METHOD FOR MANUFACTURING A COMPOSITE COMPONENT OF A TIMEPIECE OR OF A JEWELRY PART, AND COMPOSITE COMPONENT OBTAINABLE BY SUCH METHOD

    公开(公告)号:US20220133003A1

    公开(公告)日:2022-05-05

    申请号:US17575758

    申请日:2022-01-14

    Abstract: The invention relates to a method for manufacturing a composite component of a timepiece or of a jewelry part, the composite component comprising a porous ceramic part and a metallic material filling the pores of said ceramic part, said method comprising the steps of: providing a porous ceramic preform of the component, providing a metallic material, heating the metallic material to a temperature higher than the melting point of the metallic material, filling the pores of the ceramic preform with the molten metallic material, cooling the metallic material and the ceramic preform to obtain a solidified metallic material in the pores of the ceramic preform, and applying finishing treatments to obtain the composite component, wherein said porous ceramic preform consists essentially of a material selected from the group consisting of Si3N4, SiO2 and mixtures thereof, and said metallic material is selected from the group consisting of gold, platinum, palladium metals and alloys of these metals.
    The invention relates also to a composite component of a timepiece or of a jewelry part comprising a porous ceramic part and a metallic material filling the pores of said ceramic part, wherein said porous ceramic part consists essentially of a material selected from the group consisting of Si3N4, SO2 and mixtures thereof, and said metallic material which is selected from the group consisting of gold, platinum, palladium metals and alloys of these metals.

    NICKEL-FREE ZIRCONIUM AND/OR HAFNIUM-BASED BULK AMORPHOUS ALLOY
    7.
    发明申请
    NICKEL-FREE ZIRCONIUM AND/OR HAFNIUM-BASED BULK AMORPHOUS ALLOY 有权
    无镍基和/或基于高铌的大块非晶合金

    公开(公告)号:US20170038733A1

    公开(公告)日:2017-02-09

    申请号:US15188588

    申请日:2016-06-21

    CPC classification number: G04B37/22 C22C1/002 C22C45/10

    Abstract: Nickel-free bulk amorphous alloy, formed, in atomic percent, of: a zirconium and/or hafnium base, forming the balance, with a total zirconium and hafnium value greater than or equal to 52.0, and less than or equal to 62.0; copper: greater than or equal to 16.0, and less than or equal to 28.0; iron: greater than or equal to 0.5, and less than or equal to 10.0; aluminium: greater than or equal to 7.0, and less than or equal to 13.0; at least two additional metals taken from the family including Ti, V, Nb, Y, Cr, Mo, Co, Sn, Zn, P, Pd, Ag, Au, Pt, Ta, Ru, Rh, Ir, Os, and Hf when the base contains none, and Zr when the base contains none, with the cumulative atomic percentage of these additional metals being greater then 6.0 and less than or equal to 10.0.

    METHOD FOR MANUFACTURING AN AMORPHOUS METAL PART

    公开(公告)号:US20190262896A1

    公开(公告)日:2019-08-29

    申请号:US15776861

    申请日:2016-10-11

    Abstract: A method for manufacturing a micromechanical component made of a first material, the first material being a material that can become at least partially amorphous, the method including: a) providing a mold made of a second material, the mold including a cavity forming the negative of the micromechanical component; b) providing the first material and forming the first material in the cavity of the mold, the first material having undergone, at a latest at a time of the forming, treatment allowing the first material to become at least partially amorphous; c) separating the micromechanical component thus formed from the mold.