摘要:
According to one aspect, a roof membrane is provided. The roofing membrane includes a main body, a first adhesive material, and a second adhesive material. The first adhesive material is bonded to a top surface of the main body and positioned toward a first edge thereof. The second adhesive material is bonded to the top surface of the main body and positioned toward a second edge thereof. The second edge is positioned opposite the first edge such that the first and second adhesive materials are positioned toward opposite edges of the main body and the same surface thereof.
摘要:
The present relates a laminate comprising: an outer polyethylene (PE) layer; a first adhesive layer; a substrate layer with one side selectively vacuum metalized or selectively reverse printed and said printed or metalized side is toward first adhesive layer; a second adhesive layer; an ethylene vinyl alcohol (EVOH) polymer barrier film layer; an linear density polyethylene (LDPE) extrusion layer; and an inner polyethylene (PE) layer. The present disclosure further relates to tubes made of the partially opaque and partially clear laminate. The present disclosure also relates to a process of manufacturing of tubes using the said laminate.
摘要:
The present disclosure is directed to multilayer film having has an L* color less than 30 and a 60 degree gloss value less than 10. The multilayer film has a first polyimide layer and a second polyimide layer. The second polyimide layer has 25 to 50 wt % of a polyimide, 15 to 35 wt % of a polyimide particle matting agent, greater than 0 and less than 20 wt % of at least one submicron carbon black and 15 to 50 wt % of at least one submicron fumed metal oxide.
摘要:
The present specification relates to a method for manufacturing a polarizing plate and a polarizing plate. More particularly, the present specification relates to a method for manufacturing a polarizing plate locally having a depolarization region, and a polarizing plate.
摘要:
A skin material (1) includes a cellular heat-insulating layer (3) and a coloring layer (4) which are sequentially stacked on a fibrous substrate (2) and has protrusions and recesses on a front face (6). The cellular heat-insulating layer (3) has a softening temperature of 110 to 250° C. A contact cool feeling (Qmax) of the front face (6) of the skin material (1) is 0.30 W/cm2 or less both before and after a heat treatment for 2400 hours at 70° C.
摘要翻译:表皮材料(1)包括依次堆叠在纤维基材(2)上并在前表面(6)上具有凹凸的多孔隔热层(3)和着色层(4)。 多孔隔热层(3)的软化温度为110〜250℃。表皮材料(1)的前面(6)的接触冷却感(Qmax)在0.30以下,均为0.30W / cm 2以下 并在70℃热处理2400小时。
摘要:
A laminated glass comprising at least one chemically tempered pane is described. The chemically tempered pane comprises a first pane and a second pane, which are connected to each other by means of an intermediate layer. The first pane is a chemically tempered glass pane having a thickness less than or equal to 2.1 mm, wherein the intermediate layer contains at least one thermoplastic connection layer and a thermoplastic carrier layer, and the carrier layer has a functional coating or functional inclusions.
摘要:
The present invention relates to a decorative panel comprising a core layer, a decorative layer applied to said core, and a transparent or translucent outermost layer applied to said decorative layer, said outermost layer consisting essentially of a synthetic resin, wherein said decorative layer is a IR reflectivity increasing layer. An object of the present invention is to provide a decorative panel that reflects a significant part of the IR light without affecting the visual appearance of the surface.
摘要:
A label 1 includes a first colored layer 10, a second colored layer 20 having a different color from the first colored layer 10, and an indicating layer 30 having a different color from the first colored layer 10 and the second colored layer 20. The indicating layer 30 is fitted into the first colored layer 10 so as to have an exposed surface on one surface of the first colored layer 10. The second colored layer 20 is laminated on the other surface F2 of the first colored layer 10. The curing shrinkage ratio of the first colored layer 10 is larger than that of the indicating layer 30.
摘要:
The present invention relates to rear-projection film with “day/night” effect comprising at least two layers, where the film comprises at least one grey layer comprising at least one thermoplastic with transmittance of from 10% to 70% in the visible wavelength range and at least one layer comprising at least one thermoplastic and scattering particles, and also to the use of the said films as rear-projection areas in the vehicle interior sector.
摘要:
A multi layered card embodying the invention includes an outer layer of an amorphous laser reactive copolymer material which is embossed with a selected pattern at a selected temperature which is above the glass transition temperature, Tg, of the copolymer and below its melting temperature, Tm. So embossed, the selected pattern is set in the copolymer layer, and its external shape cannot be changed from the embossed form to which it was set at the selected temperature, without destroying the selected pattern. The outer layer may be laminated with the other layers of the card and laser engraved before or after lamination.