RESIN MOLDED ARTICLE FOR AUTOMOBILE INTERIOR MATERIAL
    4.
    发明申请
    RESIN MOLDED ARTICLE FOR AUTOMOBILE INTERIOR MATERIAL 有权
    用于汽车内饰材料的树脂模制品

    公开(公告)号:US20170044300A1

    公开(公告)日:2017-02-16

    申请号:US15306253

    申请日:2015-04-23

    Abstract: Provided is a resin molded article for an automobile interior material, the resin molded article achieving both resin strength permitting formation of a thin film, and crease resistance. This molded article is to be used in an automobile interior material, the resin molded article being obtained by slush-molding a powdered thermoplastic urethane urea resin composition (P) that satisfies (1)-(5) below, said resin composition (P) containing an additive and a thermoplastic urethane urea resin (U) obtained by reacting a high-molecular diol (a), a linear alkane diol (b), a monool (c), a diamine (d), and an organic diisocyanate (e): (1) (a) contains a specific polyester diol; (2) the weight of (b) is within a specific range relative to the total weight of (a)-(e); (3) the tensile strength of a film comprising (P) is 8.0 MPa or higher; (4) the storage modulus of (P) at 130° C. is 0.1-5.0 MPa; (5) the ratio of the storage modulus of (P) at 50° C. to the storage modulus at 23° C. by a specific measurement method is 50% or higher.

    Abstract translation: 提供了一种用于汽车内部材料的树脂模塑制品,该树脂模塑制品实现了能够形成薄膜的树脂强度和折皱性。 该模塑制品用于汽车内部材料中,该树脂模塑制品通过将满足下述(1) - (5)的粉末状热塑性聚氨酯脲树脂组合物(P),所述树脂组合物(P )包含通过高分子量二醇(a),直链烷二醇(b),单醇(c),二胺(d)和有机物(a))反应获得的添加剂和热塑性氨基甲酸酯脲树脂(U) 二异氰酸酯(e):(1)(a)含有特定的聚酯二醇; (2)(b)的重量相对于(a) - (e)的总重量在特定范围内; (3)包含(P)的膜的拉伸强度为8.0MPa以上; (4)130℃时(P)的储能模量为0.1-5.0 MPa; (5)采用特定的测定方法,50℃时(P)的储能模量与23℃下的储能模量的比例为50%以上。

    Polymer Manufacturing Process
    10.
    发明申请
    Polymer Manufacturing Process 有权
    聚合物制造工艺

    公开(公告)号:US20080236443A1

    公开(公告)日:2008-10-02

    申请号:US11693185

    申请日:2007-03-29

    Abstract: Embodiments relate to a relatively rapid transesterification process including transesterifying condensation polymers such as polyethylene terephthalate (PET), or other polyesters used in commerce, with a modifying monomer mix containing other monomers to manufacture new polymers containing the pre-condensed moieties. The process preferably only involves transesterification as a reaction mechanism. The process preferably produces a rapid buildup of molecular weight and/or polymer uniformity by the high temperature transesterification of the condensation polymer with the modifying monomer mixture. The process can be performed in any suitable vessel including an extrusion line, and it has the advantage of greatly reduced cycle times over currently used condensation polymer utilization processes such as the recycling of PET into other materials.

    Abstract translation: 实施方案涉及相对快速的酯交换方法,包括将缩合聚合物如聚对苯二甲酸乙二醇酯(PET)或商业使用的其它聚酯与含有其它单体的改性单体混合物酯交换反应以制备含有预缩合部分的新聚合物。 该方法优选仅涉及酯交换作为反应机理。 该方法优选通过缩合聚合物与改性单体混合物的高温酯交换产生分子量和/或聚合物均匀性的快速累积。 该方法可以在包括挤出生产线的任何合适的容器中进行,并且其优点在于比目前使用的缩合聚合物利用过程大大缩短了循环时间,例如将PET再循环到其它材料中。