摘要:
A coating composition having a total solids content of at least about 85 wt. %, based on the weight of the composition, a volatile organic chemical content of less than about 15 wt. %, based on the weight of the composition and a Brookfield viscosity of about 500-2,000 centipoises at 25.degree. C. The composition contains a polyester polyol having a weight average molecular weight of about 300-900 and a hydroxy number of about 150-400; at least one thermosettable polyester; an alkoxy aminoplast resin; a reactive diluent present in an amount of 0-30 wt. %, based on the weight of the composition; and an acid catalyst curing agent.
摘要:
Melt blended filled thermoplastic resin compositions include a thermoplastic matrix resin, a filler material and a thermoplastic additive resin. The compositions of the invention include discreet continuous phases of matrix resin and additive resin, with the filler material being present essentially entirely within the additive resin phase (i.e., essentially absent from the matrix resin phase). More specifically, the components are selected so that their respective surface tensions allow the additive resin to form a complex three-dimensional interpenetrating network structure within the matrix resin when melt-blended, and such that essentially all of the filler material is homogeneously dispersed throughout the formed three-dimensional network structure.
摘要:
The invention relates to a coating composition containingA) 50 to 90% by weight of one or more hydroxyl-containing addition polymers, prepared by copolymerization of ethylenically unsaturated monomers which are in part hydroxyalkyl esters of .alpha.,.beta.-ethylenically unsaturated carboxylic acids andB) 10 to 50% by weight of one or more amino resin crosslinking agentsthe sum of the proportions by weight of A and B being 100% by weight, and suitable auxiliaries and additives, optionally pigments, optionally fillers, organic solvent and an acid catalyst.The coating composition is one wherein the acid catalyst used comprises1) sulfo- or sulfonio[sic]-succinic esters which each contain at least one hydroxyl group and/or2) sulfo- or sulfonio[sic]-succinic polyesters which each contain at least one hydroxyl group.The invention furthermore relates to a process for the preparation of the coating compositions according to the invention and to their use as an automobile repair finish or as a stoving paint.
摘要:
The stabilized binder is a mixture of two copolymers and at least one curing agent. The one copolymer contains fluorine or silicon and a UV absorber in copolymierized form. The other copolymer is an acrylic resin. Suitalbe curing agents are melamine resins or polyisocyanates.
摘要:
A thermosetting resin composition comprising as main components(A) an acrylic resin containing in the molecule a carboxyl group, a hydroxyl group and an epoxy group and having an acid value of 15-150 mg KOH/g, a hydroxyl value of 30 mg KOH/g or more, an epoxy equivalent of 3,000-15,000 and a number-average molecular weight of 3,000-30,000,(B) an acrylic resin containing in the molecule a carboxyl group, a hydroxyl group and an epoxy group and having an acid value of 2-10 mg KOH/g, a hydroxyl value of 30 mg KOH/g or more, an epoxy equivalent of 250-2,500 and a number-average molecular weight of 3,000-30,000 and(C) an amino resin,wherein the molar ratio of the carboxyl group of the component (A)/the epoxy group of the component (B) is 1/0.5 to 0.5/1 and the amount of the component (C) is 10-40% by weight based on the total amount of the components (A) to (C). The resin composition is useful for use particularly in top coat paint composition for automobile outer panels.
摘要:
A method for forming a transparent multilayer is described, using a wet-on-wet process in which first a transparent acrylic copolymer paint A and then a transparent fluorine-containing polymer paint B comprising the formula ##STR1## wherein X represents a fluorine atom or chlorine atom, and R.sub.1, R.sub.2, R.sub.3, R.sub.4 each represents represents a hydrogenatom, hydroxyalkyl group, or carboxyalkyl group, are applied on a conventional finish coating.The method produces a protective multilayer consisting of a paint A layer to improve adhesion and a paint B layer to improve weatherability on the conventional finish coatings.
摘要:
Water-dilutable binders for water-dilutable lacquers, coating compositions or sealing compounds consist essentially of a mixture of 5 to 40 parts by weight of a crosslinker resin and 60 to 95 parts by weight of a copolymer containing carboxyl groups or acid anhydride groups or both and further containing hydroxyl groups, and wherein the carboxyl or acid anhydride groups have been at least partially converted into carboxylate groups to the degree necessary to provide solubility or dispersibility of the binder in water and said copolymer is obtained by copolymerizing an alpha, beta-unsaturated carboxylic acid, a hydroxyalkyl acrylate or methacrylate, an olefinic monomer, a hydroxy-free acrylate or methacrylate and, optionally other mono-or polyunsaturated monomer, and wherein at least 30% of the hydroxyl groups of the copolymer are modified by esterification with a lactone.
摘要:
A physical property-improving reagent which comprises an alkenoylcarbamate compound of the formula: ##STR1## wherein R is a hydrogen atom or a lower alkyl group, X is an oxygen atom (--O--), a sulfur atom (--S--) or a substituted or unsubstituted imino group (--NR'--), R' being a hydrogen atom or a lower alkyl group, and Y is the residue of an active hydrogen atom-containing compound excluding --X-H therefrom dissolved in an organic solvent having a solubility parameter of not less than 8, which can impact excellent physical properties to a polymer produced with the same.
摘要:
An aqueous coating composition characterized in that the composition comprises:(A) a water-dispersible film-forming acrylic polymer,(B) a crosslinking agent prepared by dispersing a hydrophobic melamine resin in water in the presence of a water-soluble resin, the hydrophobic melamine resin being up to about 20 in solvent dilution ratio when diluted with a water/methanol solvent mixture (35/65 in weight ratio) and about 500 to about 4000 in weight average molecular weight, and(C) a pigment.The composition is very suitable for use in the two-coat one-bake coating method as a base-coat composition.
摘要:
Dry strength resins are prepared by reacting acrylamide polymers with amino/aldehyde resin acid colloids during the formation of the colloid. The resultant copolymers are useful as dry strength resins in the formation of paper.