    摘要: A Ni-plated steel sheet is provided in which the occurrence of scratches at the time of forming a battery can is suppressed. Also provided is a method which includes a step where a surface of a steel sheet is plated with Ni in a Ni adhesion amount of 0.3-2 μm, a step where the Ni-plated steel sheet is heated to 600-800° C. to form an Fe−Ni diffusion layer as an outermost surface layer, and a step where the steel sheet is rolled by temper rolling so as to adjust the Fe−Ni diffusion layer so that the steel sheet has the surface roughness Ra of 0.9-2.0 μm and the surface roughness Ry of 4.0-15 μm. A Ni-plated steel sheet which includes an Fe−Ni diffusion layer as an outermost surface layer and in which the diffusion layer has the surface roughness Ra of 0.9-2.0 μm and the surface roughness Ry of 4.0-15 μm and the diffusion layer has such an Fe/Ni ratio that the Fe accounts for 20-50% in Auger analysis is subjected to drawing using a water-soluble liquid which contains water-soluble emersion as a press lubricant.

    摘要翻译: 提供了一种镀镍钢板,其中抑制了形成电池壳时的划痕的发生。 还提供了一种方法,其包括以0.3-2μm的Ni附着量将钢板的表面镀Ni的步骤,将镀Ni钢板加热至600-800℃至 形成作为最外表面层的Fe-Ni扩散层,并且通过回火轧制轧制钢板以调整Fe-Ni扩散层以使钢板的表面粗糙度Ra为0.9-2.0μm的步骤 表面粗糙度Ry为4.0〜15μm。 一种镀镍钢板,其包括Fe-Ni扩散层作为最外表面层,其中扩散层的表面粗糙度Ra为0.9-2.0μm,表面粗糙度Ry为4.0-15μm,扩散层具有 在俄歇分析中Fe占20-50%的Fe / Ni比例使用含有水溶性浸出物的水溶性液体作为压力润滑剂进行拉伸。