Abstract:
The invention relates to a substrate (1, 10) for electrical circuits, comprising at least one metal layer (2, 3, 14) and a paper ceramic layer (11), which is joined face to face with the at least one metal layer (2, 3, 14) and has a top side and bottom side (11a, 11b), wherein the paper ceramic layer (11) has a large number of cavities in the form of pores. Especially advantageously, the at least one metal layer (2, 3, 14) is connected to the paper ceramic layer (11) by means of at least one glue layer (6, 6a, 6b), which is produced by applying at least one glue (6a', 6a'', 6b', 6b'') to the metal layer (2, 3, 14) and/or to the paper ceramic layer (11), wherein the cavities in the form of pores in the paper ceramic layer (11) are filled at least at the surface by means of the applied glue (6a', 6a'', 6b', 6b'').
Abstract:
An article comprises a substrate; a coating comprising a carbon composite; and a binding layer disposed between the substrate and the coating. The carbon composite comprises carbon and a binder containing one or more of the following: SiO2; Si; B; B2O3; a metal; or an alloy of the metal; and the metal comprises one or more of the following: aluminum; copper; titanium; nickel; tungsten; chromium; iron; manganese; zirconium; hafnium; vanadium; niobium; molybdenum; tin; bismuth; antimony; lead; cadmium; or selenium.
Abstract:
A method of finishing a laminated glass structure (102) comprising a flexible glass sheet (130) having a thickness of no greater than about 0.3 mm laminated to a non-glass substrate (116) by an adhesive layer (135) is provided. The method includes applying a compressive force against a cut edge (106) of the flexible glass sheet (130) using an abrasive surface (108) of a hand-held finishing tool (105). Material of the laminated glass structure (102) is removed at the cut edge (106) such that a glass edge strength of the flexible glass sheet (130) is at least about 50 MPa.
Abstract:
Disclosed is a semi-amorphous, ductile brazing foil with a composition consisting essentially of NibalFeaCrbPcSidBeMof with approximately 30 atomic percent≤a≤approximately 38 atomic percent; approximately 10 atomic percent≤b≤approximately 20 atomic percent; approximately 7 atomic percent≤c≤approximately 20 atomic percent; approximately 2 atomic percent≤d≤approximately 4 atomic percent; e≤approximately 2 atomic percent; f≤approximately 5 atomic percent; and the balance being Ni and other impurities; where c+d+e
Abstract:
A carbon composite contains expanded graphite; and at least one of a filler or a reinforcement; wherein the expanded graphite comprises a plurality of randomly oriented basal planes. Methods of making the carbon composite and articles comprising the carbon composite are also disclosed.
Abstract:
A heat ray shielding material comprising a metal particle-containing layer that contains at least one kind of metal particle and an overcoat layer that is in close contact with at least one surface of the metal particle-containing layer, wherein hexagonal to circular tabular metal particles are contained in 60% by number or more relative to total number of the metal particles contained in the metal particle-containing layer, a main plane of the hexagonal to circular, tabular metal particles is plane-oriented in a range of from 0° to ±30° on average relative to one surface of the metal particle-containing layer, and the overcoat layer contains fine particles, exhibits favorable adhesion-failure resistance, scratch resistance and low haze.