Abstract:
Capable of being provided are [1] a master batch comprising polyamide (X) comprising a diamine unit containing 70 mole % or more of a metaxylylenediamine unit and a dicarboxylic acid unit and an alkali compound (A), wherein an average particle diameter of the alkali compound (A) contained in the master batch is 50 μm or less; a contained number of particles having a particle diameter of exceeding 80 μm in 5 square millimeter of a cross section of the master batch is 1.5 particle or less; and a sum (m) of values obtained by multiplying a mole concentration of an alkali metal atom and a mole concentration of an alkaline earth metal atom each contained per g of the master batch by valencies thereof respectively is 60 μmol/g or more and 1710 μmol/g or less and [2] a production process for a polyamide resin composition prepared by making use of the master batch described in the above item [1]. Making use of the master batch of the present invention makes it possible to provide a polyamide resin composition which has a good appearance and a good color tone and which forms less gels in mold processing.
Abstract:
Provided is a polyamide polymer in which a partial structure represented by the following formula (C) constitutes a portion of the main chain: wherein in Formula (C), RA and RB each independently represent a hydrogen atom or an alkyl group having 1 to 6 carbon atoms; n and m each independently represent an integer from 0 to 2; Cy represents an unsaturated 6-membered or 7-membered ring which may contain a heteroatom; and * and ** each represent a bonding hand, while * may be a bonding hand extending from RA.
Abstract:
Film or plate containing a polyamide having monomer units of butane-1,4-diamine and monomer units of decanedioic acid (PA410). In a preferred embodiment the film or plate contains PA410 and at least one further polymer.
Abstract:
Provided is a xylylenesebacamide resin molding which is excellent in mechanical strength such as elastic modulus and avoids the problem of mechanical strength loss during long-term use. This is a molding of a polyamide resin or a polyamide resin composition containing the polyamide resin, wherein 70 mol % or more of the diamine structural unit is derived from xylylenediamine (A) and 50 mol % or more of the dicarboxylic acid structural unit is derived from sebacic acid (B), and the molding has a crystallinity index of 0 to 50% and a moisture content of 0.1 to 2% by mass.
Abstract:
This invention relates to a film for a tire inner liner, which includes a copolymer including a polyamide-based segment and 5˜50 wt % of a polyether-based segment relative to the total weight of the film, and has a thickness 30˜300 μm, and to a method of manufacturing the film for a tire inner liner, including polymerizing a polyamide-based resin or its precursor with 5˜50 wt % of a polyether-based resin relative to the total weight of the film, thus preparing a copolymer, and melting and extruding the copolymer, thus forming a film.
Abstract:
The present invention provides a method of manufacturing polyamide-carbon nanotube composites. The method includes mixing a polyamide composition including 0.01-1% by weight of carbon nanotubes using a shearing rate equal to or greater than 1000-4400 sec−1.
Abstract:
At an optional stage in the production step of a biaxially stretched film using a polyamide resin including, as a first component, nylon 6, and as a second component, a polyamide including xylylenediamine and an aliphatic dicarboxylic acid having 4 to 12 carbon atoms, the film is brought into contact with water set at 40° C. or higher and lower than 70° C. for 1 to 10 minutes and further with water set at 70° C. or higher for 1 to 10 minutes. In the film thus obtained, the content of low molecular weight compounds is 0% by mass to 0.2% by mass.
Abstract:
A binder composition comprising [A] an amorphous polyamide with a glass transition temperature of 140° C. or higher having a dicyclohexylmethane skeleton in the molecule and [B] a sulfonamide compound is used to provide a binder composition, a reinforcing-fiber base material and a preform respectively most suitable for RTM, which respectively exhibit excellent impact resistance and physical properties remaining stable over the variations of molding conditions and can be used for producing a fiber-reinforced composite material most suitable for members such as primary structures of aircraft.
Abstract:
Disclosed herein are polyamide composite structures and processes for their preparation. The disclosed composite structures comprise a surface, having at least a portion made of a surface resin composition, and comprise a fibrous material being impregnated with a matrix resin composition. The surface resin composition is selected from polyamide compositions comprising a blend of (A) fully aliphatic polyamides having a melting point of less than 230° C., and (B) fully aliphatic polyamides having a melting point of at least 250° C., and wherein the matrix resin composition is independently selected from (B) or blends of (A) and (B).
Abstract:
Disclosed herein are composite structures, overmolded composites structures and processes for their preparation. The disclosed composite structures have a surface having at least a portion made of a surface resin composition, and comprise a fibrous material being impregnated with a matrix resin composition, wherein the matrix polyamide resin composition and the surface resin composition are selected from polyamide compositions comprising a blend of semi-aromatic polyamides.