摘要:
It is made possible to provide a patterned perpendicular magnetic recording medium that has smaller write magnetic field and the variation of magnetic characteristics in the bit regions, generates fewer reversed magnetic domains in the position control information regions of the head, and has excellent thermal stability. A patterned perpendicular magnetic recording medium includes: a nonmagnetic substrate; a soft magnetic base layer formed on the nonmagnetic substrate; a nonmagnetic intermediate layer formed on the soft magnetic base layer; and a perpendicular magnetic recording layer formed on the nonmagnetic intermediate layer, and including a stacked structure of a CoPt-based crystalline film having a Pt content in the range of 5 atomic percent to 35 atomic percent and a rare-earth and transition metal alloy amorphous film formed on the CoPt-based crystalline film. The CoPt-based crystalline film and the rare-earth and transition metal alloy amorphous film are exchange-coupled.
摘要:
According to one embodiment, a magnetic recording medium includes a substrate, an auxiliary layer formed on the substrate, and at least one perpendicular magnetic recording layer formed on the auxiliary layer. The perpendicular magnetic recording layer includes a magnetic dot pattern. The perpendicular magnetic recording layer is made of an alloy material containing one element selected from iron and cobalt, and one element selected from platinum and palladium. This alloy material has the L10 structure, and is (001)-oriented. The auxiliary layer includes a dot-like first region covered with the magnetic dot pattern, and a second region not covered with the magnetic dot pattern. The first region is made of one metal selected from (100)-oriented nickel and (100)-oriented iron. The second region contains an oxide of the metal used in the first region.
摘要:
According to one embodiment, a magnetic recording medium includes a substrate, an auxiliary layer formed on the substrate, and at least one perpendicular magnetic recording layer formed on the auxiliary layer. The perpendicular magnetic recording layer includes a magnetic dot pattern. The perpendicular magnetic recording layer is made of an alloy material containing one element selected from iron and cobalt, and one element selected from platinum and palladium. This alloy material has the L10 structure, and is (001)-oriented. The auxiliary layer includes a dot-like first region covered with the magnetic dot pattern, and a second region not covered with the magnetic dot pattern. The first region is made of one metal selected from (100)-oriented nickel and (100)-oriented iron. The second region contains an oxide of the metal used in the first region.
摘要:
According to one embodiment, a magnetic recording medium includes a substrate, an auxiliary layer formed on the substrate, and at least one perpendicular magnetic recording layer formed on the auxiliary layer. The perpendicular magnetic recording layer includes a magnetic dot pattern. The perpendicular magnetic recording layer is made of an alloy material containing one element selected from iron and cobalt, and one element selected from platinum and palladium. This alloy material has the L10 structure, and is (001)-oriented. The auxiliary layer includes a dot-like first region covered with the magnetic dot pattern, and a second region not covered with the magnetic dot pattern. The first region is made of a (100)-oriented nickel oxide. The second region contains nickel used in the first region as a main component.
摘要:
A perpendicular magnetic recording medium includes a substrate, an underlayer formed on the substrate, and containing at least one element selected from the group A consisting of Pt, Pd, Rh, Ag, Au, Ir and Fe, and at least one element or compound selected from the group B consisting of C, Ta, Mo, W, Nb, Zr, Hf, V, Mg, Al, Zn, Sn, In, Bi, Pb, Cd, SiO2, MgO, Al2O3, TaC, TiC, TaN, TiN, B2O3, ZrO2, In2O3 and SnO2, and a magnetic layer formed on the underlayer, containing at least one element selected from the group consisting of Fe, Co, and Ni, and at least one element selected from the group consisting of Pt, Pd, Au and Ir, and containing crystal grains having an L10 structure.
摘要翻译:垂直磁记录介质包括衬底,形成在衬底上的底层,并且包含选自由Pt,Pd,Rh,Ag,Au,Ir和Fe组成的组A中的至少一种元素,以及至少一种元素或化合物 选自由C,Ta,Mo,W,Nb,Zr,Hf,V,Mg,Al,Zn,Sn,In,Bi,Pb,Cd,SiO 2,MgO组成的组B ,Al 2 O 3,TaC,TiC,TaN,TiN,B 2 O 3 3,ZrO 2 sub> 3 sub> 3< 2>和在底层上形成的含有至少一个元素的磁性层 选自Fe,Co和Ni中的至少一种元素,以及选自Pt,Pd,Au和Ir中的至少一种元素,并且含有具有L 1 O 3结构的晶粒。
摘要:
In one embodiment, a method of manufacturing a mold includes: forming a first layer having an affinity to a second polymer on a substrate having an affinity to a first polymer; forming first and second openings in the first layer; filling a resist in the second openings and hardening the resist to obtain a hardened resist; and forming a second layer containing a block copolymer and causing it to self-assemble.
摘要:
A pattern forming method according to an embodiment includes: forming a pattern film on a first substrate, the pattern film having a concave-convex pattern, the pattern film being made of a material containing a first to-be-imprinted agent; forming a material film on a second substrate, the material film containing a second to-be-imprinted agent having a higher etching rate than an etching rate of the first to-be-imprinted agent; transferring the concave-convex pattern of the pattern film onto the material film by applying pressure between the first substrate and the second substrate, with the pattern film being positioned to face the material film, and by curing the second to-be-imprinted agent; detaching the first substrate from the pattern film; and removing the material film by etching, to leave the pattern film on the second substrate.
摘要:
A fuel pump which can suppress fuel bubbles from being sucked into a fuel pressure chamber, and can achieve a stable fuel pressure property. The fuel pump has a pump body formed with a suction passage and a pump operation chamber, and a pressure pump mechanism to pressurize and discharge fuel. The pump body has a lower side wall portion and an upper side wall portion respectively at the vertically lower and upper sides of the inner wall portion forming a suction gallery chamber partly forming the suction passage. The pressure pump mechanism has a valve retaining member having an insertion portion inserted into the suction gallery chamber. The insertion portion has internal suction inlets through which the fuel is sucked from the suction gallery chamber into the pump operation chamber, the internal suction inlets being positioned in the intermediate height area in the suction gallery chamber.
摘要:
An object of the present invention is to provide a method for manufacturing a copper foil for a negative electrode current collector (specifically, copper foil for a negative electrode current collector of a lithium ion secondary battery) more excellent in discoloration resistance to improve charge/discharge cycle life of a secondary battery. To achieve the object, a method for manufacturing a copper foil for a negative electrode current collector of a secondary battery subjecting the copper foil to rust-proofing treatment, the method characterized in that the copper foil is rust-proofing treated with a chromate-treatment solution having pH in the range from 3.5 to 7.0 to form a chromate film on the surface of the copper foil is employed.
摘要:
An object of the present invention is to provide a copper foil excellent in softening resistance performance which reduces decrease in tensile strength after heat treatment at about 350° C. to 400° C. In order to achieve the object, a surface-treated copper foil provided with a rust-proofing treatment layer on both surfaces of a copper foil in which a rust-proofing treatment layer is constituted by zinc alloy, and the either rust-proofing treatment layer is a zinc alloy layer having zinc amount of 20 mg/m2 to 1,000 mg/m2; and the copper foil contains one or two or more of small amount elements selected from carbon, sulfur, chlorine and nitrogen, and a sum amount thereof is 100 ppm or more is adopted.
摘要翻译:本发明的目的是提供一种耐软化性能优异的铜箔,其在约350℃〜400℃下热处理后的抗拉强度降低。为了达到上述目的,将表面处理铜箔 在由铜合金构成的防锈处理层的铜箔的两面上设有防锈处理层,防锈处理层为锌量为20mg / m 2的锌合金层 至1,000 mg / m2; 铜箔含有一种或两种以上选自碳,硫,氯和氮的少量元素,其总量为100ppm以上。