公开(公告)号:US20180265663A1
公开(公告)日:2018-09-20
申请号:US15762650
申请日:2016-09-08
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Kaori KUWAGAKI , Akiyoshi KUSAKA
CPC classification number: C08J9/28 , C08J3/14 , C08J2329/00
Abstract: A manufacturing method for porous resin microparticles comprising steps of: heating a polyester thermoplastic resin having biodegradability to a temperature of 80° C. or higher and 200° C. or lower in a glycol ether solvent to obtain a solution, and cooling the solution to precipitate the polyester thermoplastic resin as porous resin microparticles.
-
公开(公告)号:US20210309811A1
公开(公告)日:2021-10-07
申请号:US17347864
申请日:2021-06-15
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Kaori KUWAGAKI , Akiyoshi KUSAKA
IPC: C08J3/16 , A61K8/02 , A61K8/85 , A61Q19/00 , C08G63/06 , C08G63/08 , C08G63/16 , C08J3/11 , C09D5/03 , C09D167/02 , C09D167/04 , C08J3/12
Abstract: Generally spherical resin particles formed of a thermoplastic resin, having a sphericity of 0.90 to 1.00, a light scattering index of 0.5 to 1.0 and a linseed oil absorption of 30 to 150 mL/100 g.
-
公开(公告)号:US20180208721A1
公开(公告)日:2018-07-26
申请号:US15746153
申请日:2016-08-18
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Akiyoshi KUSAKA , Kaori KUWAGAKI , Ryosuke HARADA
CPC classification number: C08J3/12 , A61K8/0241 , A61K8/85 , A61K2800/412 , A61Q1/12 , A61Q19/00 , A61Q19/007 , C08G63/183 , C08J2367/02 , C09D7/40 , C09D7/69
Abstract: Polyester-based resin particles including a polyester-based resin as a base resin, in which the base resin exhibits a plurality of endothermic peaks corresponding to crystal melting temperatures by DSC measurement, at least one of the endothermic peaks exists in each region of a low temperature side region and a high temperature side region, a maximum endothermic peak of the low temperature side region and a maximum endothermic peak of the high temperature side region exhibit a crystal melting heat amount ratio (low temperature side crystal melting heat amount/high temperature side crystal melting heat amount) in a range of 0.1 to 1.5, and the polyester-based resin particles have a volume average particle diameter of 1 to 50 μm.
-
公开(公告)号:US20170260342A1
公开(公告)日:2017-09-14
申请号:US15509231
申请日:2015-09-09
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Akiyoshi KUSAKA , Kaori KUWAGAKI , Ryosuke HARADA
IPC: C08J3/24 , A61Q1/12 , A61K8/06 , A61Q1/02 , C08G18/78 , C08G18/44 , C08G18/34 , C08G18/32 , C08G18/48 , C08G18/73 , C09D175/16 , C08G18/83 , C08G18/66 , C08K3/36 , A61K8/87
CPC classification number: C08J3/24 , A61K8/06 , A61K8/81 , A61K8/87 , A61K2800/412 , A61Q1/02 , A61Q1/12 , A61Q19/00 , C08F2/18 , C08F2/44 , C08F290/06 , C08F299/06 , C08G18/10 , C08G18/3221 , C08G18/348 , C08G18/44 , C08G18/4829 , C08G18/6607 , C08G18/664 , C08G18/672 , C08G18/6725 , C08G18/73 , C08G18/7837 , C08G18/8016 , C08G18/8025 , C08G18/831 , C08J2375/16 , C08K3/36 , C08L55/00 , C09D7/40 , C09D175/16 , C09D201/00
Abstract: A high-recoverability resin particles having a mean particle size of 1 to 100 μm containing a crossdinked (meth)acrylic acid ester-based resin, wherein the high-recoverability resin particles have a recovery rate of 22% or greater, and a 30% compression strength of 1.5 to 5.0 kgf/mm2.
-
公开(公告)号:US20210079190A1
公开(公告)日:2021-03-18
申请号:US17106518
申请日:2020-11-30
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Kaori KUWAGAKI , Akiyoshi KUSAKA
Abstract: A manufacturing method for porous resin microparticles comprising steps of: heating a polyester thermoplastic resin having biodegradability to a temperature of 80° C. or higher and 200° C. or lower in a glycol ether solvent to obtain a solution, and cooling the solution to precipitate the polyester thermoplastic resin as porous resin microparticles.
-
6.
公开(公告)号:US20190276611A1
公开(公告)日:2019-09-12
申请号:US16318808
申请日:2016-07-22
Applicant: SEKISUI PLASTICS CO., LTD.
Inventor: Kaori KUWAGAKI , Akiyoshi KUSAKA
IPC: C08J3/16 , C08J3/11 , C08G63/16 , C08G63/08 , C08G63/06 , C09D5/03 , C09D167/02 , C09D167/04 , A61Q19/00 , A61K8/85 , A61K8/02
Abstract: Generally spherical resin particles formed of a thermoplastic resin, having a sphericity of 0.90 to 1.00, a light scattering index of 0.5 to 1.0 and a linseed oil absorption of 30 to 150 mL/100 g.
-
-
-
-
-