操作稳定性,燃料效率和加工性,以及包括由轮胎用橡胶组合物形成的轮胎部件(例如胎圈三角胶)的充气轮胎。 本发明涉及用于轮胎的橡胶组合物,其包含橡胶组分和天然衍生的酚醛树脂。

    Rubber Composition for Sidewall and Preparation Process Thereof
    14.
    发明申请
    Rubber Composition for Sidewall and Preparation Process Thereof 审中-公开
    侧壁用橡胶组合物及其制备方法

    公开(公告)号:US20100252162A1

    公开(公告)日:2010-10-07

    申请号:US12087011

    申请日:2006-12-07

    摘要: The present invention relates to a rubber composition for a sidewall, in which an effect on environments can be taken into consideration, provision for the future decrease of petroleum supply can be satisfied, and further, tear strength and flex crack growth resistance can be improved with favorable balance without increasing hardness, and a process for preparing the rubber composition. The rubber composition for a sidewall is characterized by comprising 15 to 60 parts by weight of silica and 2 to 20 parts by weight of a double bond-containing plasticizer on the basis of 100 parts by weight of a rubber component comprising 30 to 80% by weight of a natural rubber and 20 to 70% by weight of an epoxidized natural rubber.

    摘要翻译: 本发明涉及一种用于侧壁的橡胶组合物,其中可以考虑对环境的影响,可以满足将来石油供应减少的要求,并且还可以通过以下方式提高撕裂强度和抗弯曲裂纹的生长阻力: 有利的平衡而不增加硬度,以及制备橡胶组合物的方法。 用于侧壁的橡胶组合物的特征在于,基于100重量份的橡胶组分包含15至60重量份的二氧化硅和2至20重量份的含双键的增塑剂,所述橡胶组分包含30至80重量% 天然橡胶的重量和20〜70重量%的环氧化天然橡胶。

    Colored Pure Titanium or Titanium Alloy Having Low Susceptibility to Discoloration in Atmospheric Environment
    15.
    发明申请
    Colored Pure Titanium or Titanium Alloy Having Low Susceptibility to Discoloration in Atmospheric Environment 有权
    有色纯钛或钛合金在大气环境中易变色

    公开(公告)号:US20090133783A1

    公开(公告)日:2009-05-28

    申请号:US11920486

    申请日:2006-05-25

    IPC分类号: C22C14/00

    摘要: The present invention provides colored pure titanium or titanium alloy having low susceptibility to discoloration in an atmospheric environment exhibiting a superior resistance to discoloration even when the titanium is used in an environment of harsh acid rain such as a roof or wall material and free from deterioration of the aesthetic appearance over a long period of time, that is, colored pure titanium obtained by the anodic oxidation method, that is, colored pure titanium or titanium alloy having low susceptibility to discoloration in an atmospheric environment characterized by having an average phosphorus content in a range of 40 nm from a surface of a titanium oxide layer formed on the titanium surface of 5.5 atomic % or less and by having an average carbon concentration in a range of a depth of 100 nm from the titanium surface of 3 to 15 atomic %.

    摘要翻译: 本发明提供了在大气环境中具有低变色性的着色纯钛或钛合金,即使当钛在诸如屋顶或墙体材料的恶劣的酸雨环境中使用时也显示出优异的抗变色性,并且没有变质 长时间的美学外观,即通过阳极氧化法获得的着色纯钛,即在大气环境中具有低变色敏感性的着色纯钛或钛合金,其特征在于平均磷含量为 从钛表面形成的氧化钛层的表面的5.5原子%以下的范围为40nm,并且使钛表面的深度为100nm的平均碳浓度为3〜15原子%。

    Rubber composition for coating textile cord and tire using the same
    16.
    发明申请
    Rubber composition for coating textile cord and tire using the same 有权
    用于涂布纺织线和轮胎的橡胶组合物

    公开(公告)号:US20070149664A1

    公开(公告)日:2007-06-28

    申请号:US11643659

    申请日:2006-12-22

    IPC分类号: B60C1/00

    摘要: The present invention provides a rubber composition for coating a textile cord, and a tire using the rubber composition, wherein rolling resistance is lowered, and processability and rubber strength are excellent, as compared with a rubber composition for coating a textile cord comprising raw materials derived from petroleum resources as a main component, and a tire using the rubber composition, while considering environments and providing for the future decrease in petroleum resources supply. The rubber composition for coating a textile cord comprises 25 to 80 parts by mass of silica and 1 to 15 parts by mass of a silane coupling agent on the basis of 100 parts by mass of a diene rubber, wherein a nitrogen adsorbing-specific surface area of said silica is 70 to 150 m2/g.

    摘要翻译: 本发明提供一种用于涂布纺织帘线的橡胶组合物和使用该橡胶组合物的轮胎,其中滚动阻力降低,加工性和橡胶强度优异,与用于涂布纺织帘线的橡胶组合物相比, 以石油资源为主要组成部分,以及使用橡胶组合物的轮胎,同时考虑到环境并为未来石油资源供应的减少提供依据。 用于涂布纺织帘线的橡胶组合物包含基于100质量份二烯橡胶的二氧化硅25至80质量份和硅烷偶联剂1至15质量份,其中氮吸附比表面积 的二氧化硅为70〜150m 2 / g。

    Worn article and method for producing the same
    17.
    发明申请
    Worn article and method for producing the same 有权
    磨损物品及其制造方法

    公开(公告)号:US20070142808A1

    公开(公告)日:2007-06-21

    申请号:US10598028

    申请日:2005-02-07

    IPC分类号: A61F13/15

    摘要: The present invention relates to a new worn article, which gives a close fit and with which it is possible to reduce the production cost. A worn article of the present invention includes a main body portion 20 including an absorbent core 25 and covering a front torso area, a crotch area and a rear torso area of a wearer, and a pair of side panels PL and PR attached to the main body portion 20 and located between the front and rear torso areas when the worn article is worn. Each of the side panels PL and PR is stretchable in an around-the-torso direction X. At least a portion of the side panel PL and PR includes an elastic thread G sandwiched between at least two sheet-like materials S1 and S2 and is in a contracted state where the elastic thread is contracted, thus forming gathers.

    摘要翻译: 本发明涉及一种新的磨损制品,其具有紧密配合,并且可以降低生产成本。 本发明的磨损物品包括主体部分20,其包括吸收芯25并覆盖穿用者的前躯干区域,裆部区域和后躯干区域,以及附接到主体的一对侧面板PL和PR 主体部分20并且当磨损的物品被磨损时位于前后躯干区域之间。 侧板PL和PR中的每一个可沿着身体方向X伸缩。侧板PL和PR的至少一部分包括夹在至少两个片状材料S1和S2之间的弹性线G 处于收缩状态,弹性线收缩,形成褶皱。

    Rubber composition for tire, tire member, base tread rubber composition, base tread and tire
    19.
    发明授权
    Rubber composition for tire, tire member, base tread rubber composition, base tread and tire 有权
    轮胎用橡胶组合物,轮胎构件,基础胎面橡胶组合物,基底胎面和轮胎

    公开(公告)号:US08921468B2

    公开(公告)日:2014-12-30

    申请号:US12600621

    申请日:2008-03-14

    摘要: A rubber composition for a tire includes a rubber component containing at least one of a natural rubber and an epoxidized natural rubber, silica and a natural based wax, wherein the silica is contained in an amount of 10 parts by mass or more based on 100 parts by mass of the rubber component and the natural based wax is contained in an amount of 1.2% by mass or more and 2% by mass or less based on the total mass of the rubber composition for a tire, and to a tread, a side wall, a clinch and a tire using the rubber composition. A rubber composition for a base tread used to form a base tread of a tire, the rubber composition includes a rubber component composed of a diene based rubber, silica contained in an amount 20 parts by mass or more and 70 parts by mass or less based on 100 parts by mass of the rubber component consisting of a diene based rubber and a natural based wax contained in an amount of 2 parts by mass or more and 15 parts by mass or less based on 100 parts by mass of said rubber component composed of the diene based rubber, and to a base tread and a tire obtained by using the rubber composition for a base tread.

    摘要翻译: 轮胎用橡胶组合物包含含有天然橡胶和环氧化天然橡胶,二氧化硅和天然蜡中的至少一种的橡胶成分,其中所述二氧化硅的含量相对于100重量份为10质量份以上 的橡胶成分和天然蜡的含量相对于轮胎用橡胶组合物的总质量为1.2质量%以上且2质量%以下,在胎面,侧面 墙壁,搭扣和使用橡胶组合物的轮胎。 一种用于形成轮胎胎面的胎面胎面用橡胶组合物,该橡胶组合物包括由二烯系橡胶构成的橡胶成分,20质量份以上的二氧化硅和70质量份以下的二氧化硅 在100质量份由二烯类橡胶和天然基蜡组成的橡胶组分的量为2质量份以上且15质量份以下的情况下,基于100质量份所述橡胶组分由以下组成: 二烯基橡胶,以及通过使用该基础胎面的橡胶组合物而获得的基底胎面和轮胎。

    Rubber composition and tire using same
    20.
    发明授权
    Rubber composition and tire using same 失效
    橡胶组合物和轮胎使用相同

    公开(公告)号:US08044133B2

    公开(公告)日:2011-10-25

    申请号:US11812001

    申请日:2007-06-14

    IPC分类号: C08K3/04

    摘要: The present invention provides a rubber composition for a tire which makes it possible to consider an effect on environment, prepare for decrease in supply quantity of petroleum in future and improve weather resistance and rubber strength in good balance, and a tire prepared by using the rubber composition. The rubber composition of the present invention comprises not less than 20 parts by weight of a silica, not more than 5 parts by weight of a carbon black and 2 to 20 parts by weight of a turpentine soot and/or lamp black having an average particle diameter of not more than 1,000 nm, based on 100 parts by weight of a rubber component comprising a natural rubber and/or an epoxidized natural rubber, and a tire prepared by using the rubber composition.

    摘要翻译: 本发明提供一种轮胎用橡胶组合物,其可以考虑对环境的影响,为了将来减少石油供给量的准备,良好的平衡提高耐候性和橡胶强度,通过使用橡胶 组成。 本发明的橡胶组合物包含不少于20重量份的二氧化硅,不超过5重量份的炭黑和2至20重量份的具有平均颗粒的松节油烟和/或灯黑 基于100重量份的包含天然橡胶和/或环氧化天然橡胶的橡胶组分和通过使用该橡胶组合物制备的轮胎的直径不大于1000nm。