摘要:
A large Group III nitride crystal of high quality with few defects such as a distortion, a dislocation, and warping is produced by vapor phase epitaxy. A method for producing a Group III nitride crystal includes: a first Group III nitride crystal production process of producing a first Group III nitride crystal 1003 by liquid phase epitaxy; and a second Group III nitride crystal production process of producing a second Group III nitride crystal 1004 on the first crystal 1003 by vapor phase epitaxy. In the first Group III nitride crystal production process, the surfaces of seed crystals 1003a (preliminarily provided Group III nitride) are brought into contact with an alkali metal melt, a Group III element and nitrogen are cause to react with each other in a nitrogen-containing atmosphere in the alkali metal melt, and the Group III nitride crystals are bound together by growth of the Group III nitride crystals grown from the seed crystals 1003a to produce a first crystal 1003.
摘要:
The present invention is intended to provide a method of producing a Group III nitride crystal that prevents a halogen-containing by-product from adversely affecting crystal generation and is superior in reactivity and operability. A method of producing a Group III nitride crystal includes a step of causing a Group III metal to react with an oxidizing gas and nitrogen-containing gas, thereby producing a Group III nitride crystal.
摘要:
A large Group III nitride crystal of high quality with few defects such as a distortion, a dislocation, and warping is produced by vapor phase epitaxy. A method for producing a Group III nitride crystal includes: a first Group III nitride crystal production process of producing a first Group III nitride crystal 1003 by liquid phase epitaxy; and a second Group III nitride crystal production process of producing a second Group III nitride crystal 1004 on the first crystal 1003 by vapor phase epitaxy by causing a Group III element metal to react with an oxidizing agent and nitrogen-containing gas. In the first Group III nitride crystal production process, the surfaces of seed crystals 1003a (preliminarily provided Group III nitride) are brought into contact with an alkali metal melt, a Group III element and nitrogen are cause to react with each other in a nitrogen-containing atmosphere in the alkali metal melt, and the Group III nitride crystals are bound together by growth of the Group III nitride crystals grown from the seed crystals 1003a to produce a first crystal 1003.
摘要:
To provide a method for producing a Group III element nitride crystal by growing it on a plane on the −c-plane side as a crystal growth plane. The present invention is a method for producing a Group III element nitride crystal, including a vapor phase growth step of growing a Group III element nitride crystal 12 on a crystal growth plane of a Group III element nitride seed crystal 11 by vapor deposition. The vapor phase growth step is a step of causing a Group III metal, an oxidant, and a nitrogen-containing gas to react with one another to grow the Group III element nitride crystal 12 or includes: a reduced product gas generation step of causing a Group III element oxide and a reducing gas to react with each other to generate a gas of a reduced product of the Group III element oxide; and a crystal generation step of causing the gas of the reduced product and a nitrogen-containing gas to react with each other to generate the Group III element nitride crystal 12. The crystal growth plane is a plane on the −c-plane side. A crystal growth temperature is 1200° C. or more. In the vapor phase growth step, the Group III element nitride crystal is grown in an approximately −c direction.
摘要:
The present invention provides a method for producing a Group III nitride crystal that can produce a Group III nitride crystal of high quality with few defects such as crack, dislocation, and the like by vapor phase epitaxy. In order to achieve the above object, the method for producing a Group III nitride crystal of the present invention includes a step of: causing Group III element-containing gas 111a to react with nitrogen-containing gas 203a and 203b to generate a Group III nitride crystal 204, wherein in the Group III nitride crystal generation step, the reaction is performed in the presence of a carbon-containing substance.
摘要:
A method of manufacturing a group III nitride crystal according to a first aspect includes: preparing a seed substrate; generating a group III element oxide gas; supplying the group III element oxide gas; supplying a nitrogen element-containing gas; supplying an oxidizing gas containing nitrogen element containing at least one selected from the group consisting of NO gas, NO2 gas, N2O gas, and N2O4 gas; and growing the group III nitride crystal on the seed substrate.
摘要:
A method of manufacturing a group-III nitride crystal includes: a seed crystal preparation step of preparing a plurality of dot-shaped group-III nitrides on a substrate as a plurality of seed crystals for growth of a group-III nitride crystal; and a crystal growth step of bringing surfaces of the seed crystals into contact with a melt containing an alkali metal and at least one group-III element selected from gallium, aluminum, and indium in an atmosphere containing nitrogen and thereby reacting the group-III element with the nitrogen in the melt to grow the group-III nitride crystal.
摘要:
A production method for a group III nitride crystal, the production method includes: preparing a plurality of group III nitride pieces as a plurality of seed crystals on a substrate, and growing a group III nitride crystal by bringing a surface of each of the seed crystals into contact with a melt that comprises at least one group III element selected from gallium, aluminum, and indium, and an alkali metal in an atmosphere comprising nitrogen, and thereby reacting the group III element and the nitrogen in the melt, wherein the step of growing a group III nitride crystal includes: growing a plurality of first group III nitride crystals whose cross-sections each have a triangular shape or a trapezoidal shape, from the plurality of seed crystals; and growing second group III nitride crystals each in a gap among the plurality of first group III nitride crystals.
摘要:
An object of the present invention is to provide a method for producing a group III nitride crystal in which generation of breaking or cracks is less likely to occur. To achieve the object, the method for producing a group III nitride crystal includes: seed crystal preparation including disposing a plurality of crystals of a group III nitride as a plurality of seed crystals on a substrate; and crystal growth including growing group III nitride crystals by contacting a surface of each of the seed crystals with a melt containing at least one group III element selected from gallium, aluminum, and indium and an alkali metal in an atmosphere containing nitrogen. In the seed crystal preparation, the plurality of seed crystals are disposed within a hexagonal region provided on the substrate.
摘要:
There is provided a method for manufacturing a nitride crystal substrate, including: arranging a plurality of seed crystal substrates made of a nitride crystal in a planar appearance, so that their main surfaces are parallel to each other and their lateral surfaces are in contact with each other; growing a first crystal film using a vapor-phase growth method on a surface of the plurality of seed crystal substrates arranged in the planar appearance, and preparing a combined substrate formed by combining the adjacent seed crystal substrates each other by the first crystal film; growing a second crystal film using a liquid-phase growth method on a main surface of the combined substrate so as to be embedded in a groove that exists at a combined part of the seed crystal substrates, and preparing a substrate for crystal growth having a smoothened main surface; and growing a third crystal film using the vapor-phase growth method, on the smoothed main surface of the substrate for crystal growth.