Abstract:
The invention is directed to a coating formulation for preparing a hydrophilic coating a hydrophilic polymer, a Norrish Type II photoinitiator, comprising a substituted benzohenone, xanthone, tioxanthone or anthraquinone, and more than 70 wt % of a carrier liquid; to a method of forming a hydrophilic coating on a substrate, the method comprising: applying a coating formulation to at least one surface of an article and allowing the coating formulation to cure for a time period less than 360 seconds; and to an article comprising at least one hydrophilic coating.
Abstract:
Spin finish having solid microparticles of a specified kind dispersed colloidally at a specified ratio in a dispersoid of a specified kind containing a smoothing agent component of a specified kind and a nitrogen-containing compound of a specified kind at specified ratios is for elastomer fibers such that packages having superior roll shape and unwinding property can be obtained in the production and fabrication process.
Abstract:
The present invention has for its object a prefabricated sealing membrane formed by a support, coated on at least one surface, and preferably impregnated throughout, with a modified bitumen base composition, characterized in that the thermoplastic bituminous composition for coating and/or impregnation is a bituminous binder modified by a thermoplastic polyurethane having the following weight proportion: 40 to 90% bitumen, 10 to 50% thermoplastic polyurethane, 0 to 10% aromatic oil, 0 to 50% filler, 0 to 0.5% catalyst.
Abstract:
The invention provides an anti-corrosive package which can be added to release agents used in preparing textiles and molded articles from lignocellulosic materials, concrete and polyurethane foam.
Abstract:
The present invention provides a polyolefin-based composite resin spherical particle that gives a coating film having a matte appearance, a soft feeling, and excellent scratch resistance by being used for a coating material. The present invention also provides a coating composition containing the polyolefin-based composite resin spherical particle and a coating resin, and a coated article obtained by applying the coating composition to a substrate.The invention relates to a polyolefin-based composite resin spherical particle, which is a spherical particle obtained by mixing 100 parts by mass of a polyolefin-based resin, 40 to 1,500 parts by mass of water, and 3 to 30 parts by mass of an ethylene oxide/propylene oxide copolymer having a weight average molecular weight of 4,000 to 30,000 to prepare a mixture, emulsifying the mixture at a temperature of the highest melting point of the polyolefin-based resin or higher, and cooling the mixture from a temperature at least 25° C. higher than the highest crystallization temperature of the polyolefin-based resin to a temperature at least 25° C. lower than the lowest crystallization temperature of the polyolefin-based resin at a cooling speed of 0.2° C./min or more, wherein the polyolefin-based resin is a composite resin containing 5 to 70% by mass of a partially saponified ethylene/vinyl acetate copolymer.
Abstract:
An improved method for lowering the surface tension of coating compositions wherein a surfactant is contacted with the coating composition, wherein the improvement comprises contacting said coating composition with a surfactant having mono-substituted fluorophosphates present at greater than or equal to 50 mol % than bis-substituted phosphates and substrates treated with the coating composition.
Abstract:
To provide metal microparticles, with less content of alkali metal, halogen, sulfur, and phosphorus as impurities, wherein surfaces thereof are coated with a protective agent, and the protective agent is selected from at least one type of an amine compound and a calboxylic acid compound, and a total content of the alkali metal, halogen, sulfur, and phosphorus contained in the metal microparticles is less than 0.1 mass % relative to a mass of the metal microparticles.
Abstract:
Disclosed is a cellulose ester optical film containing cellulose ester, a polymer (a) below and a compound (b) below: (a) a polymer obtained by copolymerization of an ethylenically unsaturated monomer having in the molecule a partial structure represented by formula (1) below with at least one ethylenically unsaturated monomer, and (b) at least one compound selected from the group consisting of a compound represented by formula (2) below and a compound represented by formula (3) below,
Abstract:
Presently described are self-assembling antireflective (“AR”) coating compositions comprising high refractive index surface modified nanoparticles. Also described are various articles such as protective films, optical displays, and windows, comprising such (e.g. dried and cured) AR coating.
Abstract:
The invention relates to a liquid bis(acyl)phosphine oxide of formula (I): wherein R is C1-C18 alkyl, and wherein R is optionally substituted as described herein. The invention also relates to radiation curable compositions comprising liquid bis(acyl)phosphine oxide of formula (I).