Metal passivating agents
    45.
    发明授权
    Metal passivating agents 失效
    金属钝化剂

    公开(公告)号:US4919787A

    公开(公告)日:1990-04-24

    申请号:US335069

    申请日:1989-04-07

    IPC分类号: B01J33/00 C10G11/05

    摘要: An improved method for passivating metals in a hydrocarbon feedstock during catalytic cracking has been discovered. The method involves contacting the feedstock with a passivating agent comprising a precipitated porous rare earth oxide, alumina, and aluminum phosphate precipitate. The passivating agent may be coated on a cracking catalyst, be part of the matrix of a cracking catalyst, or be added to the cracking operation as discrete particles.

    摘要翻译: 已经发现了一种在催化裂化过程中钝化烃原料中的金属的改进方法。 该方法包括使原料与包含沉淀的多孔稀土氧化物,氧化铝和磷酸铝沉淀物的钝化剂接触。 钝化剂可以涂覆在裂化催化剂上,作为裂化催化剂的基质的一部分,或作为离散颗粒加入到裂化操作中。

    Lanthana-alumina-aluminum phosphate catalyst composition
    46.
    发明授权
    Lanthana-alumina-aluminum phosphate catalyst composition 失效
    氧化镧 - 磷酸铝 - 磷酸铝催化剂组合物

    公开(公告)号:US4873216A

    公开(公告)日:1989-10-10

    申请号:US283778

    申请日:1988-12-13

    IPC分类号: B01J27/18 B01J35/10 C10G45/04

    摘要: This invention relates to a new catalyst composition. The catalyst composition comprises a catalytic component and a support comprising an amorphous combination of lanthana, alumina and aluminum phosphate, and may be characterized after calcination by a pore size distribution including about 5 to 20 vol. % within the pore size diameter range of 50 to 100 Angstroms, about 10 to 35 vol. % within the pore size diameter range of 100 to 150 Angstroms, about 15 to 50 vol. % within the pore size diameter range of 150 to 200 Angstroms and about 10 to 50 vol. % within the pore size diameter range of 200 to 400 Angstroms.