摘要:
The present invention relates to parts for automobiles, electrical/electronic devices, home appliances, office equipment, or daily necessities, which are manufactured by using a polymer resin composition that is capable of providing an environmentally friendly biomass-containing synthetic resin having improved chemical resistance. The parts for automobiles, electrical/electronic devices, home appliances, office equipment, or daily necessities which are manufactured by using a polymer resin composition including: a polyester copolymer including a residue of a dicarboxylic acid component containing terephthalic acid, and a residue of a diol component containing dianhydrohexitol; and one or more copolymers selected from the group consisting of an unsaturated nitrile-diene-based rubber-aromatic vinyl graft copolymer, an alkyl methacrylate-diene-based rubber-aromatic vinyl graft copolymer, and an alkyl methacrylate-silicone/alkyl acrylate graft copolymer, and which has a tensile strength loss defined in the following Equation 1 ranging from 0.5 to 30%, can be provided. Tensile Strength Loss (%)=[(Tensile Strength before Test−Tensile Strength after Test)/Tensile Strength before Test]×100 [Equation 1]
摘要:
The present invention relates to a polymer resin composition that is capable of providing an environmentally friendly biomass-containing synthetic resin having improved chemical resistance. The present invention provides a polymer resin composition including: a polyester copolymer including a residue of a dicarboxylic acid component containing terephthalic acid, and a residue of a diol component including dianhydrohexitol; and one or more copolymers selected from the group consisting of an unsaturated nitrile-diene-based rubber-aromatic vinyl graft copolymer, an alkyl methacrylate-diene-based rubber-aromatic vinyl graft copolymer, and an alkyl methacrylate-silicone/alkyl acrylate graft copolymer, and which has a tensile strength loss defined in the following Equation 1 ranging from 0.5 to 30%. Tensile Strength Loss (%)=[(Tensile Strength before Test−Tensile Strength after Test)/Tensile Strength before Test]×100 [Equation 1]
摘要:
This disclosure relates to a continuous solution polymerization process wherein production rate is increased. Process solvent, ethylene, optional comonomers, optional hydrogen and a single site catalyst formulation are injected into a first reactor forming a first ethylene interpolymer. Process solvent, ethylene, optional comonomers, optional hydrogen and a heterogeneous catalyst formulation are injected into a second reactor forming a second ethylene interpolymer. The first and second reactors may be configured in series or parallel modes of operation. Optionally, a third ethylene interpolymer is formed in an optional third reactor, wherein an optional heterogeneous catalyst formulation may be employed. In a solution phase, the first, second and optional third ethylene interpolymers are combined, the catalyst is deactivated, the solution is passivated and following a phase separation process an ethylene interpolymer product is recovered.
摘要:
An aqueous binder composition is provided that includes a carbohydrate and a crosslinking agent. In exemplary embodiments, the carbohydrate-based binder composition may also include a catalyst, a coupling agent, a process aid, a crosslinking density enhancer, an extender, a moisture resistant agent, a dedusting oil, a colorant, a corrosion inhibitor, a surfactant, a pH adjuster, and combinations thereof. The carbohydrate may be natural in origin and derived from renewable resources. Additionally, the carbohydrate polymer may have a dextrose equivalent (DE) number from 2 to 20. In at least one exemplary embodiment, the carbohydrate is a water-soluble polysaccharide such as dextrin or maltodextrin and the crosslinking agent is citric acid. Advantageously, the carbohydrates have a low viscosity and cure at moderate temperatures. The environmentally friendly, formaldehyde-free binder may be used in the formation of insulation materials and non-woven chopped strand mats. A method of making fibrous insulation products is also provided.
摘要:
Described herein is a melt-processible polymer composition comprising: a non-fluorinated melt-processible polymer; and a fluorine-containing polymer comprising an end-group having a structures from group consisting of: and combinations thereof; wherein X1, X2, and X3 are each independently selected from H, F, Cl, a C1 to C4 alkyl group, and a C1 to C4 fluorinated alkyl group; R7 is a linking group comprising at least 2 or more catenary atoms; and Z1 and Z2 are independently selected from F, CF3, and a perfluoroalkyl group.
摘要:
The invention provides a composition comprising the following components: A) a first composition, wherein the first composition comprises a first ethylene-based polymer and a second ethylene-based polymer, and wherein the ratio of the “high load melt index (I21) of the first composition” to the “high load melt index (I21) of the first ethylene-based polymer” is greater than, or equal to, 40, and B) one or more azide compounds present in an amount greater than, or equal to, 50 ppm, based on the weight of the first composition.
摘要:
The invention relates to a thermoplastic composition capable of being plated after being activated using a laser, with improved mechanical properties the composition comprising: a) from 30 to 60 wt. % of a thermoplastic base resin; b) from 1.0 to 8.0 wt. % of a laser direct structuring additive; c) from 5 to 40 wt. % of aluminum oxide, boron nitride, or a combination thereof, d) from 5 to 25 w % of a flame retardant and e) from 5 to 30 wt. % of glass fibers.
摘要:
The invention relates to composite polymer modifiers for thermoplastic resins, and especially for polyvinyl chloride (PVC). The composite modifier is an intimate blend of mineral filler and polymeric process aid, which is formed by the co-powderization of aqueous emulsions, suspensions or slurries of one or more mineral filler(s) and process aid(s). The resulting composite modifier provides more effective modification of the thermoplastic resin than by the use of the dried components formed separately. The composite modifier may also contain other co-powderized components such as impact modifiers, for additional benefits.
摘要:
The extrudable composition may be an extrudable composition having a heat deflection temperature greater than about 50° C. and a melting point between about 80° C. to about 190° C., the extrudable composition includes about 60 to about 99.8% partially crystalline or crystalline polylactic acid, about 0.05 to about 8% cyclodextrin, about 0.1 to about 8% natural oil, fatty acid, fatty acid ester, wax or waxy ester, about 0.01 to about 5% nanofibers, about 0 to about 10% crystallinity agent, about 0 to about 1% starch-based melt rheology modifier, about 0 to about 5% colorant, about 0 to about 1% plasticizer, about 0 to about 1% gloss agent, and about 0 to about 1% barrier agent.
摘要:
A low-wear microporous friction material with a high stability coefficient and a manufacturing method thereof are provided. The formula of the friction material includes GM-15 resin 15-50 wt %, rubber 0-10 wt %, shaping aid 0.5-5 wt %, sintering aid 0.5-5 wt %, foaming aid 0.5-5 wt %, kaolin powder 0.5-20 wt %, barite powder 5-40 wt %, carbon fiber 2-20 wt %, KEVLAR 1-5 wt %, zinc oxide 1-10 wt %, and iron oxide red 0-2 wt %. By adjusting the hydrophilicity of the friction material and controlling the surface tension of the material, the friction coefficient of the material is kept from lowering under wet conditions and is rendered stable in dry and wet conditions. More specifically, the friction coefficient of the friction material stays above 0.25 under wet conditions, and the stability coefficient of the friction coefficient can reach 85% or above on an MM 1000 tester.