    摘要: A birefringent film with excellent uniformity in in-plane retardation, retardation in the thickness direction, and alignment axis is provided. The birefringent film is produced in such a manner that, in the step of stretching a polymer film, the polymer film is stretched in a width direction while being shrunk in a longitudinal direction, and assuming that lengths in the width direction and the longitudinal direction of the polymer film before being stretched are 1, a change ratio (STD) of the length in the width direction of the polymer film resulting from the stretching and a change ratio (SMD) of the length in the longitudinal direction of the polymer film resulting from the shrinking satisfy the following formula (1). (1/STD)1/2≦SMD

    摘要翻译: 提供了具有优异的面内延迟均匀性,厚度方向延迟和取向轴的双折射膜。 双折射膜的制造方法是,在拉伸高分子膜的工序中,聚合物膜沿长度方向收缩而沿宽度方向拉伸,假设宽度方向和长度方向的长度 拉伸前的聚合物膜为1,由拉伸得到的聚合物膜的宽度方向的长度的变化率(STD)和聚合物膜的长度方向的长度的变化率(SMD)由 收缩满足下式(1)。 (1 / STD)1/2&nlE; SMD <1(1)

    Process for producing coated sheet, optically functional layer, optically compensating plate, optical device and image display
    2.
    发明授权
    Process for producing coated sheet, optically functional layer, optically compensating plate, optical device and image display 有权
    生产涂层板,光学功能层,光学补偿板,光学装置和图像显示器的方法

    公开(公告)号:US07820235B2

    公开(公告)日:2010-10-26

    申请号:US10563865

    申请日:2004-03-19

    IPC分类号: B05D5/06

    CPC分类号: G02B5/3083

    摘要: The method of cleaning a coated sheet according to the present invention is characterized in that dry wind is brown along the traveling direction of a film onto the surface of a coating layer wherein the solid content and the viscosity of the coating solution are within specified ranges. By this method, the thickness precision of the coating film can be improved in its large area, and the evenness of its in-plane optically functional property can be made even therein. The speed of the dry wind, the temperature of the wind, and the thickness of the dried coating film are preferably within specified ranges. In particular, the coated sheet is very useful as an optical material having good properties in an optically functional layer which is frequently used as a large-area coated sheet, an optical device having such an optically functional layer, an optically compensating layer, or an optically compensating plate. The coated sheet is particularly effective for an image display on which they are mounted.

    摘要翻译: 根据本发明的清洁涂布纸的方法的特征在于,干燥风沿着涂膜的表面上的膜的行进方向为棕色,其中固体含量和涂布溶液的粘度在规定范围内。 通过这种方法,可以在大面积上提高涂膜的厚度精度,并且甚至可以使其平面内的光学功能性均匀。 干风的速度,风的温度和干燥的涂膜的厚度优选在规定的范围内。 特别地,涂布片材作为光学功能层具有良好性能的光学材料是非常有用的,该功能层经常用作大面积涂布片材,具有这种光学功能层的光学器件,光学补偿层或 光学补偿板。 涂布片对于安装它们的图像显示器是特别有效的。

    Polarizer, polarizing plate, and visual display
    6.
    发明授权
    Polarizer, polarizing plate, and visual display 有权
    偏光镜,偏光板和视觉显示

    公开(公告)号:US06757102B2

    公开(公告)日:2004-06-29

    申请号:US10355185

    申请日:2003-01-31

    IPC分类号: G02B530

    CPC分类号: G02B5/3025

    摘要: A polarizer comprising a polyvinyl alcohol based film being dyed by iodine and treated with potassium iodide, wherein an element content ratio (K/I) of iodine (I) and potassium (K) is 0.05 through 0.24, show an effect controlling coloring and satisfying high durability under conditions of high temperature.

    摘要翻译: 一种偏光镜,其由碘染色的聚乙烯醇系膜和碘化钾处理,其中碘(I)和钾(K)的元素含量比(K / I)为0.05〜0.24,显示出控制着色的效果,满足 耐高温条件下耐高温。

    Process for producing polarizing film, polarizing film, polarizing plate, optical film, and image display
    8.
    发明授权
    Process for producing polarizing film, polarizing film, polarizing plate, optical film, and image display 有权
    用于制造偏光膜,偏振片,偏振片,光学膜和图像显示器的方法

    公开(公告)号:US07871665B2

    公开(公告)日:2011-01-18

    申请号:US10581610

    申请日:2005-07-25

    IPC分类号: G02B1/10

    摘要: The present invention pertains to a method of fabricating a polarizing film by uniaxially stretching a resin film such as a polyvinyl alcohol-based film in a fabrication process including a swelling step and a dyeing step following the swelling step, comprising the steps of immersing a resin film in bath liquids in at least two or more swelling baths in sequence in the above-mentioned swelling step, wherein at least a bath temperature of a swelling bath located at a Nth position from the front-stage side is set at a temperature which is higher than a bath temperature of a swelling bath located at a (N+M)th position by 3° C. or more (both N and M are specified positive integers).

    摘要翻译: 本发明涉及在包括溶胀步骤和膨胀步骤之后的染色步骤的制造方法中通过单轴拉伸树脂膜如聚乙烯醇基膜制造偏光膜的方法,包括以下步骤:将树脂 在上述溶胀步骤中依次在至少两个或更多个溶胀浴中的浴液中的膜,其中位于前段侧的第N位置的溶胀浴的浴温至少为 高于位于(N + M)位置3℃以上的溶胀浴的浴温度(N和M均为正整数)。

    Method for manufacturing coated sheet, optical functional layer, optical element, and image display device
    10.
    发明授权
    Method for manufacturing coated sheet, optical functional layer, optical element, and image display device 失效
    制造涂布片,光学功能层,光学元件和图像显示装置的方法

    公开(公告)号:US07320812B2

    公开(公告)日:2008-01-22

    申请号:US10641117

    申请日:2003-08-15

    IPC分类号: B05D5/06

    摘要: A method for manufacturing a coated sheet that may form a coated layer having a uniform film thickness by a coating liquid even when a substrate has a large area is provided.A method for manufacturing a coated sheet to form a coated layer by a process including a process (1) for coating a coating liquid including a resin material and a solvent on a substrate, and a drying process (2) for drying a coated liquid, wherein a drying is performed under drying wind flow having an average wind speed of 10 m/s or less until a viscosity of the coated liquid in the drying process (2) reaches at least 50 [mPa·s] at drying temperatures.

    摘要翻译: 提供了即使在基板面积大的情况下也可以通过涂布液形成具有均匀膜厚的涂布层的涂布片材的制造方法。 一种通过包括用于在基材上涂布包括树脂材料和溶剂的涂布液的方法(1)的方法和用于干燥涂布液体的干燥工艺(2)的方法制造涂覆的薄板以形成涂层的方法, 其特征在于,干燥风干燥时的平均风速为10m / s以下,干燥工序(2)中的涂布液的粘度在干燥温度下达到至少50 [mPa·s]。