Cross-linked polyurethane resin sheet and laminated product employing it
    2.
    发明授权
    Cross-linked polyurethane resin sheet and laminated product employing it 失效
    交联聚氨酯树脂片和采用它的层合制品

    公开(公告)号:US5786070A

    公开(公告)日:1998-07-28

    申请号:US777671

    申请日:1996-12-20

    摘要: A transparent, smooth and cross-linked polyurethane resin sheet prepared from a reaction-curable composition which comprises a high molecular weight polyol mixture (A) comprising a polyester polyol and/or a polycarbonate polyol, as its main components, and containing a diol and a trivalent or higher valent polyol, the average hydroxyl value of the mixture being from 40 to 120, and the equivalent ratio of (the trivalent or higher valent polyol)/(the diol) being from 0.1 to 0.8, a substantially bivalent chain extender (B) in an amount of from 1.9 to 6.0 equivalents per equivalent of the polyol mixture (A), and a substantially bivalent alicyclic or aliphatic polyisocyanate compound (C) in an amount of from 0.8 to 1.2 equivalents per equivalent of the sum of the polyol mixture (A) and the chain extender (B), as its main components.

    摘要翻译: 由反应固化性组合物制备的透明,平滑且交联的聚氨酯树脂片材,其包含以聚酯多元醇和/或聚碳酸酯多元醇为主要成分的高分子量多元醇混合物(A),并含有二醇和 三价以上的多元醇,所述混合物的平均羟值为40〜120,(三价以上的多元醇)/(二醇)的当量比为0.1〜0.8,基本上为二价扩链剂( B)的量为每当量多元醇混合物(A)1.9至6.0当量,基本上为每当量多元醇的总数为0.8至1.2当量的脂族或脂族多异氰酸酯化合物(C) 混合物(A)和扩链剂(B)作为其主要组分。

    Method for manufacturing laminated glasses
    3.
    发明授权
    Method for manufacturing laminated glasses 失效
    夹层玻璃的制造方法

    公开(公告)号:US4789600A

    公开(公告)日:1988-12-06

    申请号:US29650

    申请日:1987-03-24

    摘要: A method for the manufacture of a laminated glass assembly comprising (1) a monolithic or laminated glass and/or plastic support having an glazed edge, and (2) a plastic sheet comprising at least one layer of polyurethane in contact with the surface having the glazed edge is disclosed. In the invention, at least one of the two contact surfaces of the glazed edge with the polyurethane layer is treated, before the assembly of the support with the plastic sheet on an area corresponding essentially to the glazed edge, by the deposit of a primer comprising a reactive mixture having free NCO groups. The free NCO groups are capable of reacting with the glazed support and with the plastic sheet and of forming cross-linking bonds with the other components of the primer at the time of the heat cycle of the subsequent assembly. The plastic sheet is the assembled with the support, and the glass undergoes a heat cycle which enables the reaction of the primer and the definitive peripheral adhesion of the glass.

    摘要翻译: 一种用于制造夹层玻璃组件的方法,包括(1)具有玻璃边缘的整体或夹层的玻璃和/或塑料支撑件,以及(2)塑料片,其包括至少一层与表面接触的聚氨酯层, 玻璃边缘被披露。 在本发明中,在将具有聚氨酯层的上光玻璃边缘的两个接触表面中的至少一个处理之前,在将载体与塑料片组装在基本上与玻璃边缘相对的区域之前,通过沉积包含 具有游离NCO基团的反应混合物。 游离的NCO基团能够与玻璃载体和塑料片反应,并在随后组装的热循环时与底漆的其它组分形成交联键。 塑料片与支撑体组装在一起,并且玻璃经受热循环,使得底漆的反应和玻璃的确定的周边粘合。