COATING METHOD FOR A WORKPIECE
    1.
    发明申请
    COATING METHOD FOR A WORKPIECE 审中-公开
    工作涂料方法

    公开(公告)号:US20110000793A1

    公开(公告)日:2011-01-06

    申请号:US12919697

    申请日:2009-02-20

    摘要: The invention relates to a coating method for a workpiece, including the following method steps: a) applying a coating liquid to the workpiece, wherein the coating liquid comprises an ionic liquid containing ions of at least one element, b) electrochemically depositing a layer of the at least one element from the coating liquid on the workpiece, c) removing the workpiece from the coating liquid, d) removing excess coating liquid from the workpiece. In order to suggest an industrially suitable coating process, particularly for workpieces having at least a partial metal surface, using stable, durable baths, it is provided that the temperature of the workpiece is set such that the temperature of the coating liquid deviates by no more than 10° C. from a predetermined set temperature during the coating process

    摘要翻译: 本发明涉及一种用于工件的涂覆方法,包括以下方法步骤:a)将涂布液施加到工件上,其中涂布液体包含含有至少一种元素离子的离子液体,b)电化学沉积一层 来自工件上的涂覆液体的至少一种元素,c)从涂布液中去除工件,d)从工件中去除多余的涂布液体。 为了提出工业上合适的涂覆方法,特别是对于具有至少部分金属表面的工件,使用稳定,耐用的浴,可以将工件的温度设定为使涂层液体的温度不再偏离 在涂布过程中从预定的设定温度超过10℃

    Weldable Corrosion-Protective Agent and Binder Therefor
    2.
    发明申请
    Weldable Corrosion-Protective Agent and Binder Therefor 审中-公开
    可焊接防腐剂及其粘合剂

    公开(公告)号:US20080226923A1

    公开(公告)日:2008-09-18

    申请号:US12066266

    申请日:2006-09-08

    摘要: The invention relates to a binding agent comprising at least one titanium and/or one zircon compound (at least 0.5 wt. % in relation to 100 wt. % binding agent), at least one organo-functional silan, in particular, a monosilan, and a solution. The invention is characterised in that the binding agent comprises at least one fluorinated polymer which is insoluble in the binding agent solution. The invention also relates to a corrosion protection agent which is produced using the binding agent and a weldable corrosion protection agent, in addition to a workpiece which is coated with the inventive corrosion protection agent.

    摘要翻译: 本发明涉及包含至少一种钛和/或一种锆石化合物(相对于100重量%粘合剂为至少0.5重量%)的粘合剂,至少一种有机官能硅烷,特别是单硅氧烷, 和解决方案。 本发明的特征在于粘合剂包含至少一种不溶于粘合剂溶液的含氟聚合物。 本发明还涉及除了涂有本发明的防腐蚀剂的工件之外,还使用粘结剂和可焊接防腐蚀剂制造的防腐剂。

    Corrosion Control Coating Composition For Metal Workpieces and Method of Producing Same
    3.
    发明申请
    Corrosion Control Coating Composition For Metal Workpieces and Method of Producing Same 审中-公开
    金属工件的腐蚀控制涂料组合物及其制备方法

    公开(公告)号:US20080193743A1

    公开(公告)日:2008-08-14

    申请号:US11632628

    申请日:2005-07-07

    摘要: The invention relates to an anti-corrosive coating agent for metal workpieces. For the purpose of good cathodic corrosion prevention, the anti-corrosive coating agent comprises an organic binder having a silicon-organic compound and particulate metal. The workpiece having an anti-corrosive coating is characterized in that the anti-corrosive coating comprises an organic binder having a silicon-organic compound and particulate metal. The method for producing an anti-corrosive coating on a workpiece is characterized by applying, in liquid form, a first coating, comprising an organic binder having a silicon-organic compound and particulate metal as the anti-corrosive coating, and then applying a second coating the composition of which preferably differs from that of the anti-corrosive coating.

    摘要翻译: 本发明涉及一种用于金属工件的防腐蚀涂层剂。 为了防止良好的阴极腐蚀,防腐涂料包括具有硅 - 有机化合物和颗粒状金属的有机粘合剂。 具有防腐蚀涂层的工件的特征在于防腐涂层包括具有硅 - 有机化合物和颗粒状金属的有机粘合剂。 用于在工件上生产防腐涂层的方法的特征在于以液体形式施加第一涂层,其包括具有硅有机化合物和颗粒金属的有机粘合剂作为防腐蚀涂层,然后施加第二涂层 涂覆其组成优选不同于防腐涂层的组合物。