Abstract:
A system may include one or both of a light emitter (46) and a light receiver (40), and an optical filter (10). The optical filter (10) includes a wavelength selective scattering layer (14). The wavelength selective scattering layer (14) may have a near-infrared scattering ratio of less than about 0.9. The filter (10) may have a visible reflective haze ratio of greater than about 0.5. A method may include disposing the wavelength selective scattering layer (14) adjacent one or both of the light emitter (46) and the light receiver (40). The optical filter (10) may include a wavelength selective reflective layer (16). The optical filter (10) may include a wavelength selective absorbing layer (34). An article may include the optical filter (10). The wavelength selective scattering layer (14) may have an average near-infrared scattering of less than 60%, an average visible scattering of greater than 10%, and a difference between the % total visible reflectance and the % diffuse visible reflectance of less than 20.
Abstract:
A film is described comprising a first film layer having a Tg ranging from 30° C. to 60° C. The first film layer comprises a (meth)acrylic polymer and polyvinyl acetal polymer composition. The film further comprises a second layer proximate the first film layer. The second layer is different than the first film layer. The second may be a cured (meth)acrylic polymer film or coating; a backing such as thermoplastic polymer, woven or nonwoven fabrics, metal foils, paper, foams; or a coverfilm such as a fluoropolymer.
Abstract:
Optical films are described having a polymerized microstructured surface that comprises the reaction product of a polymerizable resin composition comprising at least one polymerizable ethylenically unsaturated triphenyl monomer. Also described are certain triphenyl (meth)acrylate monomers and polymerizable resin compositions.
Abstract:
An optical construction includes a reflective polarizer and an optically diffusive film disposed on the reflective polarizer. The reflective polarizer includes an outer layer including a plurality of first particles partially protruding from a first major surface thereof to form a structured major surface. A first optically diffusive layer is conformably disposed on the structured major surface. The optically diffusive film includes a second optically diffusive layer including a plurality of nanoparticles dispersed therein, and a structured layer including a structured major surface. For a substantially normally incident light and a visible wavelength range from about 450 nm to about 650 nm and an infrared wavelength range from about 930 nm to about 970 nm, the second optically diffusive layer has an average specular transmittance Vs in the visible wavelength range and an average specular transmittance Is in the infrared wavelength range, where Is/Vs≥2.5.
Abstract:
Optical films and stacks include at least one optically diffusive layer. The optically diffusive layer can include a plurality of nanoparticles and a polymeric material bonding the nanoparticles to each other to form a plurality of nanoparticle aggregates defining a plurality of voids therebetween. For substantially normally incident light and a visible wavelength range from about 450 nm to about 650 nm and an infrared wavelength range from about 930 nm to about 970 nm: in the visible wavelength range, the optical film or optically diffusive layer has an average specular transmittance Vs; and in the infrared wavelength range, the optical film or optically diffusive layer has an average total transmittance It and an average specular transmittance Is, Is/It≥0.6, Is/Vs≥2.5.
Abstract:
Optical films are described having a polymerized microstructured surface that comprises the reaction product of a polymerizable resin composition comprising at least one polymerizable ethylenically unsaturated triphenyl monomer. Also described are certain triphenyl (meth)acrylate monomers and polymerizable resin compositions.
Abstract:
Presently described are optical films, such as a brightness enhancing film, having a polymerized microstructured surface disposed on a preformed polymeric film wherein the film has a thickness of no greater than 3 mils and the polymerized microstructured surface consists of the reaction product of a substantially non-brominated polymerizable resin composition.
Abstract:
Presently described are hardcoat compositions comprising at least one first (meth)acrylate monomer comprising at least three (meth)acrylate groups and C2-C4 alkoxy repeat units wherein the monomer has a molecular weight per (meth)acrylate group ranging from about 220 to 375 g/mole and at least one second (meth)acrylate monomer comprising at least three (meth)acrylate groups. In one embodiment, the hardcoat composition further comprises and at least 30 wt-% solids of silica nanoparticles having an average particle size ranging from 50 to 150 nm. In another embodiment, the hardcoat composition further comprises and at least 30 wt-% solids of inorganic oxide nanoparticles having an average particle size ranging from 50 to 150 nm. Also described are articles, such as protective films, displays, and touch screens comprising such cured hardcoat compositions.
Abstract:
A method of making optical films having a polymerized microstructured surface are described. The polymerized microstructured surface comprises the reaction product of a polymerizable resin composition comprising 10% to 100 wt-% of at least one biphenyl di(meth)acrylate monomer. The di(meth)acrylate monomer comprises a core biphenyl structure having two aromatic rings connected with a C—C bond. The biphenyl di(meth)acrylate monomer preferably comprises a sufficient amount of ortho and/or meta(meth)acrylate substituents such that the monomer is a liquid at 25° C.
Abstract:
An article includes an optical filter that comprises a wavelength selective reflective layer and at least one wavelength selective absorbing layer. The optical filter has visible transmittance between 400 nm-700 nm of less than about 30% and near infrared transmittance at 830 nm-900 nm greater than about 30%.