Method for the production of adhesive-coated articles, articles obtainable thereby and their use
    2.
    发明授权
    Method for the production of adhesive-coated articles, articles obtainable thereby and their use 有权
    用于生产粘合剂涂覆制品的方法,可获得的制品及其用途

    公开(公告)号:US09321939B2

    公开(公告)日:2016-04-26

    申请号:US13823335

    申请日:2011-09-14

    摘要: Method for the production of adhesive-coated articles, articles obtainable thereby and their use A method for the production of adhesive-coated articles comprises the steps of: (I) providing a substrate; (II) applying a first polyurethane and/or polyurethane-polyurea polymer onto the substrate, the first polyurethane and/or polyurethane-polyurea polymer being capable of attaining an at least partially crystalline state with a final degree of crystallinity and wherein during and/or after the application the first polyurethane and/or polyurethane-polyurea polymer is present in a non-crystalline state. The method further comprises the steps: (III) applying onto the first polyurethane and/or polyurethane-polyurea polymer of step (II) a composition comprising a mixture of a second polyurethane and/or polyurethane-polyurea polymer and furthermore an acrylate polymer, wherein the application is performed while the degree of crystallinity of the first polyurethane-polyurea polymer is lower than its final degree of crystallinity; and (IV) cooling the article obtained to a temperature below the glass transition temperature of the acrylate polymer.

    摘要翻译: 用于生产粘合剂涂覆制品的方法,可获得的制品及其用途制备粘合剂涂覆制品的方法包括以下步骤:(I)提供基材; (II)将第一聚氨酯和/或聚氨酯 - 聚脲聚合物施加到所述基材上,所述第一聚氨酯和/或聚氨酯 - 聚脲聚合物能够获得具有最终结晶度的至少部分结晶状态,并且其中在和/或 在施用之后,第一种聚氨酯和/或聚氨酯 - 聚脲聚合物以非结晶状态存在。 该方法还包括以下步骤:(III)将步骤(II)的第一聚氨酯和/或聚氨酯 - 聚脲聚合物施加到包含第二聚氨酯和/或聚氨酯 - 聚脲聚合物以及丙烯酸酯聚合物的混合物的组合物中,其中 在第一聚氨酯 - 聚脲聚合物的结晶度低于其最终结晶度的同时进行应用; 和(IV)将获得的制品冷却到低于丙烯酸酯聚合物的玻璃化转变温度的温度。

    COMPRESSION OF A CRYOGENIC MEDIUM
    4.
    发明申请
    COMPRESSION OF A CRYOGENIC MEDIUM 审中-公开
    低温介质的压缩

    公开(公告)号:US20130213059A1

    公开(公告)日:2013-08-22

    申请号:US13771510

    申请日:2013-02-20

    IPC分类号: F25B1/10

    CPC分类号: F25B1/10 F04B37/14 F04B41/06

    摘要: A method for compressing a cryogenic medium, in particular hydrogen, oxygen, nitrogen or argon is described. The cryogenic medium is compressed in two compressor stages from an initial pressure to a final pressure by way of an intermediate pressure, such that the first compressor stage is designed as a cryogenic compressor stage. The cryogenic medium is advantageously compressed to a pressure between 30 and 70 bar in the first compressor stage and in the second compressor stage is compressed to the desired final pressure by means of a hot gas compression.

    摘要翻译: 描述了一种用于压缩低温介质,特别是氢气,氧气,氮气或氩气的方法。 低温介质在两个压缩机阶段通过中间压力从初始压力压缩到最终压力,使得第一压缩机级被设计为低温压缩机级。 低温介质有利地在第一压缩机级中压缩至30至70巴之间的压力,并且通过热气体压缩将低温介质压缩至期望的最终压力。

    Sol-gel coating from water-soluble oxalamides
    5.
    发明授权
    Sol-gel coating from water-soluble oxalamides 有权
    溶胶 - 凝胶涂层从水溶性草酰胺

    公开(公告)号:US07371463B2

    公开(公告)日:2008-05-13

    申请号:US11058339

    申请日:2005-02-15

    IPC分类号: B32B25/20

    CPC分类号: C08K5/5455 Y10T428/31663

    摘要: Coating compositions for producing sol-gel coatings that include: a) one or more alkoxysilyl-containing oxalamides of the general formula (II), where R″ is hydrogen or an organic C1-C10 radical, R′ radicals are organic, optionally oxygen-attached C1-C10 radicals, R is an oxygen-attached radical optionally containing one or more ether groups and having 1 to 30 carbon atoms and n is an integer between 0 and 2, b) optionally further crosslinkers, c) one or more catalysts and d) water. The sol-gel coatings are produced by a method that includes combining a silica sol and one or more alkoxysilyl-containing oxalamides. The sol-gel coatings obtained from the above-described coating compositions can be used to coat substrates.

    摘要翻译: 用于生产溶胶 - 凝胶涂层的涂料组合物,其包括:a)一种或多种通式(II)的含烷氧基甲硅烷基的草酰胺,其中R“为氢或有机C 1 -C 3 R 10自由基是有机的,任选地与氧连接的C 1 -C 10基团,R是含氧的基团,任选地含有一个或多个 更多的醚基团并且具有1至30个碳原子,n是0和2之间的整数,b)任选地进一步的交联剂,c)一种或多种催化剂和d)水。 溶胶 - 凝胶涂层通过包括将硅溶胶与一种或多种含有烷氧基甲硅烷基的草酰胺结合的方法制备。 由上述涂料组合物获得的溶胶 - 凝胶涂层可用于涂覆基材。

    Waterborne polyurethane adhesive composition and method for bonding articles
    6.
    发明授权
    Waterborne polyurethane adhesive composition and method for bonding articles 有权
    水性聚氨酯粘合剂组合物和粘合物品的方法

    公开(公告)号:US09475971B2

    公开(公告)日:2016-10-25

    申请号:US13989532

    申请日:2011-11-24

    摘要: The present invention relates to novel waterborne adhesives which are polymerizable by UV light and are capable of being activated by heat, and which particularly display good adhesion to difficult substrates, such as ethylene vinyl acetate copolymers (EVA) with a low vinyl acetate content, or rubber. The invention further provides a novel method in which, after the application of the waterborne adhesive to an article and drying, irradiation with UV light and at the same time or thereafter activation by heat are performed. The adhesive film which is irradiated and activated in this way is then bonded to a further article. The invention also provides the use of the adhesives to make items such as shoes.

    摘要翻译: 本发明涉及通过紫外光可聚合并能够被热活化的新型水性粘合剂,并且其特别显示出对困难的基材的良好粘附性,例如具有低乙酸乙烯酯含量的乙烯乙酸乙烯酯共聚物(EVA)或 橡胶。 本发明还提供了一种新的方法,其中在将水性粘合剂施加到制品上并干燥之后,进行紫外线照射,同时或之后进行热激活。 以这种方式照射和活化的粘合剂膜然后与另外的制品粘合。 本发明还提供了粘合剂用于制造诸如鞋的物品的用途。

    Device and method for removing liquid from a surface of a disc-like article
    8.
    发明授权
    Device and method for removing liquid from a surface of a disc-like article 有权
    用于从盘状物品的表面去除液体的装置和方法

    公开(公告)号:US08911561B2

    公开(公告)日:2014-12-16

    申请号:US13053587

    申请日:2011-03-22

    IPC分类号: H01L21/67

    摘要: A method for removing liquid from a surface of a disc includes, rotating the disc article about an axis perpendicular to the disc's main surface, supplying liquid from a supply port, moved across the substrate towards the edge of the disc, onto the rotated disc, supplying a first gas flow through a first gas supply port onto the disc article to an area whose center has a distance to the center of rotational movement of not more than 20 mm, the area being covered with a liquid layer thereby opening the liquid layer at a discrete area, and supplying a second gas flow through a second gas supply port moved across the substrate towards the edge of the substrate onto the rotated disc wherein the distance of the second gas supply port to the center is lower than the distance of the liquid supply port to the center.

    摘要翻译: 从盘的表面去除液体的方法包括:围绕垂直于盘的主表面的轴旋转盘制品,将来自供给口的液体从基板朝向盘的边缘移动到旋转盘上, 将第一气体流通过第一气体供给口到盘制品上至中心与旋转中心的距离不大于20mm的区域,该区域被液层覆盖,从而将液体层打开 离散区域,并且将第二气体流动通过第二气体供给口移动跨过衬底朝向衬底的边缘移动到旋转盘上,其中第二气体供给口到中心的距离低于液体的距离 供应端口到中心。

    HOT-SEALABLE COATING SYSTEMS AND METHOD FOR JOINING SURFACES
    10.
    发明申请
    HOT-SEALABLE COATING SYSTEMS AND METHOD FOR JOINING SURFACES 有权
    热封涂层系统和接合表面的方法

    公开(公告)号:US20130269874A1

    公开(公告)日:2013-10-17

    申请号:US13883784

    申请日:2011-11-08

    IPC分类号: C09J131/04 C09J175/00

    摘要: Hot-sealable coating systems and method for joining surfaces The present invention relates to a hot-sealable coating system, comprising a polyurethane and/or polyurethane-polyurea polymer (I) and an olefin vinyl acetate copolymer (II). The polyurethane and/or polyurethane-polyurea polymer (I) is obtainable by the reaction of (A) at least one diol and/or polyol component, (B) at least one di-and/or polyisocyanate component, (C) at least one component having sulphonate and/or carboxylate groups, (D) mono-, di-and/or tri-amino-functional and/or hydroxyamino-functional compounds (as appropriate), (E) other isocyanate—reactive compounds (as appropriate). The polyurethane and/or polyurethane-polyurea polymer (I) has a glass transition temperature of ≦10 ° C. and the olefin vinyl acetate copolymer (II) has a minimum film forming temperature (white point temperature) of >+40° C. The invention also relates to the use of the coating system and a method for joining surfaces in which the coating system according to the invention is used.

    摘要翻译: 热封性涂料体系和表面接合方法技术领域本发明涉及一种可热封的涂料体系,其包含聚氨酯和/或聚氨酯 - 聚脲聚合物(I)和烯烃乙酸乙烯酯共聚物(II)。 聚氨酯和/或聚氨酯 - 聚脲聚合物(I)可通过(A)至少一种二醇和/或多元醇组分,(B)至少一种二 - 和/或多异氰酸酯组分(C)至少 一种具有磺酸盐和/或羧酸盐基团的组分,(D)单 - ,二 - 和/或三 - 氨基官能和/或羟基氨基官能化合物(如适用),(E)其它异氰酸酯反应性化合物 。 聚氨酯和/或聚氨酯 - 聚脲聚合物(I)的玻璃化转变温度为10℃,烯烃乙酸乙烯酯共聚物(II)的最低成膜温度(白点温度)> 40℃。 本发明还涉及涂层系统的使用以及其中使用根据本发明的涂层系统的表面接合方法。