ROUGHENED NICKEL-PLATED SHEET
    4.
    发明申请

    公开(公告)号:US20230057775A1

    公开(公告)日:2023-02-23

    申请号:US17794509

    申请日:2021-01-22

    IPC分类号: C25D5/00 C25D5/36

    摘要: A roughened nickel-plated sheet including a roughened nickel layer on at least one surface of a metal substrate as the outermost layer thereof, the roughened nickel layer being formed of a plurality of nickel protrusions. When the structure of the roughened nickel-plated sheet is observed at height positions with a focused ion beam scanning electron microscope (FIB-SEM), the absolute value of the change rate of the nickel occupancy is equal to or less than a predetermined value, and the nickel occupancy and the number of nickel protrusions present at a height position located 2.0 μm from the base position of the roughened nickel layer toward the surface in the height direction are equal to or more than predetermined values, respectively.

    Surface-treated steel sheet for battery containers, battery container, and battery

    公开(公告)号:US10665825B2

    公开(公告)日:2020-05-26

    申请号:US15876894

    申请日:2018-01-22

    摘要: A surface-treated steel sheet for battery containers is provided. The surface-treated sheet is used to form a battery container for a battery. The battery uses a nonaqueous electrolytic solution as an electrolytic solution. The surface-treated steel sheet includes a base material made of steel and an iron-nickel diffusion layer formed by performing thermal diffusion treatment after forming a nickel plating layer at least on a surface of the base material to be located at the inner surface side of the battery container. The iron-nickel diffusion layer has an outermost layer of which a ratio of Ni and Fe is 7.5 or less as a molar ratio of Ni/Fe. The iron-nickel diffusion layer has a thickness of 0.6 μm or more.

    SURFACE-TREATED METAL PLATE, CELL CONTAINER, AND CELL

    公开(公告)号:US20200035960A1

    公开(公告)日:2020-01-30

    申请号:US16498741

    申请日:2018-03-30

    摘要: A surface-treated metal plate including: a metal plate; and a nickel-cobalt binary alloy layer formed on the metal plate. When a part having a content ratio of oxygen atoms of 5 atomic % or more as measured by X-ray photoelectron spectroscopic analysis is an oxide coating film, the nickel-cobalt binary alloy layer contains the oxide coating film with a thickness of 0.5 to 30 nm on a surface thereof, and when a pressure cooker test including temperature increasing, retention for 72 hours under a water-vapor atmosphere at a temperature of 105° C. and a relative humidity of 100% RH, and temperature decreasing is performed, the amount of increase in the thickness of the oxide coating film is 28 nm or less.