METHOD OF METALIZING SURFACE AND ARTICLE OBTAINABLE
    2.
    发明申请
    METHOD OF METALIZING SURFACE AND ARTICLE OBTAINABLE 有权
    金属化表面和可获得物品的方法

    公开(公告)号:US20140308450A1

    公开(公告)日:2014-10-16

    申请号:US14315166

    申请日:2014-06-25

    发明人: Weifeng MIAO

    IPC分类号: C23C18/18 C23C28/00 C23C18/16

    摘要: A method of metalizing a surface of an insulation substrate includes: applying an ink composition onto the surface to form an ink layer; subjecting the insulation substrate to heat treatment at a temperature of about 500 to 1000 degrees Celsius in a non-reactive atmosphere; plating a metal layer on the ink layer. The ink composition comprises a metal compound and an ink vehicle. The metal compound includes at least one selected from a group consisting of a nano-copper oxide, a nano-cuprous oxide, a compound of formula I, and a compound of formula II, TiO2-σ (I), M1M2pOq (II), 0.05≦σ

    摘要翻译: 绝缘基板的表面金属化的方法包括:将油墨组合物施加到所述表面上以形成油墨层; 使绝缘基板在非反应性气氛中在约500至1000摄氏度的温度下进行热处理; 在油墨层上镀金属层。 油墨组合物包含金属化合物和油墨载体。 金属化合物包括选自纳米氧化铜,纳米氧化亚铜,式I化合物和式II化合物的至少一种,TiO 2 - (I)中,M1M2pOq(II),0.05&nlE;&sgr; <1.8,其中,M1是选自元素周期表第2,9-12族中的至少一种元素,M2是选自 由周期表第3-8,10和13组组成的组,0

    INK COMPOSITION, METHOD OF METALIZING SURFACE AND ARTICLE OBTAINABLE
    3.
    发明申请
    INK COMPOSITION, METHOD OF METALIZING SURFACE AND ARTICLE OBTAINABLE 有权
    墨水组合物,表面金属化方法和可获得的物品

    公开(公告)号:US20140308531A1

    公开(公告)日:2014-10-16

    申请号:US14315137

    申请日:2014-06-25

    发明人: Weifeng MIAO

    IPC分类号: C09D11/02

    摘要: An ink composition is provided, a method of metalizing a surface of an insulation substrate and an article obtainable by the method are also provided. The ink composition may comprise a metal compound and an ink vehicle, the metal compound is at least one selected from a group consisting of a compound of formula I and a compound of formula II, TiO2-σ(I), M1M2pOq (II), 0.05≦σ

    摘要翻译: 提供了一种油墨组合物,还提供了一种使绝缘基材的表面金属化的方法和可通过该方法获得的制品。 油墨组合物可以包含金属化合物和油墨载体,金属化合物是选自由式I化合物和式II化合物组成的组中的至少一种,TiO 2 - 和(I),M1M2pOq(II) ,0.05&nlE;&lt; 1.8,M1是根据IUPAC命名从元素周期表的组2,9-12中选择的至少一种元素,M2是选自组3中的至少一种元素 -8,10和13根据IUPAC命名,0

    METALIZED PLASTIC ARTICLES AND METHODS THEREOF
    7.
    发明申请
    METALIZED PLASTIC ARTICLES AND METHODS THEREOF 审中-公开
    金属化塑料制品及其方法

    公开(公告)号:US20150104668A1

    公开(公告)日:2015-04-16

    申请号:US14576950

    申请日:2014-12-19

    摘要: Metalized plastic substrates, and methods thereof are provided herein. The method includes providing a plastic having a plurality of accelerators dispersed in the plastic. The accelerators have a formula ABO3, wherein A is one or more elements selected from Groups 9, 10, and 11 of the Periodic Table of Elements, B is one or more elements selected from Groups 4B and 5B of the Periodic Table of Elements, and O is oxygen. The method includes the step of irradiating a surface of plastic substrate to expose at least a first accelerator. The method further includes plating the irradiated surface of the plastic substrate to form at least a first metal layer on the at least first accelerator, and then plating the first metal layer to form at least a second metal layer.

    摘要翻译: 金属化塑料基板及其方法在此提供。 该方法包括提供具有分散在塑料中的多个加速器的塑料。 加速剂具有式ABO 3,其中A是选自元素周期表第9,10和11族的一种或多种元素,B是选自元素周期表的第4B和5B族的一种或多种元素,以及 O是氧气。 该方法包括照射塑料基板的表面以暴露至少第一加速器的步骤。 该方法还包括电镀塑料基板的照射表面以在至少第一加速器上形成至少第一金属层,然后电镀第一金属层以形成至少第二金属层。

    METALIZED PLASTIC ARTICLES AND METHODS THEREOF
    9.
    发明申请
    METALIZED PLASTIC ARTICLES AND METHODS THEREOF 有权
    金属化塑料制品及其方法

    公开(公告)号:US20140356645A1

    公开(公告)日:2014-12-04

    申请号:US14462293

    申请日:2014-08-18

    IPC分类号: B32B15/08 H05K1/05 B32B15/04

    摘要: Metalized plastic substrates, and methods thereof are provided herein. The method includes providing a plastic substrate having a plurality of accelerators dispersed in the plastic substrate. The accelerators have a formula selected from the group consisting of: CuFe2O4-δ, Ca0.25Cu0.75TiO3-β, and TiO2-σ, wherein δ, β, σ denotes oxygen vacancies in corresponding accelerators and 0.05≦δ≦0.8, 0.05≦β≦0.5, and 0.05≦σ≦1.0. The method further includes removing at least a portion of a surface of the plastic substrate to expose at least a first accelerator. The method further includes plating the exposed surface of the plastic substrate to form at least a first metal layer on the at least first accelerator, and then plating the first metal layer to form at least a second metal layer.

    摘要翻译: 金属化塑料基板及其方法在此提供。 该方法包括提供具有分散在塑料基板中的多个加速器的塑料基板。 所述促进剂具有选自CuFe 2 O 4-δ,Ca 0.25 La 0.75 TiO 3 - &bgr,和TiO 2 - &amp; Gr,其中δ,&bgr; 表示相应促进剂中的氧空位,0.05&amp; NlE;δ&nlE; 0.8,0.05&nlE;&bgr;&nlE; 0.5和0.05&nlE;&sgr;&nlE; 1.0。 该方法还包括去除塑料基板表面的至少一部分以暴露至少第一加速器。 该方法还包括电镀塑料基板的暴露表面以在至少第一加速器上形成至少第一金属层,然后电镀第一金属层以形成至少第二金属层。