Abstract:
Provided is a photocurable resin composition including a reactive compound, and a photopolymerization initiator. A cured product of the photocurable resin composition has two or more glass transition points including a TgA and a TgB. The TgA is less than 25° C., and the TgB is 25° C. or more. An elongation at break in accordance with ASTM D638 of the cured product of the photocurable resin composition is 130% or more, and a breaking strength in accordance with ASTM D638 of the cured product of the photocurable resin composition is 3 MPa or more.
Abstract:
A photocurable resin composition includes a reactive monomer, a reactive oligomer, and a photopolymerization initiator. A cured product of the reactive monomer has a glass transition point of less than 20° C., and a cured product of the reactive oligomer has a glass transition point of less than 20° C. A cured product of the photocurable resin composition has a loss tangent tan δ at 25° C. of 0.2 or less. The cured product of the photocurable resin composition has an elongation at break in accordance with ASTM D638 of 150% or more.
Abstract:
A manufacturing method of a mounting structure, the method including: a step of preparing a mounting member including a first circuit member and a plurality of second circuit members placed on the first circuit member, the mounting member having a space between the first circuit member and the second circuit member; a step of preparing a laminate sheet including a first thermal-conductive layer and a second thermal-conductive layer, the first thermal-conductive layer disposed at least on one outermost side; a disposing step of disposing the laminate sheet on the mounting member such that the first thermal-conductive layer faces the second circuit members; and a sealing step of pressing the laminate sheet against the first circuit member and heating the laminate sheet, to seal the second circuit members so as to maintain the space, and to cure the laminate sheet. The first thermal-conductive layer after curing has a coefficient of thermal conductivity in a thickness direction at room temperature being equal to or greater than that in a principal surface direction, and the second thermal-conductive layer after curing has a coefficient of thermal conductivity in a principal surface direction at room temperature being greater than that in a thickness direction.
Abstract:
A manufacturing method of a mounting structure, the method including: a step of preparing a mounting member including a first circuit member and a plurality of second circuit members placed on the first circuit member via bumps, the mounting member having a space between the first circuit member and the second circuit member; a step of preparing a sheet having a space maintaining layer; a disposing step of disposing the sheet on the mounting member such that the space maintaining layer faces the second circuit members; and a sealing step of pressing the sheet against the first circuit member and heating the sheet, to seal the second circuit members so as to maintain the space, and to cure the sheet. The bumps are solder bumps. The space maintaining layer after curing has a glass transition temperature of higher than 125° C., and a coefficient of thermal expansion at 125° C. or lower of 20 ppm/K or less.
Abstract:
A cured product of a curable material is a cured product of a curable material containing a benzoxazine compound and a polymerization initiator. The benzoxazine compound has a polymerizable functional group on a nitrogen atom constituting an oxazine ring. The cured product has a curing rate of 60% or more. The present invention also encompasses a polymer composition including a polymer including repeating units of a polymerizable monomer having a benzoxazine ring.
Abstract:
An electric conductive fiber structure includes an electric conductive resin containing electric conductive polymer(s), the electric conductive resin being filled in gaps between single fibers included in a fiber structure, the electric conductive fiber structure having 15% or more area ratio of the electric conductive resin present in an area of 15 to 30 μm from a surface when a cross section in a thickness direction of the fiber structure is observed.
Abstract:
Disclosed is an acrylic resin and a metal fine particle dispersion including the acrylic resin. The acrylic resin contains a unit of a (meth)acrylate monomer A having a polyalkylene glycol moiety and has at least at one end a carboxylic acid group and/or a carboxylic acid salt group.
Abstract:
An endotoxin adsorbent comprising a crystalline cellulose having a nitrogen atom-containing cationic group can sufficiently remove endotoxin from a material containing endotoxin to be removed and containing a substance having a cationic group and can efficiently remove endotoxin also from a highly viscous material. The nitrogen atom-containing cationic group may be typically a functional group derived from a polyvalent amine and/or a quaternary ammonium salt. The crystalline cellulose having a nitrogen atom-containing cationic group may comprise the nitrogen atom-containing cationic group at a content of 0.05 to 3 meq/dry·g in terms of anion exchange capacity.
Abstract:
The present invention aims to maximize the advantageous physical properties of sulfur and provide a cathode mixture that can be suitably used in a cathode mixture layer of an all-solid-state lithium-sulfur battery having excellent charge/discharge capacity. The present invention also aims to provide an all-solid-state lithium-sulfur battery including a cathode mixture layer containing the cathode mixture. The present invention relates to a cathode mixture for use in a cathode mixture layer of an all-solid-state lithium-sulfur battery, the cathode mixture containing the following components (A) to (D): (A) sulfur and/or its discharge product; (B) elemental phosphorus and/or PxSy where x and y independently represent an integer that gives a stoichiometric ratio; (C) an ion-conductive material; and (D) a conductive material.
Abstract:
The present invention aims to maximize the advantageous physical properties of sulfur and provide a cathode mixture that can be suitably used in a cathode mixture layer of an all-solid-state lithium sulfur battery exhibiting excellent charge/discharge capacity. The present invention also aims to provide an all-solid-state lithium sulfur battery including a cathode mixture layer containing the cathode mixture. The present invention provides a cathode mixture for use in a cathode mixture layer of an all-solid-state lithium sulfur battery, the cathode mixture containing: (A) an ion-conductive material containing phosphorus at a weight ratio of 0.2 to 0.55; (B) sulfur and/or its discharge product (B); and (C) a conductive material, the amount of the component (B) being 40% by weight or more of the total amount of the components (A), (B), and (C).