A composite material having a substrate material and at least one barrier coating on one side of the substrate material. The barrier coating is plasma impulse chemical vapor deposited (PICVD) to the substrate material. The barrier coating includes at least one of material selected from the group consisting of SiOx, TiOx, SnOx, Si3Ny, Nb2Oy, and Al2Oy.
摘要翻译:一种复合材料,其具有衬底材料和在衬底材料的一侧上的至少一个阻挡涂层。 阻挡涂层是等离子体脉冲化学气相沉积(PICVD)到基底材料。 阻挡涂层包括选自SiO x,TiO x,SnO x,Si 3 N y,Nb 2 O y和Al 2 O y的材料中的至少一种。
摘要:
A process for applying alternating layers by chemical vapor deposition comprises the process steps of depositing an adhesion-promoter layer on a substrate and applying a barrier layer. Alternating layers comprising organic and inorganic materials are deposited alternately, and in this process the coating time for application of the adhesion-promoter layer is between 0.05 s and 4.0 s and the coating time for application of the inorganic barrier layer is between 0.1 s and 6.0 s. A composite material is also produced using the process.
摘要:
The invention describes a process for applying alternating layers by chemical vapor deposition which comprises the process steps of depositing an adhesion-promoter layer on a substrate and of applying a barrier layer, alternating layers comprising organic and inorganic materials being deposited alternately, in which process the coating time for application of the adhesion-promoter layer is between 0.05 s and 4.0 s and the coating time for application of the inorganic barrier layer is between 0.1 s and 6.0 s, and also a composite material produced using the process.
摘要:
A transparent, colorless glass or glass-ceramic panel has a visually dense, high-temperature-stable coating having an organic/inorganic network structure containing filling material particles and a color-imparting pigment. The mechanically stable, visually dense coating has no melt-reaction zone at the surface of the panel, which is coated with the coating, so that it does not impair the panel strength. The inorganic network structure can be made from a SiO2-based sol. The coating is made by introducing the color-imparting pigment and the filling material particles into a reactive organic/inorganic network structure; applying the resulting organic/inorganic network structure containing the pigment and the filling material particles to the panel to coat the panel and then burning-in the organic/inorganic network structure with the pigment and the filling material particles under thermal conditions to form the coating with no melt-reaction zone.
摘要:
A method for producing optical functional coatings comprising niobium, tantalum, titanium or aluminum by supplying a precursor gas of low vapor pressure in a CVD coating system. A precursor selected from the group consisting of Nb, Ta, Ti, and Al compounds having a vapor pressure is maintained within a first supply container at a first temperature T1 and a first pressure p1. Precursor vapor of the precursor is supplied from the first supply container to an intermediate storage device through a first gas line which fluidly communicates the first supply container and the intermediate storage device. A carrier gas or reaction gas is supplied to the first gas line such that a mixture of the precursor with the carrier gas or the reaction gas is provided. The mixture is maintained in the intermediate storage device at a constant second pressure p2 lower than the first pressure p1 and at a second temperature T2 lower than the first temperature T1, and the mixture is supplied from the intermediate storage device through a second gas line.
摘要:
A protective layer having at least one hard-material layer is provided. The hard-material layer is formed from one or more of the following materials metal oxide, metal nitride, metal carbide, metal oxynitride, metal carbonitride, and metal oxycarbonitride. The hard-material layer has laterally closely cohesive, crystalline columns which grow perpendicular to the surface of the body. In some embodiments, the crystalline columns have a lateral dimension which is on average less than 1 μm, preferably less than 200 nm, and which predominantly has crystal orientations which, in the case of columnar growth, have little tendency to widen out, the surface roughness of the hard-material layer having an Ra value of less than 50 nm, preferably less than 20 nm.
摘要:
Many applications, in particular in the domestic sector, require bodies which have a protective layer with a high scratch resistance and thermal stability. One typical example is glass-ceramic cooking surfaces of modern cooking hobs. The invention provides a corresponding protective layer which comprises at least one hard-material layer formed from a metal oxide and/or metal nitride and/or metal carbide and/or metal oxynitride and/or metal carbonitride and/or metal oxycarbonitride which has laterally closely cohesive, crystalline columns which grow perpendicular to the surface of the body and the lateral dimension of which is on average less than 1 μm, preferably less than 200 nm, and which predominantly has crystal orientations which, in the case of columnar growth, have little tendency to widen out, the surface roughness of the hard-material layer having an Ra value of less than 50 nm, preferably less than 20 nm.
摘要:
A glass-ceramic cooktop is provided that is made of glass-ceramic material with a flat upper side and an underside. The glass-ceramic material has transmittance values of greater than 0.1% in the visible light range in the total wavelength region greater than 420 nm, a light transmittance in the visible range of 0.8-2.5%, and a transmittance of 0-85% in the infrared at 1600 nm, and wherein the glass-ceramic material has high quartz mixed crystals as the prevalent crystal phase. The underside is flat, unstructured, and coplanar with the upper side.
摘要:
A transparent, colorless glass or glass-ceramic panel has a visually dense, high-temperature-stable coating having an organic/inorganic network structure containing filling material particles and a color-imparting pigment. The mechanically stable, visually dense coating has no melt-reaction zone at the surface of the panel, which is coated with the coating, so that it does not impair the panel strength. The inorganic network structure can be made from a SiO2-based sol. The coating is made by introducing the color-imparting pigment and the filling material particles into a reactive organic/inorganic network structure; applying the resulting organic/inorganic network structure containing the pigment and the filling material particles to the panel to coat the panel and then burning-in the organic/inorganic network structure with the pigment and the filling material particles under thermal conditions to form the coating with no melt-reaction zone.
摘要:
A scratchproof, temperature-stable protective layer, in particular a scratch-resistant protective layer for cooking hobs is provided. In addition, processes and an apparatus for producing these protective layers are provided. The protective layer includes at least one hard-material layer having a functional layer interrupted by very thin interlayers so that the functional layer has a morphologically dense columnar structure that grows substantially perpendicular to the body surface. The production of layers of this type is achieved by a magnetron sputtering process and a corresponding arrangement, with the tendency of the columnar structures to widen out being reduced by targeted interruption of the growth of the functional layers.