UV RELEASE TAPE
    1.
    发明公开
    UV RELEASE TAPE 审中-公开

    公开(公告)号:US20240191102A1

    公开(公告)日:2024-06-13

    申请号:US18169847

    申请日:2023-02-15

    Abstract: A UV release tape includes a substrate layer, a UV release layer, and a separation layer. The UV release layer is disposed between the substrate layer and the separation layer. A material of the substrate layer includes a polyvinyl chloride, a plasticizer, and a metal salt compound. Relative to 100 phr of the polyvinyl chloride, an amount of the metal salt compound ranges from 1 phr to 8 phr. The metal salt compound includes a calcium salt compound and a zinc salt compound. A peeling strength of the UV release layer toward a silicon wafer is higher than 10 N/in. After being exposed to UV light, the peeling strength of the UV release layer toward the silicon wafer is lower than 0.3 N/in.

    PRESSURE-SENSITIVE ADHESIVE TAPE
    9.
    发明申请
    PRESSURE-SENSITIVE ADHESIVE TAPE 有权
    压敏胶带

    公开(公告)号:US20150259576A1

    公开(公告)日:2015-09-17

    申请号:US14629681

    申请日:2015-02-24

    Abstract: Disclosed is a pressure-sensitive adhesive tape that uses, as a plasticizer, an alternative compound to bis(2-ethylhexyl)phthalate (DOP) and dibutyl phthalate (DBP), has excellent tackiness, and can be unwound satisfactorily, where DOP and DBP are to be restricted under the REACH regulation. The pressure-sensitive adhesive tape includes a poly(vinyl chloride) substrate and a pressure-sensitive adhesive layer. The pressure-sensitive adhesive layer is disposed on or over one side of the substrate. The poly(vinyl chloride) substrate contains 10 to 40 percent by weight of bis(2-ethylhexyl)terephthalate. The pressure-sensitive adhesive tape preferably has an unwinding force of 0.4 N/20 mm or less at a tensile speed of 0.3 m/min and an unwinding force of 1.2 N/20 mm or less at a tensile speed of 30 m/min.

    Abstract translation: 公开了使用邻苯二甲酸双(2-乙基己基)酯和邻苯二甲酸二丁酯(DBP)作为增塑剂作为增塑剂的粘合带,具有优异的粘合性,并且可令人满意地展开,其中DOP和DBP 将受到REACH法规的限制。 粘合带包括聚(氯乙烯)基材和压敏粘合剂层。 压敏粘合剂层设置在基材的一侧或上方。 聚(氯乙烯)基材含有10〜40重量%的对苯二甲酸双(2-乙基己基)酯。 压敏粘合带优选在拉伸速度为0.3m / min,退绕力为1.2N / 20mm以下,拉伸速度为30m / min时,退绕力为0.4N / 20mm以下。

Patent Agency Ranking