METHOD FOR PRODUCING PERFORATED WORKPIECES IN A STRESS-RELIEVING MANNER
    1.
    发明申请
    METHOD FOR PRODUCING PERFORATED WORKPIECES IN A STRESS-RELIEVING MANNER 审中-公开
    在应力消除器中生产执行工件的方法

    公开(公告)号:US20130340480A1

    公开(公告)日:2013-12-26

    申请号:US13807411

    申请日:2011-06-04

    IPC分类号: C03B21/06

    摘要: A method for producing perforated work pieces from glass, glass ceramics, or semiconductors in a stress-relieving manner is provided. The method includes heating the work piece up to the glass transition temperature and perforating the work piece using a high-voltage electric field of suitable frequency or pulse shape. Then, the perforated work piece is allowed to cool down from the transition temperature range to room temperature at a rate at which the mechanical stresses generated by the perforation process relax.

    摘要翻译: 提供了一种从玻璃,玻璃陶瓷或半导体中产生应力消除方式的多孔工件的制造方法。 该方法包括将工件加热至玻璃化转变温度,并使用合适频率或脉冲形状的高压电场对工件进行穿孔。 然后,将穿孔工件从穿过过程产生的机械应力放松的速度从过渡温度范围冷却至室温。

    Rare earth doped luminescent glass
    6.
    发明申请
    Rare earth doped luminescent glass 审中-公开
    稀土掺杂发光玻璃

    公开(公告)号:US20050253113A1

    公开(公告)日:2005-11-17

    申请号:US11116044

    申请日:2005-04-27

    摘要: A white cold light source uses an LED or a gas discharge lamp and a luminescent rare earth doped glass comprising multiple rare earth cations and a particularly high total rare earth content to generate white light emission. Preferably, the luminescent glass has a 2700K to 7000K black body temperature and color rendering index value exceeding 80. A first embodiment of the glass is composed primarily of P2O5, Al2O3, and alkaline earth and alkali metal oxides, and possesses other properties such as physical and thermal properties that are compatible with conventional melting, forming and other manufacturing steps. Other embodiments of the luminescent glass have a maximum water content of 0.1 wt-% and do not contain any boron. Also the luminescent glass is preferably free of water, boron oxides and nitrides. The luminescent glass can be used as a wavelength converter to produce bright white light emission when pumped by conventional commercially available blue and UV light emitting diode sources.

    摘要翻译: 白色冷光源使​​用LED或气体放电灯以及包含多种稀土阳离子和特别高的总稀土含量的发光稀土掺杂玻璃以产生白光发射。 优选地,发光玻璃具有2700K至7000K黑色体温和显色指数值超过80.玻璃的第一实施方案主要由P 2 O 5 O 5组成, Al 2 O 3 O 3和碱土金属和碱金属氧化物,并且具有与常规熔融,成型和其它制造步骤相容的其它性能如物理和热性能。 发光玻璃的其它实施方案的最大含水量为0.1重量%,不含硼。 此外,发光玻璃优选不含水,氧化硼和氮化物。 当通过常规市售的蓝色和UV发光二极管源泵浦时,发光玻璃可用作波长转换器以产生明亮的白色发光。

    Borosilicate glass with high chemical resistance and use thereof
    8.
    发明授权
    Borosilicate glass with high chemical resistance and use thereof 有权
    具有高耐化学性的硼硅酸盐玻璃及其用途

    公开(公告)号:US06794323B2

    公开(公告)日:2004-09-21

    申请号:US10088618

    申请日:2002-08-13

    IPC分类号: C03C3091

    摘要: The borosilicate glass has a hydrolytic stability class of 1, an acid resistance class of 1 and a lye resistance class of at least 2 and a composition (in % by weight, based on oxide) of SiO2 70.5-76.5; B2O36.5-

    摘要翻译: 硼硅酸盐玻璃的水解稳定性等级为1,耐酸性等级为1,碱碱度等级为至少2,组成(按重量计,基于氧化物)为SiO2 70.5-76.5; B2O36.5- <11.5; AL2O3 4-8; Li2O 0.5-2; Na2O 4.5-9; K2O 0-5; Li2O + Na2O + K2O 5.5-10.5; MgO 0-1; CaO 0-2; 和CeO 2 0-1,以及任选的澄清剂。 该硼硅酸盐玻璃优选不含As 2 O 3,Sb 2 O 3和BaO,因此作为药物包装材料是特别有利的。 它还可以含有高达3重量%的TiO 2以阻挡UV辐射。 硼硅酸盐玻璃可以包括至多0.5重量%的ZrO 2以达到碱碱度等级1。