摘要:
Provided is a resin powder for producing a three-dimensional object, wherein the resin powder has a number-average equivalent circle diameter of 10 micrometers or greater but 150 micrometers or less, and wherein a median in an equivalent circle diameter-based particle size distribution of the resin powder is higher than the average equivalent circle diameter.
摘要:
A resin powder for solid freeform fabrication includes a particle having a pillar-like form, wherein the ratio of the height of the particle to the diameter or the long side of the bottom of the particle is 0.5 to 2.0, the particle has a 50 percent cumulative volume particle diameter of from 5 to 200 μm, and the ratio (Mv/Mn) of the volume average particle diameter (Mv) to the number average particle diameter (Mn) of the particle is 2.00 or less.
摘要:
A resin powder for solid freeform fabrication has a 50 percent cumulative volume particle diameter of from 5 to 100 μm and a ratio (Mv/Mn) of a volume average particle diameter (Mv) to the number average particle diameter (Mn) of 2.50 or less and satisfies at least one of the following conditions (1) to (3): (1): Tmf1>Tmf2 and (Tmf1−Tmf2)≧3 degrees C., both Tmf1 and Tmf2 are measured in differential scanning calorimetry measuring according to ISO 3146, (2): Cd1>Cd2 and (Cd1−Cd2)≧3 percent, both Cd1 and Cd2 are measured in differential scanning calorimetry measuring according to ISO 3146, and (3): C×1>C×2 and (C1−C2)≧3 percent.
摘要:
A resin powder for solid freeform fabrication, having a melting point of 100 degrees C. or higher as measured according to ISO 3146 regulation and a ratio of melt mass-flow rate B to melt mass-flow rate A of greater than 0.80 to 1.20, wherein the melt mass-flow rate A and the melt mass-flow rate B are respectively measured at 15 degrees C. higher than the melting point under a load of 2.16 kg according to JIS K7210 format before and after the resin powder is maintained at a temperature 15 degrees C. lower than the melting point under a pressure of 0.1 kPa for four hours.
摘要:
A resin powder for solid freeform fabrication, having a ratio (Mv/Mn) of 2.00 or less, where Mv represents a volume average particle diameter and Mn represents a number average particle diameter and a ratio of melt mass-flow rate B to melt mass-flow rate A of greater than 0.80 to 1.20, wherein the melt mass-flow rate A and the melt mass-flow rate B are respectively measured at 15 degrees C. higher than the melting point under a load of 2.16 kg according to JIS K7210 format before and after the resin powder is maintained at a temperature 15 degrees C. lower than the melting point under a pressure of 0.1 kPa for four hours.
摘要:
A powder material for three-dimensional modeling includes a base particle and a coverage film including an organic material. The coverage film covers the base particle. The powder material is used for three dimensional modeling and when the coverage film is dissolved in a solvent to prepare a solution and the solution is formed into a coated film on a smooth surface, the coated film has a wetting tension of from 22 mN/m to 28 mN/m.
摘要翻译:用于三维建模的粉末材料包括基础颗粒和包括有机材料的覆盖膜。 覆盖膜覆盖基础颗粒。 粉末材料用于三维建模,当覆盖膜溶解在溶剂中以制备溶液并将溶液形成为光滑表面上的涂膜时,涂膜的润湿张力为22mN / m 至28 mN / m。
摘要:
Provided are resin particles including columnar resin particles each including filaments of a fibrous material, wherein the filaments of the fibrous material are aligned in an axial direction of each of the columnar resin particles.
摘要:
A replenishing developer housing container according to the present invention includes: a container body housing a replenishing developer; a conveying portion; a pipe receiving port; and an uplifting portion, wherein the replenishing developer contains a toner and a carrier, wherein the container body includes a protruding portion protruding from a container body interior side of the container opening portion toward one end of the container body and a curving portion curving so as to conform to the protruding portion, wherein the uplifting portion includes an uplifting wall surface extending from an internal wall surface of the container body toward the protruding portion, wherein the protruding portion is provided such that when the replenishing developer housing container is mounted on the replenishing developer conveying device, the protruding portion is present between the curving portion and the replenishing developer receiving port of a conveying pipe being inserted.
摘要:
A carrier for developing electrostatic latent images produced in an image developer includes a magnetic particulate core material and a covering layer covering the surface of the core material. The image developer includes an image bearer, a developer bearer including comprising a magnetic field generator inside and a developer regulation member facing the surface of the image developer with a predetermined gap. The carrier has a bulk density of from 1.6 to 2.25 g/cm3, a BET specific surface area of from 0.5 to 2.0 m3/g, a saturated magnetization (σ5000) not less than 70 emu/g at 5 kOe, and a residual magnetization (σr) not greater than 2 emu/g.