摘要:
Numerous applications for hollow glass bodies made from low melting glass material require an increase in the chemical resistance of the interior surface of the glass body. In order to avoid a disadvantageous de-alkalizing process the hollow glass body must be provided with an interior coating in a comparatively expensive prior art process. In an improved process according to the invention a glass tube acting as a semifinished product from which the hollow glass body is made is provided with an interior coating of oxide material, preferably SiO2, Al2O3, TiO2 or mixtures thereof, having a predetermined coating thickness according to the required chemical resistance or working conditions for forming the glass body and then the hollow glass body is made from the glass tube. The coating is advantageously provided by means of a PICVD process.
摘要翻译:由低熔点玻璃材料制成的中空玻璃体的许多应用需要增加玻璃体的内表面的耐化学性。 为了避免不利的去碱化过程,中空玻璃体必须在比较昂贵的现有技术方法中提供内部涂层。 在根据本发明的改进方法中,用作中空玻璃体制成的半成品的玻璃管设置有氧化物材料(优选SiO 2,Al 2 O 3,TiO 2或其混合物)的内部涂层,其具有预定的涂层厚度,根据 达到用于形成玻璃体的所需的耐化学性或工作条件,然后中空玻璃体由玻璃管制成。 该涂层有利地通过PICVD工艺提供。
摘要:
Glass containers specifically for the storage of pharmaceutical or diagnostic solutions whose surface which comes into contact with the solutions is coated with a layer of oxides and/or nitrides of the elements Si, Ti, Ta, Al or mixtures thereof applied by means of a plasma CVD process.
摘要:
A plastic vessel has a barrier coating comprising sequentially arranged barrier layers of organic polymer and of inorganic oxides, nitrides or oxynitrides. The barrier coating preferably has at least two inorganic barrier layers. The thickness of the inorganic barrier layers lies between 2 and 300 nm and the thickness of the organic barrier layer lies between 2 and 1000 nm. The total thickness of the layer packet should not exceed 0.1 mm.
摘要:
A plastic vessel has a barrier coating comprising sequentially arranged barrier layers of organic polymer and of inorganic oxides, nitrides or oxynitrides. The barrier coating preferably has at least two inorganic barrier layers. The thickness of the inorganic barrier layers lies between 2 and 300 nm and the thickness of the organic barrier layer lies between 2 and 1000 nm. The total thickness of the layer packet should not exceed 0.1 mm.
摘要:
The invention concerns a plasma CVD system (in particular a plasma pulse CVD system) with an array of microwave antennas. According to the invention, in order to improve the homogeneity of the layer, interference is prevented by controlling adjacent antennas in a chronologically offset manner. To that end, microcapsules are provided within the macrocapsules of the plasma pulse CVD process. Additionally, the uniformity of the layer deposition at the interfaces between adjacent modules can be optimized by radio-frequency excitation by means of suitable electrodes, magnetic fields or the configuration of the gas inlets. The surface coated in an operating cycle can thus be scaled as required.
摘要:
The glass container stores and preserves pharmaceutical or diagnostic solutions for medicinal purposes. So that the container is free of silicones and other residues, it is provided with an amorphous, transparent anti-adherent coating (4) over its entire interior surface from its bottom over the wall (3) to the closure device (2). This anti-adherent coating (4) is free of heavy metals, free of silicones, is stable after autoclaving at about 120° C. for about 20 min or hot air sterilization for 30 min at 300° C., has a contact angle for wetting with water of ≧80°, contains silicon, oxygen, carbon, fluorine and hydrogen and is deposited by a PECVD method, especially a PICVD method. If the coating contains less than 0.1% by weight fluorine, then it contains greater than or equal to 10% by weight carbon, but if it contains greater than or equal to 0.1% fluorine then it contains greater than or equal to 5% by weight carbon.
摘要:
In order to guarantee that individual elastomeric components used for medicinal or pharmaceutical purposes have improved inertness and static and sliding friction properties, a suitable layer is provided on the elastomeric components for this purpose by the method of the invention. This method includes providing an extended flat mat made of elastomeric material including connected protruding elastomeric components; coating at least one side of the mat including the connected elastomeric components by means of a PECVD or PICVD method to provide a silicon dioxide layer containing carbon, hydrogen and/or nitrogen on the at least one side of the mat; and punching the connected elastomeric components out of the mat to form individual unconnected elastomeric components, each at least partially coated with a portion of the layer.
摘要:
The invention is a glass container which can be sterilized for medical purposes, including the storage of pharmaceutical or diagnostic products, further including solutions. The container is made from glass containing a stabilizer which inhibits the deleterious effects of high energy radiation, wherein the surface which is in direct contact with the product or solution has a coating that has a thickness of less than 400 nm and is formed from oxides or nitrides of the elements Si, Ti, Ta, AI or a mixture thereof.
摘要:
This invention relates to optical, preferably ophthalmic lenses with a body made of plastic, in particular for spectacle glasses, and the plastic incorporates cycloolefinic polymers and the plastic body is coated with a transparent coating resistant to corrosion. Another object of this invention is a process for the production of these lenses. The lenses according to the invention are especially resistant to greases, sweat and/or solvents.
摘要:
A device, in particular a cover panel for a display device or a monitor auxiliary panel or a surface for input devices, includes a substrate and a coating applied onto the substrate. The coating has a surface having a coefficient of friction in the range between approximately 0.01 and 0.12, in particular between approximately 0.02 and 0.1, or between approximately 0.03 and 0.09.