公开(公告)号:US10436973B2
公开(公告)日:2019-10-08
申请号:US15362120
申请日:2016-11-28
Applicant: Lextar Electronics Corporation
Inventor: Hung-Chia Wang , Xue-Jie Zhang , Shin-Ying Lin , An-Cih Tang , Ru-Shi Liu , Tzong-Liang Tsai , Yu-Chun Lee , Ching-Yi Chen , Hung-Chun Tong
IPC: F21V8/00 , C09K11/66 , H01L25/075 , H01L33/50 , H01L33/56 , H01L33/62 , C09K11/02 , B82Y20/00 , B82Y40/00
Abstract: A quantum dot composite material and a manufacturing method and an application thereof are provided. The quantum dot composite material includes an all-inorganic perovskite quantum dot and a modification protection on a surface of the all-inorganic perovskite quantum dot. The all-inorganic perovskite quantum dot has a chemical formula of CsPb(ClaBr1-a-bIb)3, wherein 0≤a≤1, 0≤b≤1.
-
2.
公开(公告)号:US20180105744A1
公开(公告)日:2018-04-19
申请号:US15725434
申请日:2017-10-05
Applicant: Lextar Electronics Corporation
Inventor: Ren-Hong Wang , Wen-Li Zhou , Ru-Shi Liu , Ching-Yi Chen , Wen-Wan Tai , Yu-Chun Lee , Tzong-Liang Tsai
CPC classification number: C09K11/675 , H01L33/06 , H01L33/46 , H01L33/502
Abstract: A fluoride phosphor including a sheet-like crystal and a manufacturing method and an application therefore are disclosed. The fluoride phosphor has a chemical formula A2[MF6]:Mn4+, with Mn4+ as an activator. The A is Li, Na, K, Rb, Cs, NH4 or a combination thereof. The M is Ge, Si, Sn, Ti, Zr or a combination thereof. The sheet-like crystal has a thickness d. A crystal flat surface of the sheet-like crystal has a maximum length a. The maximum length a is defined as a distance between two end points on an edge of the crystal flat surface and farthest from each other. 8≤a/d≤35.
-
公开(公告)号:US09966505B2
公开(公告)日:2018-05-08
申请号:US14887451
申请日:2015-10-20
Applicant: Lextar Electronics Corporation
Inventor: Ching-Yi Chen , Hung-Chun Tong , Li-Cheng Yang , Wen-Wan Tai , Yu-Chun Lee , Tzong-Liang Tsai
CPC classification number: H01L33/504 , G02B6/0003 , G02B6/0035 , G02B6/0073
Abstract: The present disclosure provides a light emitting structure including a blue light source, a first fluorescent material layer and a second fluorescent material layer. The blue light source has a light emitting surface. The first fluorescent material layer covers the light emitting surface of the blue light source. The first fluorescent material layer consists of a first fluorescent material. An excitation band of the first fluorescent material is in a blue wave band, and an emission band of the first fluorescent material is in a green wave band. The second fluorescent material layer covers the first fluorescent material layer. The second fluorescent material layer consists of a second fluorescent material. An excitation band of the second fluorescent material is in a green wave band, and an emission band of the second fluorescent material is in a red wave band. A light device and a backlight module are also provided herein.
-
公开(公告)号:US20170190968A1
公开(公告)日:2017-07-06
申请号:US15364207
申请日:2016-11-29
Applicant: LEXTAR ELECTRONICS CORPORATION
Inventor: Wen-Li Zhou , Wei- Lun Wu , Ru-Shi Liu , Yu-Chun Lee , Ching-Yi Chen , Tzong-Liang Tsai
CPC classification number: C09K11/665 , C30B7/14 , C30B29/12
Abstract: The present disclosure provides a method for fabricating a phosphor. A first solution is formed by dissolving potassium hexafluorogermanate (K2GeF6) and either K2MnF6 or KMnO4 in a hydrofluoric acid solution. An anhydrous ethanol is added to the first solution to make a total concentration of fluoride ions of potassium hexafluorogermanate (K2GeF6), hydrofluoric acid, and either K2MnF6 or KMnO4 equal to or less than 48M to form a precipitate. Afterward, the precipitate is collected.
-
公开(公告)号:US20170155020A1
公开(公告)日:2017-06-01
申请号:US15358339
申请日:2016-11-22
Applicant: Lextar Electronics Corporation
Inventor: Shin-Ying Lin , Hung-Chia Wang , An-Cih Tang , Ru-Shi Liu , Tzong-Liang Tsai , Yu-Chun Lee , Ching-Yi Chen , Hung-Chun Tong
CPC classification number: H01L33/502 , B82Y20/00 , C09K11/665 , H01L27/153 , H01L33/38 , H01L33/44 , H01L33/504 , H01L33/505 , H01L33/507 , H01L33/60 , H01L33/62 , H01L2224/48091 , H01L2224/49111 , H01L2224/73265 , H01L2933/0083 , Y10S977/774 , Y10S977/813 , Y10S977/95 , H01L2924/00014
Abstract: A wavelength-converting material and an application thereof are provided. The wavelength-converting material includes an all-inorganic perovskite quantum dot having a chemical formula of CsPb(ClaBr1-a-bIb)3, wherein 0≦a≦1, 0≦b≦1.
-
公开(公告)号:US20170153382A1
公开(公告)日:2017-06-01
申请号:US15362120
申请日:2016-11-28
Applicant: Lextar Electronics Corporation
Inventor: Hung-Chia Wang , Xue-Jie Zhang , Shin-Ying Lin , An-Cih Tang , Ru-Shi Liu , Tzong-Liang Tsai , Yu-Chun Lee , Ching-Yi Chen , Hung-Chun Tong
CPC classification number: G02B6/0073 , B82Y20/00 , B82Y40/00 , C09K11/025 , C09K11/665 , G02B6/0031 , G02B6/0051 , H01L25/0753 , H01L33/504 , H01L33/56 , H01L33/62 , H01L2224/48091 , H01L2224/49111 , H01L2224/73265 , H01L2933/0041 , Y10S977/774 , Y10S977/892 , Y10S977/95 , H01L2924/00014
Abstract: A quantum dot composite material and a manufacturing method and an application thereof are provided. The quantum dot composite material includes an all-inorganic perovskite quantum dot and a modification protection on a surface of the all-inorganic perovskite quantum dot. The all-inorganic perovskite quantum dot has a chemical formula of CsPb(ClaBr1-a-bIb)3, wherein 0≦a≦1, 0≦b≦1.
-
公开(公告)号:US20170137707A1
公开(公告)日:2017-05-18
申请号:US15253688
申请日:2016-08-31
Applicant: LEXTAR ELECTRONICS CORPORATION
Inventor: Ye Jin , Ru-Shi Liu , Yu-Chun Lee , Ching-Yi Chen , Tzong-Liang Tsai
CPC classification number: C09K11/617 , H01L33/502 , H01L33/504 , H01L2224/48091 , H01L2224/48247 , H01L2224/48257 , H01L2224/49107 , H01L2224/73265 , H01L2933/0041 , H01L2924/00014
Abstract: The present invention provides a method for fabricating a fluoride phosphor. A first solution is formed by dissolving potassium fluoride (KF) and either K2MnF6 or KMnO4 in a hydrofluoric acid solution. A second solution is formed by mixing a surfactant and a silane. The first solution and the second solution are mixed to form a precipitate. The precipitate is collected after the first solution and the second solution are mixed. The present invention also provides a fluoride phosphor represented by the following formula: K2[SiF6]:Mn4+. The fluoride phosphor has a particle size in a range of about 1 μm to about 10 μm. The present invention further provides a light-emitting apparatus and backlight module employing the same.
-
8.
公开(公告)号:US20180122999A1
公开(公告)日:2018-05-03
申请号:US15793026
申请日:2017-10-25
Applicant: Lextar Electronics Corporation
Inventor: Ching-Yi Chen , Wen-Wan Tai , Yu-Chun Lee , Tzong-Liang Tsai
CPC classification number: H01L33/502 , C09K11/727 , C09K11/7774 , F21K9/64 , F21V9/30 , F21Y2115/10 , H01L25/0753 , H01L33/0095 , H01L33/507 , H01L33/56 , H01L2224/32225 , H01L2224/48091 , H01L2224/48227 , H01L2224/73265 , H01L2924/12041 , H01L2924/00012 , H01L2924/00014
Abstract: A wavelength-converting film and a light emitting device and a display device using the same are disclosed. The wavelength converting film comprises a fluoride phosphor powder with a Mn4+ as an activator, wherein the fluoride phosphor powder with the Mn4+ as the activator comprises a sheet-like crystal and has a chemical formula of A2[MF6]:Mn4+, wherein A is Li, Na, K, Rb, Cs, NH4, or a combination thereof, and M is Ge, Si, Sn, Ti, Zr, or a combination thereof.
-
9.
公开(公告)号:US10023794B2
公开(公告)日:2018-07-17
申请号:US15725434
申请日:2017-10-05
Applicant: Lextar Electronics Corporation
Inventor: Ren-Hong Wang , Wen-Li Zhou , Ru-Shi Liu , Ching-Yi Chen , Wen-Wan Tai , Yu-Chun Lee , Tzong-Liang Tsai
CPC classification number: C09K11/675 , H01L33/06 , H01L33/46 , H01L33/502
Abstract: A fluoride phosphor including a sheet-like crystal and a manufacturing method and an application therefore are disclosed. The fluoride phosphor has a chemical formula A2[MF6]:Mn4+, with Mn4+ as an activator. The A is Li, Na, K, Rb, Cs, NH4 or a combination thereof. The M is Ge, Si, Sn, Ti, Zr or a combination thereof. The sheet-like crystal has a thickness d. A crystal flat surface of the sheet-like crystal has a maximum length a. The maximum length a is defined as a distance between two end points on an edge of the crystal flat surface and farthest from each other. 8≤a/d≤35.
-
公开(公告)号:US10020430B2
公开(公告)日:2018-07-10
申请号:US15162531
申请日:2016-05-23
Applicant: LEXTAR ELECTRONICS CORPORATION
Inventor: Hoang Duy Nguyen , Ren Hong Wang , Chaochin Su , Ru-Shi Liu , Ching-Yi Chen , Yu-Chun Lee , Tzong-Liang Tsai
CPC classification number: H01L33/504 , C09K11/675 , H01L33/501 , H01L33/56 , H01L2224/16245 , H01L2224/48091 , H01L2224/48247 , H01L2224/48257 , H01L2924/181 , H01L2924/00014 , H01L2924/00012
Abstract: The present invention provides a phosphor with a preferred orientation represented by the following formula: A2[MF6]:Mn4+, wherein A is selected from a group consisting of Li, Na, K, Rb, Cs, and NH4, M is selected from a group consisting of Ge, Si, Sn, Ti, and Zr. The preferred orientation is a (001)/(011) preferred orientation. The present invention also provides a method for fabricating the above phosphor. The present invention further provides a light-emitting element package structure employing the same.
-
-
-
-
-
-
-
-
-