摘要:
According to the present invention, the adaptability to producing the cellulose acylate film and the surface properties of the cellulose acylate film produced by means of the melt film-forming method can be remarkably improved. Accordingly, there is also improved the surface properties of a stretched cellulose acylate film produced by stretching such an unstretched cellulose acylate film.
摘要:
Provided is a method for producing a polyester film, including: subjecting a polyester raw material resin, which contains a titanium compound and has an intrinsic viscosity of from 0.71 to 1.00, to melt extrusion using a twin-screw extruder which includes a cylinder; two screws disposed inside the cylinder; and a kneading disk unit disposed in at least a portion of a region extending from a 10%-position to a 65%-position of screw length with respect to an upstream end of the screws in a resin extrusion direction as a starting point, at a maximum shear rate generated inside the twin-screw extruder of from 10 sec−1 to 2000 sec−1; forming an unstretched film by cooling and solidifying the melt extruded polyester resin on a cast roll; subjecting the unstretched film to biaxial stretching in a longitudinal direction and a lateral direction; and heat fixing the stretched film formed by biaxial stretching.
摘要:
According to the present invention, a cellulose acylate film having high thickness precision and no streaks can be formed by producing a film with a cellulose acylate resin by means of the polishing roller method, and a high-performance optical film, which is free from the retardation distribution, can be produced by subsequently stretching the cellulose acylate film thus obtained within a magnification range from 1 or more and 2.5 or less.
摘要:
When amorphous thermoplastic resin is supplied from a hopper, the resin is rotated by a screw in a barrel and generates frictional heat. In this point of view, in a melt extruder according to an aspect of the present invention, a temperature control zone that generates particularly high frictional heat is constantly cooled by a cooling device, and heated by a heating device to obtain a target temperature, thereby significantly reducing variations in barrel temperature. This can stabilize screw tip pressure, and reduce variations in thickness of a resin film discharged from the barrel.
摘要:
To provide a thermoplastic resin film, and process for producing the same, which can obtain a film having high optical properties in which the occurrence of residual strain and the exhibition of retardation during film forming are suppressed. A film (12) is produced by extruding melted thermoplastic resins in sheet form through a die (24), and sandwiching the sheet between a pair of rollers (26), (28) configured so that at least one of the rollers is an elastic roller (26) made from metal, to cool and solidify the sheet into the film, the thickness Z of a metal tube (44) constituting an outer shell of the elastic roller (26) being in a range of 0.05 mm
摘要:
An aspect of the present invention is a method for manufacturing a thermoplastic resin film, comprising the steps of: extruding a molten thermoplastic resin from a die in the form of sheet; and sandwiching the sheet-form thermoplastic resin between one support and the other support, wherein at least one of the supports has such a surface property that the arithmetic average surface depth (Ra) is 100 nm or less, and the support is a hollow drum and the thickness Z (mm) of an outercylinder of the drum satisfies the following expression; 0.2 mm
摘要:
The present invention provides a method for producing a cellulose acylate film which can prevent the generation of foreign matter problems and can produce a high-quality film. A cellulose acylate resin is molten in a twin-screw extruder and extruded from a die to form a cellulose acylate film. The average residence time of the resin in the extruder is set at 5 minutes or less.
摘要:
The present invention provides a method for producing a thermoplastic film which makes it possible to improve the optical properties of the thermoplastic film obtained by stretching and a thermoplastic film manufactured thereby. The transverse stretching section in which a cellulose acylate film is transversely stretched includes: a preheating zone, a transverse stretching zone, a cooling zone and a thermal relaxation zone, and the cellulose acylate film having been cooled in the cooling zone is immediately subjected to thermal relaxation treatment in the thermal relaxation zone.
摘要:
According to the present invention, a cellulose acylate film having high thickness precision and no streaks can be formed by producing a film with a cellulose acylate resin by means of the polishing roller method, and a high-performance optical film, which is free from the retardation distribution, can be produced by subsequently stretching the cellulose acylate film thus obtained within a magnification range from 1 or more and 2.5 or less.
摘要:
A thermoplastic film having at least two thermoplastic resin layers laminated on each other, wherein at least the thermoplastic resin layer of the film surface and the thermoplastic resin layer of the film back each have a tilt structure in the thickness direction of the film, and in the plane including the tilt direction of the tilt structure and the film normal line, the sign of the angle, φ between the normal direction of the film surface and the tilt direction differs between the thermoplastic resin layer of the film surface and the thermoplastic resin layer of the film back, and wherein φ is from −90° to 90°.