摘要:
A large Group III nitride crystal of high quality with few defects such as a distortion, a dislocation, and warping is produced by vapor phase epitaxy. A method for producing a Group III nitride crystal includes: a first Group III nitride crystal production process of producing a first Group III nitride crystal 1003 by liquid phase epitaxy; and a second Group III nitride crystal production process of producing a second Group III nitride crystal 1004 on the first crystal 1003 by vapor phase epitaxy. In the first Group III nitride crystal production process, the surfaces of seed crystals 1003a (preliminarily provided Group III nitride) are brought into contact with an alkali metal melt, a Group III element and nitrogen are cause to react with each other in a nitrogen-containing atmosphere in the alkali metal melt, and the Group III nitride crystals are bound together by growth of the Group III nitride crystals grown from the seed crystals 1003a to produce a first crystal 1003.
摘要:
The present invention is intended to provide a method of producing a Group III nitride crystal that prevents a halogen-containing by-product from adversely affecting crystal generation and is superior in reactivity and operability. A method of producing a Group III nitride crystal includes a step of causing a Group III metal to react with an oxidizing gas and nitrogen-containing gas, thereby producing a Group III nitride crystal.
摘要:
To provide a method for producing a Group III element nitride crystal by growing it on a plane on the −c-plane side as a crystal growth plane. The present invention is a method for producing a Group III element nitride crystal, including a vapor phase growth step of growing a Group III element nitride crystal 12 on a crystal growth plane of a Group III element nitride seed crystal 11 by vapor deposition. The vapor phase growth step is a step of causing a Group III metal, an oxidant, and a nitrogen-containing gas to react with one another to grow the Group III element nitride crystal 12 or includes: a reduced product gas generation step of causing a Group III element oxide and a reducing gas to react with each other to generate a gas of a reduced product of the Group III element oxide; and a crystal generation step of causing the gas of the reduced product and a nitrogen-containing gas to react with each other to generate the Group III element nitride crystal 12. The crystal growth plane is a plane on the −c-plane side. A crystal growth temperature is 1200° C. or more. In the vapor phase growth step, the Group III element nitride crystal is grown in an approximately −c direction.
摘要:
A large Group III nitride crystal of high quality with few defects such as a distortion, a dislocation, and warping is produced by vapor phase epitaxy. A method for producing a Group III nitride crystal includes: a first Group III nitride crystal production process of producing a first Group III nitride crystal 1003 by liquid phase epitaxy; and a second Group III nitride crystal production process of producing a second Group III nitride crystal 1004 on the first crystal 1003 by vapor phase epitaxy by causing a Group III element metal to react with an oxidizing agent and nitrogen-containing gas. In the first Group III nitride crystal production process, the surfaces of seed crystals 1003a (preliminarily provided Group III nitride) are brought into contact with an alkali metal melt, a Group III element and nitrogen are cause to react with each other in a nitrogen-containing atmosphere in the alkali metal melt, and the Group III nitride crystals are bound together by growth of the Group III nitride crystals grown from the seed crystals 1003a to produce a first crystal 1003.
摘要:
The present invention provides a method for producing a Group III nitride crystal that can produce a Group III nitride crystal of high quality with few defects such as crack, dislocation, and the like by vapor phase epitaxy. In order to achieve the above object, the method for producing a Group III nitride crystal of the present invention includes a step of: causing Group III element-containing gas 111a to react with nitrogen-containing gas 203a and 203b to generate a Group III nitride crystal 204, wherein in the Group III nitride crystal generation step, the reaction is performed in the presence of a carbon-containing substance.